ASTM D3885-07a (Reapproved 2024), Standard Test Method for Abrasion Resistance of Textile Fabrics (Flexing and Abrasion Method), provides a standardized procedure for evaluating the resistance of woven and nonwoven fabrics to combined flexing and abrasive wear. Often referred to as the “Stoll Flex” test, this method simulates the dynamic strains experienced by textiles in demanding applications.
ASTM D3885 requires specimens to be cut to precise dimensions of 25 by 200 mm (1.0 by 8.0 in