IEC 62168 Symbol and Labels for Moisture-Sensitive Devices

IEC 62168 (based on JEDEC JEP113-B) defines the standard symbols, identification labels, and caution labels used globally to communicate moisture sensitivity levels for plastic-encapsulated surface-mount devices (SMDs). Proper labeling prevents catastrophic “popcorning” failures during solder reflow, where absorbed moisture vaporizes…