Category ASTM Standards

ASTM Standards Interpretation

D269-97 – Standard Test Method Technical Guide

📌 Scope and Significance This test method, designated D269-97 (Reapproved 2020), provides a standardized procedure for determining the amount of insoluble matter in rosin and rosin derivatives, as defined in Terminology D804. The values stated in SI units are regarded…

D2687-95 – Standard Test Method Technical Guide

🔍 Scope and Applicability of D2687-95 ASTM D2687-95 (Reapproved 2024) defines the standard practices for obtaining representative samples of particulate ion-exchange materials. The scope of this standard is divided into three core protocols based on the physical configuration of the…

D2688-23 – Standard Test Method Technical Guide

📐 Scope and Specimen Configuration ASTM D2688-23 provides a definitive gravimetric procedure for determining the corrosion rate of metals exposed to water systems under isothermal conditions, strictly excluding the variable of heat transfer. The method relies on exposing metal specimens…

D2686-19 – Standard Test Method Technical Guide

This specification, designated ASTM D2686-19, provides the standardized requirements for electrical insulating tape comprised of a polytetrafluoroethylene (PTFE) backing film coated on one side with a pressure-sensitive adhesive. This standard is similar to IEC 60454-3-14 and classifies tape products based…

D2684 – Standard Test Method Technical Guide

ASTM D2684/D2684M −24 provides a standardized framework for evaluating the permeability of thermoplastic containers. This test method is essential for ensuring that packaging maintains its integrity and prevents product loss during storage, specifically for packaged reagents or proprietary products under…

D2685-11 – Standard Test Method Technical Guide

📐 Test Method Overview This test method, designated ASTM D2685-11 (Reapproved 2019), provides a gas chromatographic procedure for the determination of air and carbon tetrafluoride (CF₄) as impurities in sulfur hexafluoride (SF₆). Air is defined as nitrogen, oxygen, or any…

D268-22 – Standard Test Method Technical Guide

ASTM D268-22 is a standard guide under the jurisdiction of ASTM Committee D01 on Paint and Related Coatings. Originally approved in 1927, it was last revised in 2022, replacing the previous version D268-01 (2012). This guide provides essential procedures for…

D2680-20 – Standard Test Method Technical Guide

📐 Scope and Application ASTM D2680-20 standardizes the specification for composite sewer piping made from Acrylonitrile-Butadiene-Styrene (ABS) and Poly(Vinyl Chloride) (PVC). This specification covers thermoplastic composite pipe, fittings, and joining systems designed for gravity flow, non-pressure sanitary sewer, and storm…

D2683-20 – Standard Test Method Technical Guide

ASTM D2683-20, originally approved in 1968 and revised in 2020, specifies requirements for socket-type polyethylene fittings for use with outside diameter-controlled polyethylene pipe and tubing. It ensures these fittings meet stringent criteria for materials, workmanship, dimensions, and pressure performance, making…

D2673-14 – Standard Test Method Technical Guide

📐 Scope and Key Specifications This specification, ASTM D2673-14 (Reapproved 2022), covers oriented polypropylene (OPP) film with a thickness range of 10 to 75 µm (0.4 to 3.0 mils). The film may include colorants, stabilizers, and other additives, and can…

D2674-72 – Standard Test Method Technical Guide

📐 Scope and Purpose of ASTM D2674-72 ASTM D2674-72 (Reapproved 2021) provides standardized methods for the chemical analysis of sulfochromate etch solutions used to prepare aluminum alloy surfaces for adhesive bonding. As the etchant reacts with aluminum, hexavalent chromium (Cr⁶⁺)…

D2671-21 – Standard Test Method Technical Guide

📐 Scope and Applicability of ASTM D2671-21 ASTM D2671-21 provides standard test methods for testing heat-shrinkable tubing used for electrical insulation. Materials covered include poly(vinyl chloride), polyolefins, fluorocarbon polymers, silicone rubber, and other plastic or elastomeric compounds. The values stated…