D3168-85 – Standard Test Method Technical Guide

📘 Overview and Scope This standard practice, designated ASTM D3168 −85 (Reapproved 2022), establishes a reliable dual-method procedure for the qualitative identification of polymers that constitute the major components of the vehicle in emulsion paints. Designed to overcome the analytical…

D3169-89 – Standard Test Method Technical Guide

🌻 Scope and Material Sourcing This specification (Designation D 3169 – 89, Reapproved 2001) defines the quality requirements for once-refined sunflower oil intended for use in protective coatings. The material must be derived exclusively from sunflower seeds and subjected to…

D3167-10 – Standard Test Method Technical Guide

The ASTM D3167-10 (Reapproved 2017) standard specifically defines the Floating Roller Peel Resistance of Adhesives. This test method provides a robust means for determining the metal-to-metal peel strength of adhesive bonds, using a simple specimen preparation and testing procedure that…

D3165-07 – Standard Test Method Technical Guide

📐 Specimen Configuration and Scope ASTM D3165 – 07 (Reapproved 2023) is formally designated as the Standard Test Method for Strength Properties of Adhesives in Shear by Tension Loading of Single-Lap-Joint Laminated Assemblies. This test method is intended for determining…

D3166-99 – Standard Test Method Technical Guide

ASTM D3166-99 (Reapproved 2020) is a standardized test method used to evaluate the fatigue properties of adhesives in shear under tension loading, specifically for metal-to-metal bonded assemblies. This method provides critical data on the durability of adhesive joints under cyclic…

D3164-03 – Standard Test Method Technical Guide

📐 Scope and Application of ASTM D3164 The ASTM D3164-03 (Reapproved 2017) standard provides a method for determining the strength properties of adhesively bonded plastic lap-shear sandwich joints in shear by tension loading. It is specifically designed to complement Test…

D3164M-03 – Standard Test Method Technical Guide

📐 Scope and Applicability The D3164M-03 standard specifically addresses the determination of strength properties for adhesively bonded single-lap-shear joints utilizing rigid plastic adherends. It is intended to complement Test Methods D 1002 and D 3163, extending their application from metal-to-metal…

D3162-21 – Standard Test Method Technical Guide

This test method, designated as ASTM D3162-21, details the procedure for the continuous measurement of carbon monoxide (CO) in the atmosphere using Nondispersive Infrared Spectrometry (NDIR). This standard is a critical component of ambient air quality monitoring programs focused on…

D3163-01 – Standard Test Method Technical Guide

🧪 Scope and Application for Plastic Adherends ASTM D3163‑01 (Reapproved 2023) is a standard test method designed to complement Test Method D1002, extending its application to single‑lap shear adhesive joints of rigid plastic adherends under tension loading. The method provides…

D3160-20 – Standard Test Method Technical Guide

ASTM D3160-20a provides a reliable spectrophotometric method for quantifying phenol contamination in refined cumene (isopropylbenzene) and AMS (α–Methylstyrene). This test method is critical for quality control, as phenol can inhibit the chemical reactions these feedstocks undergo in downstream processing. 📐…

D3161 – Standard Test Method Technical Guide

📐 Scope and Applicable Products This test method, D3161/D3161M-20 (Reapproved 2025), evaluates the wind resistance of discontinuous, air permeable, steep slope roofing products. The resistance is due to rigidity, with or without sealant or mechanical interlocking. Products are applied to…

D3157-05 – Standard Test Method Technical Guide

🌐 Scope and Significance of Color Measurement ASTM D3157‑05 (Reapproved 2020) provides a standardized procedure for classifying the color of raw natural rubber using a defined color scale. The method relies on the visual comparison of a molded test specimen…

D3159-22 – Standard Test Method Technical Guide

📜 Scope and Application This specification covers molding and extrusion materials of modified ETFE fluoropolymer. The ETFE resin is a copolymer of ethylene and tetrafluoroethylene, with modified grades containing no more than 5 mole % of other fluoromonomers. It is…

D3155-11 – Standard Test Method Technical Guide

ASTM D3155-11, formally titled “Standard Test Method for Lime Content of Uncured Soil-Lime Mixtures,” is a standard procedure used extensively in geotechnical engineering and construction quality control. The method provides a reliable means to quantify the percentage of lime present…

D3156-96 – Standard Test Method Technical Guide

📐 Scope, Significance, and Application of D3156-96 ASTM D3156-96 (Reapproved 2021), titled “Standard Practice for Rubber—Chromatographic Analysis of Antidegradants (Antioxidants, Antiozonants and Stabilizers)”, provides a standardized framework for the detection and identification of these critical chemical agents in raw rubber…

D3154-14 – Standard Test Method Technical Guide

The ASTM D3154-14 (Reapproved 2023) standard, developed by Committee D22 on Air Quality, describes the standard test method for measuring average velocity in ducts using the Pitot tube method. This method is technically complex but is considered the most accurate…

D3152-72 – Standard Test Method Technical Guide

🔬 Scope and Summary of Test Method This test method, designated ASTM D3152 – 72 (Reapproved 2000), covers the determination of capillary-moisture properties of fine-textured soils. It specifically utilizes a pressure-membrane apparatus to establish the moisture content vs. moisture tension…