admin

admin

D2625-20 – Standard Test Method Technical Guide

📐 Scope and Test Overview ASTM D2625-20, developed under the jurisdiction of Subcommittee D02.L0.05 on Solid Lubricants, provides a standardized methodology for evaluating the performance of dry solid film lubricants under sliding steel-on-steel conditions. This test method is approved for…

D2626 – Standard Test Method Technical Guide

🛠️ Materials and Manufacture ASTM D2626/D2626M covers asphalt-saturated and coated organic felt base sheet designed for built-up roofing systems. During manufacture, a single thickness of dry organic felt is saturated with hot asphalt, coated on both sides with a hot…

D2622-24 – Standard Test Method Technical Guide

ASTM D2622-24a is a standard test method for determining the total sulfur content in petroleum and petroleum products using wavelength dispersive X-ray fluorescence (WDXRF) spectrometry. It serves as a critical tool for regulatory compliance, quality control, and process management across…

D2624-22 – Standard Test Method Technical Guide

Designation: D2624−22 / 274 These test methods, under the jurisdiction of ASTM Subcommittee D02.J0.04 on Additives and Electrical Properties, provide standardized procedures for the determination of the electrical conductivity of aviation and distillate fuels, both with and without static dissipator…

D2621-87 – Standard Test Method Technical Guide

This test method covers the qualitative characterization or identification of separated paint vehicle solids using infrared spectroscopy within the limitations of the technique. It is part of ASTM D2621-87, reaffirmed in 2024. 📐 Scope and Significance 1.1 This test method…

D262-81 – Standard Test Method Technical Guide

The ASTM D262-81 (Reapproved 1999) specification defines the rigorous requirements for the manufactured inorganic pigment known as ultramarine blue. Recognized for its distinctive hue and chemical stability, this pigment is primarily intended for use in architectural paints, industrial enamels, printing…

D2617-24 – Standard Test Method Technical Guide

📐 Test Overview and Significance ASTM D2617-24 outlines a standard test method for determining the total ash content in leather, which represents the approximate amount of nonvolatile inorganic material such as salts and oxides. The procedure involves igniting a test…

D2619-21 – Standard Test Method Technical Guide

ASTM D2619‑21, the Standard Test Method for Hydrolytic Stability of Hydraulic Fluids (Beverage Bottle Method), specifies a stringent accelerated aging test to evaluate the resistance of hydraulic fluids to chemical decomposition in the presence of water. This method helps predict…

D2613-01 – Standard Test Method Technical Guide

ASTM D2613-01 (Reapproved 2023) provides a standardized titrimetric procedure for the quantitative determination of calcium and zinc in pure liquid paint driers. It relies on the selective chelation of these metal ions using the disodium salt of ethylenediaminetetraacetic acid dihydrate…