D371-89 – Standard Test Method Technical Guide

📐 Product Types and Classifications

This specification covers asphalt roll roofing in sheet form, typically 36 in. (914 mm) wide, used as a cap sheet in built-up roofs. The material is classified into four types based on minimum mass per unit area.

🏷️ Type 📏 Min Mass (lb/100 ft²) 📐 Min Mass (g/m²)
I37.01806
II46.32260
III35.51733
IV42.82090

⚙️ Physical Requirements and Testing

The finished product must not crack or be sticky when unrolled at ambient temperatures above 50°F (10°C). Pliability at 77°F (25°