Category ASTM Standards

ASTM Standards Interpretation

D3617 – Standard Test Method Technical Guide

ASTM Standard D3617/D3617M – 17 (Reapproved 2022) provides a standardized guide for removing and analyzing specimens from built-up bituminous roof systems during the application process. The primary goal of this practice is to determine the approximate quantities of the roof…

D3618-05 – Standard Test Method Technical Guide

ASTM D3618−05 (Reapproved 2022) specifies a qualitative screening test to determine whether the solids in a paint contain more than 0.5% lead by weight. This method is widely used in the coatings industry for rapid compliance checks and quality assurance,…

D3616-95 – Standard Test Method Technical Guide

📐 Scope & Key Apparatus This test method, designated D3616 – 95 (2024), specifies procedures for determining the Dilute Solution Viscosity (DSV), gel characteristics, and swelling index of raw, non-oil-extended, and non-pigmented SBR (Styrene-Butadiene Rubber) and NBR (Acrylonitrile-Butadiene Rubber) polymers.…

D3613-98 – Standard Test Method Technical Guide

ASTM D3613–98 establishes the standard practice for sampling electrical insulating liquids with a viscosity less than 650 cSt at 40°C. Proper sampling is essential for accurate dissolved gas analysis (DGA) and water content determination, providing critical early indications of abnormal…

D3614-07 – Standard Test Method Technical Guide

🏛️ Scope and Organizational Framework ASTM D3614‑07 (Reapproved 2021) establishes essential criteria for the selection, evaluation, operation, and control of laboratory organisations engaged in the sampling and analysis of environmental atmospheres. The standard covers ambient air, workspace environments, source emissions,…

D3611-06 – Standard Test Method Technical Guide

This practice, designated ASTM D3611 – 06 (Reapproved 2019), provides a standardized environment for the accelerated aging of finished pressure-sensitive tape material. It is intended for use in conjunction with subsequent appearance or physical property tests, such as Test Methods…

D3612-02 – Standard Test Method Technical Guide

🧪 Scope and Applicability This standard, designated D3612 −02 (Reapproved 2017), specifies three procedures for the extraction and gas chromatographic measurement of dissolved gases in electrical insulating oils. It is applicable to oils having a viscosity of 20 cSt (100…

D3609-22 – Standard Test Method Technical Guide

ASTM D3609-22 establishes the standard practice for utilizing permeation tubes to dynamically calibrate instruments and analyzers used in measuring gas and vapor concentrations in atmospheric environments. As outlined in Section 1, this method is ideal for reactive and unstable substances,…

D3610-22 – Standard Test Method Technical Guide

📐 Scope and Application of D3610-22 ASTM D3610 – 22 is a standard test method specifically designed for the potentiometric determination of total cobalt in fresh alumina-base cobalt-molybdenum catalysts. The cobalt content is expressed as the oxide (Co₃O₄) and the…

D3608-19 – Standard Test Method Technical Guide

📋 Scope and Significance Overview The ASTM D3608-19 standard specifies the manual determination of combined nitrogen dioxide (NO₂) and nitric oxide (NO), expressed as total NOx, in the atmosphere using the Griess-Saltzman reaction. This test method covers a measurement range…

D3606-24 – Standard Test Method Technical Guide

📐 Scope and Applicability This test method, designated D3606-24a, provides a standardized gas chromatographic approach for quantifying benzene and toluene in finished motor and aviation spark ignition fuels. It encompasses two distinct procedures: Procedure A utilizing capillary column gas chromatography…

D3607-08 – Standard Test Method Technical Guide

ASTM D3607-08 (Reapproved 2016) provides a standardized procedure for the removal of volatile contaminants—specifically gasoline and water—from used engine oils prior to further analysis. This stripping process is essential for accurate subsequent testing of the oil’s mechanical and oxidative properties,…