D3735-22 – Standard Test Method Technical Guide

📐 Scope and Classification ASTM D3735-22, under Committee D01 jurisdiction, specifies four types of VM&P naphthas: Type I (Regular), Type II (High Flash), Type III (Odorless), and Type IV (Low Aromatics). These are moderately volatile, mainly aliphatic hydrocarbon solvents used…

D3737-18 – Standard Test Method Technical Guide

The ASTM D3737-18 (Reapproved 2023) practice provides the standard framework for calculating allowable properties in structural glued laminated timber (glulam). This practice governs the derivation of design values needed for engineered wood construction, relying heavily on specific material grade arrangements…

D3734-05 – Standard Test Method Technical Guide

📐 Scope and Classification of High-Flash Aromatic Naphthas ASTM D3734 – 05 (Reapproved 2018), Standard Specification for High-Flash Aromatic Naphthas, provides the specification for aromatic hydrocarbon solvents that are high-flash, moderately low-volatility petroleum distillates. These solvents feature a distillation range…

D3732-23 – Standard Test Method Technical Guide

ASTM D3732−23 provides a standardized framework for reporting cure times of ultraviolet (UV)-cured coatings. The core of the standard defines a “cure” not by a single physical property, but by the condition of the coating as measured by end-use performance…

D3733-93 – Standard Test Method Technical Guide

🧪 Scope and Significance of ASTM D3733-93 ASTM D3733-93 (Reapproved 1998) establishes a standard test method for determining the silicon content of silicone polymers and silicone‑modified alkyds. This method is specifically applicable when silicon is present in the nonvolatile portion…

D3730-17 – Standard Test Method Technical Guide

ASTM D3730-17 (Reapproved 2022) is a standardized guide covering the selection and use of test methods for High-Performance Interior Architectural Wall Coatings (HIPAC). These coatings differ from conventional paints by being formulated to be tougher, more stain-resistant, and more abrasion-resistant,…

D3731-24 – Standard Test Method Technical Guide

🌿 Overview and Scope of Measurement Practices These practices encompass the extraction and measurement of chlorophyll a, b, and c, and pheophytin a in freshwater and marine plankton and periphyton. Three distinct practices are provided: spectrophotometric trichromatic, spectrophotometric monochromatic, and…

D3725-78 – Standard Test Method Technical Guide

🎯 Scope and Summary of the Test Method This test method, designated ASTM D3725-78 (Reapproved 1998), covers the semiquantitative determination by gas-liquid chromatography (GLC) of herring and menhaden fish oil when present in small quantities in other drying oils and…

D3728-08 – Standard Test Method Technical Guide

📋 Scope, Referenced Documents, and Key Test Methods ASTM D3728-08 (Reapproved 2012) specifically covers the requirements for 99% grade 2-Ethoxyethyl Acetate, a solvent widely used in paints, coatings, and chemical intermediate applications. The values stated in SI units are regarded…

D3723-22 – Standard Test Method Technical Guide

🧪 Scope and Significance of D3723-22 This standard test method outlines a reliable procedure for determining the pigment content of water-emulsion paints using low-temperature ashing. It is ideally suited for coatings where the pigment load consists of materials thermally stable…

D3724-01 – Standard Test Method Technical Guide

🧪 Composition and Chemical Requirements Standard D3724-01 (Reapproved 2019) specifies the requirements for synthetic brown iron oxide pigments used in paints and coatings. The pigment must be a manufactured iron oxide or a blend, produced via precipitation of iron salts,…

D3721-05 – Standard Test Method Technical Guide

📐 Scope and Composition Requirements ASTM D3721 – 05 (Reapproved 2019) specifies the requirements for synthetic red iron oxide pigment intended for use in paints and coatings. This standard is directly under the jurisdiction of ASTM Committee D01. The pigment…

D3722-05 – Standard Test Method Technical Guide

📜 Scope and Specifications This specification covers dry and wet ground naturally occurring iron oxide, dry and wet ground calcined naturally occurring iron oxide, and mixtures of these with synthetic iron oxides. These pigments are suitable for use in paints,…

D372-00 – Standard Test Method Technical Guide

📋 Classification and Types of Flexible Treated Sleeving ASTM D372-00 defines seven types of flexible treated sleeving for electrical insulation based on base fiber material and temperature index. These tubular products are made from woven textile fibers impregnated or coated…

D3720-90 – Standard Test Method Technical Guide

🧪 Scope and Summary of Test Method ASTM D3720‑90 (Reapproved 2019) establishes a standardized X‑ray diffraction (XRD) procedure for determining the ratio of anatase to rutile phases in titanium dioxide pigments. The method is applicable to single pigments, pigment mixtures,…

D3718-85 – Standard Test Method Technical Guide

ASTM D3718-85a (Reapproved 2022) specifies a standard test method for determining low concentrations of chromium in paint by atomic absorption spectroscopy. This method is applicable for chromium content in the range of 0.005% to 1.0% in the solids of liquid…

D3719-00 – Standard Test Method Technical Guide

ASTM D3719-00 establishes a standardized instrumental method for quantifying the degree of dirt collection on exposed coated exterior panels. The protocol relies on measuring color changes—specifically the reduction in lightness (L*) over a defined exposure period. This article provides a…