admin

admin

D2674-72 – Standard Test Method Technical Guide

📐 Scope and Purpose of ASTM D2674-72 ASTM D2674-72 (Reapproved 2021) provides standardized methods for the chemical analysis of sulfochromate etch solutions used to prepare aluminum alloy surfaces for adhesive bonding. As the etchant reacts with aluminum, hexavalent chromium (Cr⁶⁺)…

D2671-21 – Standard Test Method Technical Guide

📐 Scope and Applicability of ASTM D2671-21 ASTM D2671-21 provides standard test methods for testing heat-shrinkable tubing used for electrical insulation. Materials covered include poly(vinyl chloride), polyolefins, fluorocarbon polymers, silicone rubber, and other plastic or elastomeric compounds. The values stated…

D2672-20 – Standard Test Method Technical Guide

📐 Scope and Referenced Documents This specification, designated D2672-20, covers the socket produced for solvent cement joints on both pressure and non-pressure IPS PVC pipe. It includes requirements for socket dimensions, burst pressure, and joint tightness tests of solvent cemented…

D267-82 – Standard Test Method Technical Guide

ASTM D267-82 (Reapproved 2020) provides the standard specification for gold bronze, pale gold bronze, and rich gold bronze powders used in decorative and protective coatings. These pigments, composed of finely polished metal flakes suspended in a lubricant, are designed to…

D2670-20 – Standard Test Method Technical Guide

📐 Test Apparatus and Specimen Configuration ASTM D2670-20 specifies the use of the Falex Pin and Vee Block Lubricant Test Machine for conducting a preliminary evaluation of the wear properties of fluid lubricants. The test geometry involves a rotating steel…

D2668-07 – Standard Test Method Technical Guide

ASTM D2668 −07 (Reapproved 2021) provides a standardized infrared absorption methodology for the quantitative determination of two key oxidation inhibitors—2,6-di-tert-butyl-p-cresol (DBPC) and 2,6-di-tert-butyl phenol (DBP)—in electrical insulating mineral oils. The method is effective for concentrations up to 0.5 % by…

D2669-16 – Standard Test Method Technical Guide

ASTM D2669-16, titled Standard Test Method for Apparent Viscosity of Petroleum Waxes Compounded with Additives (Hot Melts), provides a standardized procedure for determining the flow characteristics of hot melt adhesives and wax blends. This testing is critical for quality control…

D2666-96 – Standard Test Method Technical Guide

📐 Scope and Referenced Documents ASTM D2666-96a is an American National Standard that specifies requirements for polybutylene (PB) plastic tubing. The tubing is outside diameter controlled and produced in standard thermoplastic tubing dimension ratios. It is pressure rated for water…

D2667-95 – Standard Test Method Technical Guide

📖 Overview and Scope of D2667-95 ASTM D2667-95 (Reapproved 2008) is the standard test method for assessing the biodegradability of alkylbenzene sulfonates. This method acts as an index for the suitability of the sulfonate for general use as a surfactant,…

D2665-24 – Standard Test Method Technical Guide

ASTM D2665-24 is an American National Standard that specifies requirements for poly(vinyl chloride) (PVC) plastic drain, waste, and vent (DWV) pipe and fittings. It covers materials, dimensions and tolerances, pipe stiffness, crush resistance, impact resistance, and solvent cement properties. The…