Standard D5224-12 (Reapproved 2019) defines the general principles for compression molding test specimens of thermosetting compounds such as phenolics, aminoplastics, melamine phenolics, epoxies, and unsaturated polyesters. Standardized conditions are vital for valid material comparisons.
Specimens are produced by loading a mold cavity with material, applying pressure at a