The ASTM D2729-21 standard specifies requirements for poly(vinyl chloride) (PVC) sewer pipe and fittings for non-pressure, gravity-flow drainage systems outside buildings. It covers materials, dimensions, workmanship, chemical resistance, and joint tightness for solid and perforated pipe.
Per Sections 1.1 and 4.1, D2729-21 specifically excludes these products from use as public or municipal collector sewers. The pipe is strictly intended for outside building drainage. Typical applications are grouped into standard and perforated categories:
| 🟦 Application Area | 📏 Pipe Type |
|---|---|
| Building sewers, underground drains | Standard |