ASTM D3406-95 (Reapproved 2000) specifies an elastomeric-type, one-component, hot-applied joint sealant intended for sealing joints and cracks in Portland cement concrete (PCC) highway and airfield pavements. The material must be resistant to weathering and effectively seal against moisture and incompressibles throughout thermal expansion and contraction cycles.
The sealant must form a resilient and cohesive compound in place. It must not flow from