D1636-21 – Standard Test Method Technical Guide

The ASTM D1636-21 standard specifies the requirements for compression molding, thermosetting allyl compounds. This specification covers classification based on filler and resin composition, general requirements for uniformity, and references standard test methods for evaluation. The compounds are identified by type, class, and grade as outlined in Section 4.

📋 Classification of Allyl Molding Compounds

According to Section 4, compounds are classified into three types based on filler, with classes indicating resin composition and flame retardancy. The table below summarizes the classification.

🟦 Type 📏 Class 📐 Filler 🎯 Resin ⚡ Flame-Retardant 🌟 Grades per Class
IAGlassDAPNo4
IBGlassDAPYes4
ICGlassDMPNo4
IDGlassDMPYes4
IIAMineralDAPNo2
IIBMineralDAPYes2
IICMineralDMPNo2
IIDMineralDMPYes2
IIIASynthetic FiberDAPNo3

DAP: Diallyl ortho-phthalate; DMP: Diallyl meta