ASTM D1708-18 defines the tensile testing of plastics using a standard microtensile “dog-bone” specimen. While superseded for general use by D638 (Type V specimen) or D882, it remains the standard for specific material specifications relying on a historical dataset derived from this geometry. The precisely machined reduced section ensures uniform stress concentration during testing.
| 🟦 Dimension | 📐 SI Value | 📏 Imperial Value |
|---|---|---|
📥 Standard Documents DownloadTrending now |