Standard Test Method D139-24, under the jurisdiction of ASTM Committee D04 on Road and Paving Materials, covers the float test for determining the consistency of asphalt materials. Values stated in SI units are regarded as standard. 📐 Apparatus and Specimen…
📐 Scope and Significance of the Acid Number Test Standard D1386-15 (Reapproved 2022) defines an empirical test method for determining the acid number of synthetic and natural waxes. The acid number, as defined in Section 3.1.1 of the standard, represents…
🧪 Test Principle and Scope of Application ASTM D1387‑89 (Reapproved 2019) standardizes the empirical determination of the saponification number for synthetic and natural waxes. This value is defined as the number of milligrams of potassium hydroxide (KOH) required to completely…
🧪 Standard Overview and Significance ASTM D1384‑24 provides a standard beaker‑type procedure for evaluating the effects of engine coolants on metal specimens under controlled laboratory conditions. This test method is designed to assess the corrosion‑inhibitive properties of coolant formulations by…
This standard under the designation D1385 –07 (Reapproved 2018) covers the colorimetric determination of hydrazine in water. The method is applicable to treated waters such as boiler feed and condensates. 📌 Scope and Application This test method covers the colorimetric…
📐 Apparatus and Material Specifications ASTM D1367-96 (Reapproved 2001) specifies a rigorous procedure for evaluating the abrasive properties of graphites intended for lubricating applications. The test method relies on a Graphite Lubricant Tester (ASTM Adjunct ADJD1367) which incorporates a bearing…
ASTM D1369-19 provides a standardized practice for determining the quantities of asphalt materials and aggregates required for constructing high-quality asphalt-aggregate surface treatments. This practice applies to both single and multiple surface treatments applied over prepared pavements or bases. The standard…
ASTM D1370/D1370M – 12 (Reapproved 2021) defines the standard test method for evaluating the contact compatibility between asphaltic materials, commonly known as the Oliensis Test. Primarily utilized in the roofing industry, this method assesses the interaction between saturants and coatings…
🔬 Test Method Scope and Core Chemistry ASTM D1364‑22 provides a definitive procedure for measuring water content in volatile solvents and chemical intermediates integral to the coatings industry (paints, varnishes, lacquers). The test method hinges on the Karl Fischer reaction,…
This standard practice, designated ASTM D1366-86 (Reapproved 2019), provides a standardized framework for reporting the fineness characteristics of pigments. Originally approved in 1955, it is under the jurisdiction of ASTM Subcommittee D01.31 on Pigment Specifications and has been approved for…
🔍 Test Overview and Significance This standard test method, D 1358–86, covers the spectrophotometric determination of diene value in dehydrated castor oil and its derivatives. During dehydration, ricinoleic acid forms either conjugated linoleic or normal linoleic fatty acid segments. The…
📐 Test Method Overview and Scope ASTM D1360 – 98 (Reapproved 2011), the “Standard Test Method for Fire Retardancy of Paints (Cabinet Method),” provides a quantitative laboratory procedure for assessing coating performance on wood substrates. The method specifically measures the…
📐 Scope and Purpose of the Permanganate Time Test The ASTM D1363-06 (Reapproved 2019) standard is a critical quality control method used to detect the presence of easily oxidizable impurities in acetone and methanol. As stated in Section 1.1 of…
📐 Scope and Structure of Terminology Standard D1356-20 ASTM D1356-20, officially titled Standard Terminology Relating to Sampling and Analysis of Atmospheres, establishes the definitive controlled vocabulary for ASTM Committee D22 on Air Quality. This standard centralizes critical definitions from dozens…
ASTM D1357-95 (Reapproved 2019) provides the foundational standard practice for planning the sampling of the ambient atmosphere. It outlines the broad concepts, critical uncontrollable variables, and rigorous statistical framework required to design a representative air quality monitoring program. Rather than…
ASTM D1352 – 02 establishes the standard specification for an ozone-resisting crosslinked rubber insulating compound whose polymer consists substantially of butyl rubber, intended for electrical wires and cables. This document defines the physical, electrical, and aging requirements necessary to ensure…
🔬 Scope and Significance of the Test Method ASTM D1353-13 (Reapproved 2021) establishes a standardized procedure for quantifying the nonvolatile matter (residue) present in volatile solvents intended for use in paints, varnishes, lacquers, and related coatings. This test is critical…