D586-23 – Standard Test Method Technical Guide

ASTM D586‑23, designated as the Standard Test Method for Ash and Organic Matter Content of Degradable Erosion Control Products, establishes the procedure for determining these properties by ignition at a specified high temperature.

📐 Scope and Significance of D586‑23

This test method (Section 1.1) covers the determination of the ash and organic matter contents of degradable Erosion Control Products (ECPs) by ignition at 900 ± 25°C. The test method is primarily used to satisfy specifications set forth by various agencies. According to Section 5.1 (Significance and Use), the ash content determined by this method may consist of various residues from chemicals