ASTM D6496/D6496M-23a specifies the standard test method for determining the average bonding peel strength between the top and bottom layers of needle-punched geosynthetic clay liners (GCLs). This index test is essential for quality control of the manufacturing bonding process.
The test method (Section 1) covers the laboratory determination of the average bonding strength of a GCL. The standard requires values to be reported in SI or inch-pound units independently (Section 1.2). The method serves as an index test to evaluate the quality of the needle-punching bonding process (Section 5).