These test methods provide direct-current procedures for measuring dc insulation resistance, volume resistance, and surface resistance of electrical insulating materials. The geometric dimensions of the specimen and electrodes are used to calculate volume and surface resistivity, as well as corresponding conductances and conductivities. For accurate results