🌻 Scope and Material Sourcing This specification (Designation D 3169 – 89, Reapproved 2001) defines the quality requirements for once-refined sunflower oil intended for use in protective coatings. The material must be derived exclusively from sunflower seeds and subjected to…
The ASTM D3167-10 (Reapproved 2017) standard specifically defines the Floating Roller Peel Resistance of Adhesives. This test method provides a robust means for determining the metal-to-metal peel strength of adhesive bonds, using a simple specimen preparation and testing procedure that…
📐 Specimen Configuration and Scope ASTM D3165 – 07 (Reapproved 2023) is formally designated as the Standard Test Method for Strength Properties of Adhesives in Shear by Tension Loading of Single-Lap-Joint Laminated Assemblies. This test method is intended for determining…
ASTM D3166-99 (Reapproved 2020) is a standardized test method used to evaluate the fatigue properties of adhesives in shear under tension loading, specifically for metal-to-metal bonded assemblies. This method provides critical data on the durability of adhesive joints under cyclic…
📐 Scope and Application of ASTM D3164 The ASTM D3164-03 (Reapproved 2017) standard provides a method for determining the strength properties of adhesively bonded plastic lap-shear sandwich joints in shear by tension loading. It is specifically designed to complement Test…
📐 Scope and Applicability The D3164M-03 standard specifically addresses the determination of strength properties for adhesively bonded single-lap-shear joints utilizing rigid plastic adherends. It is intended to complement Test Methods D 1002 and D 3163, extending their application from metal-to-metal…
This test method, designated as ASTM D3162-21, details the procedure for the continuous measurement of carbon monoxide (CO) in the atmosphere using Nondispersive Infrared Spectrometry (NDIR). This standard is a critical component of ambient air quality monitoring programs focused on…
🧪 Scope and Application for Plastic Adherends ASTM D3163‑01 (Reapproved 2023) is a standard test method designed to complement Test Method D1002, extending its application to single‑lap shear adhesive joints of rigid plastic adherends under tension loading. The method provides…
ASTM D3160-20a provides a reliable spectrophotometric method for quantifying phenol contamination in refined cumene (isopropylbenzene) and AMS (α–Methylstyrene). This test method is critical for quality control, as phenol can inhibit the chemical reactions these feedstocks undergo in downstream processing. 📐…
📐 Scope and Applicable Products This test method, D3161/D3161M-20 (Reapproved 2025), evaluates the wind resistance of discontinuous, air permeable, steep slope roofing products. The resistance is due to rigidity, with or without sealant or mechanical interlocking. Products are applied to…