D4019-94 – Standard Test Method Technical Guide

🔬 Summary of Test Method and Scope

ASTM D 4019 – 94a defines a standard procedure for determining moisture in plastics using coulometric regeneration of phosphorus pentoxide (P₂O₅). The method is applicable for moisture contents