D3369-01 – Standard Test Method Technical Guide

📐 Product Classification and Dimensions This specification covers PTFE-fluorocarbon resin cast film with thicknesses from 0.025 to 0.127 mm (0.001 to 0.005 in). The film is classified as one type under Section 4. Length and width are subject to agreement…

D3370-18 – Standard Test Method Technical Guide

ASTM Standard D3370-18, “Standard Practices for Sampling Water from Flowing Process Streams,” is a critical document authorized by the U.S. Department of Defense and developed under the jurisdiction of ASTM Committee D19 on Water. It establishes standardized methods for extracting…

D3368-17 – Standard Test Method Technical Guide

ASTM D3368-17 (Reapproved 2022) covers the standard specification for unfilled, unpigmented FEP resin sheet and film with a thickness less than 3.175 mm (0.125 in.). The standard establishes a classification system based on material performance and intended use, allowing for…

D3366-18 – Standard Test Method Technical Guide

ASTM D3366-18 specifically covers the visual measurement of color in molten maleic anhydride on the Platinum-Cobalt (Pt-Co) scale (0–100 range). It requires testing a fresh melt prepared at 60°C and a second specimen after an accelerated aging period of 2…

D3367-21 – Standard Test Method Technical Guide

📐 Scope and Principles of the Test Method The ASTM D3367-21 standard establishes a definitive procedure for determining the plasticizer sorption of poly(vinyl chloride) (PVC) homopolymers under a controlled applied centrifugal force. This quantitative method is crucial for evaluating the…

D3363-22 – Standard Test Method Technical Guide

The ASTM D3363-22 standard describes a widely utilized, rapid screening method for evaluating the hardness of organic coating films through the use of standard drawing leads or pencils. Often referred to as the “pencil hardness test,” this method is essential…

D3364-99 – Standard Test Method Technical Guide

🧪 Standard Overview and Scope ASTM D3364-99 (Reapproved 2019) is a specialized extension of Test Method D1238, specifically designed for measuring the flow rates of poly(vinyl chloride) (PVC) compounds. This test method uniquely detects and controls the various polymer instabilities…

D3361 – Standard Test Method Technical Guide

📐 Scope and Significance of D3361/D3361M ASTM D3361/D3361M defines a standard practice for accelerating the exposure of paints and related coatings using an unfiltered open-flame carbon-arc device. This practice covers the selection of test conditions, preparation of test specimens, and…

D3362-05 – Standard Test Method Technical Guide

📐 Scope and Applicability of the Standard ASTM D3362-05 is a standardized gas chromatographic test method for determining the purity of commercially available acrylate esters. It specifically covers methyl acrylate, ethyl acrylate, n-butyl acrylate, and 2-ethylhexyl acrylate. The method simultaneously…

D3359-23 – Standard Test Method Technical Guide

ASTM D3359 – 23 outlines standard test methods for assessing the adhesion of relatively ductile coating films to metallic substrates. The procedure involves applying and removing pressure-sensitive tape over cuts made in the coating film. These test methods are designed…

D3360-96 – Standard Test Method Technical Guide

📐 Scope and Application This test method covers the determination of the particle-size distribution in the sub-sieve size range of common extender pigments such as aluminum silicate (kaolin clay), magnesium silicate (talc), calcium carbonate (calcite or dolomite or precipitated calcium…

D3353-18 – Standard Test Method Technical Guide

ASTM D3353 – 18 (Reapproved 2024) defines standard test methods for fibrous-insulated magnet wire. It covers fibers or fibrous-tape insulation served or wrapped helically over bare conductors or film-insulated substrates (D1676). These test methods are intended primarily for the evaluation…

D3354-21 – Standard Test Method Technical Guide

🧪 Scope and Summary This test method, D3354‑21, provides quantitative information on the blocking load of plastic film using the parallel plate method. Blocking refers to unwanted adhesion between layers of film. The test measures the force required to separate…

D3352-15 – Standard Test Method Technical Guide

📋 Overview and Applicability of D3352-15 ASTM D3352-15 provides a standard atomic absorption spectrophotometry (AAS) method for the determination of soluble strontium ion in brackish water, seawater, and brines. This test method is applicable for samples containing strontium concentrations ranging…

D3350-24 – Standard Test Method Technical Guide

📜 Scope and Application ASTM D3350-24 establishes a cell classification system for identifying polyethylene plastic pipe and fittings materials. The specification focuses on material identification and does not provide design engineering data or application suitability. It covers both base materials…

D3351-93 – Standard Test Method Technical Guide

The ASTM D3351-93 standard establishes a test method for quantifying the number of gels in plastic film. Gels, defined as nodules of oxidised or high-molecular-weight material, are objectionable due to their impact on film appearance and printability. This method uses…

D3348-12 – Standard Test Method Technical Guide

ASTM D3348-12 (Reapproved 2017) provides a standardized procedure for the rapid colorimetric determination of trace lead in unleaded gasoline. Designed specifically for field use by nontechnical personnel, this method leverages a chemical extraction reaction combined with a standard test kit…