ASTM D1153-22 defines the specification for methyl isobutyl ketone (MIBK, 99.0 % grade), also known chemically as 2-methyl-4-pentanone. This standard is essential for ensuring quality in solvent applications, particularly within the paint, varnish, lacquer, and related coatings industries. The specification requires that all conformance determinations be made using the rounding-off method of Practice E29, applied “to the nearest unit” in the last significant digit. All property limits are expressed in SI units, and this standard is approved for use by agencies of the U.S. Department of Defense.
Methyl isobutyl ketone conforming to this specification must meet the following detailed property requirements. Each property is verified using a specific ASTM test method to ensure strict conformance.
| 🟦 Property | 🎯 Specification Limit | ⚡ Test Method |
|---|---|---|
| Purity (MIBK by GC) | 99.0 % min (by mass) | D3329 |
| Color | 15 max (Platinum-Cobalt Scale) | D1209 / D5386 |
| Distillation Range (Initial to Dry Point) | 114.0 °C – 117.0 °C | D1078 |
| Nonvolatile Matter | 5.0 mg / 100 mL max | D1353 |
| Water Content | 0.1 % max | D1364 |