Category ASTM Standards

ASTM Standards Interpretation

D2111-10 – Standard Test Method Technical Guide

ASTM D2111-10 (Reapproved 2020) defines standardized procedures for the determination of specific gravity and density specifically tailored for halogenated organic solvents and their admixtures. Developed by Committee D26 on Halogenated Organic Solvents and Fire Extinguishing Agents, this standard is essential…

D2109-01 – Standard Test Method Technical Guide

🧪 Standard Test Methods and Scope ASTM D2109‑01 (Reapproved 2022) defines five distinct procedures for quantifying nonvolatile matter in halogenated organic solvents and their admixtures. The appropriate method depends on the expected residue level, the required precision, and the physical…

D211-67 – Standard Test Method Technical Guide

🧪 Standard Coverage and Pigment Classification ASTM D211-67 (Reapproved 2023) specifies six distinct types of commercially pure lead chromate pigments. These are chemical precipitates consisting of normal or basic lead chromates, and the classification is strictly based on the pigment’s…

D2105-01 – Standard Test Method Technical Guide

📐 Scope and General Requirements This test method, designated D2105-01 (Reapproved 2019), covers the determination of the comparative longitudinal tensile properties of fiberglass pipe under defined conditions of pretreatment, temperature, and testing machine speed. Both Glass-Fiber-Reinforced Thermosetting-Resin Pipe (RTRP) and…

D2106-07 – Standard Test Method Technical Guide

🧪 Overview of Standard D2106-07 ASTM D2106-07 (Reapproved 2022) specifies standard test methods for determining the amine acid acceptance (alkalinity) of halogenated organic solvents. This test specifically quantifies the stabilizing capacity of titratable organic amines present in the solvent. It…

D2108-10 – Standard Test Method Technical Guide

🧪 Scope and Significance of Color Measurement The ASTM D2108-10 (Reapproved 2020) standard establishes a test method for the visual measurement of color in halogenated organic solvents and their admixtures. The measurement range for this method is strictly limited to…

D2103-23 – Standard Test Method Technical Guide

📐 Scope and Classification of Polyethylene Films ASTM D2103-23a is a comprehensive specification governing the classification of polyethylene film with a thickness up to 0.254 mm (0.010 in.). It covers films manufactured from virgin or recycled polyethylene resin, and may…

D2104-03 – Standard Test Method Technical Guide

The ASTM D2104-03 standard, formally designated as the Standard Specification for Polyethylene (PE) Plastic Pipe, Schedule 40, provides comprehensive requirements for PE piping systems utilizing insert fittings. This document establishes critical criteria for materials, dimensions, and performance, ensuring reliability in…

D2100 – Standard Test Method Technical Guide

📜 Scope, Terminology, and Classification Overview This specification, formally designated D2100/D2100M –95 (Reapproved 2017), covers asbestos textile materials explicitly intended for electrical insulating purposes. These materials must contain a minimum of 80% asbestos fiber by mass, excluding the mass of…

D2102-02 – Standard Test Method Technical Guide

ASTM D2102-02 (Reapproved 2018) provides a standardized procedure for determining the unrestrained shrinkage of a bundle of textile fibers. Applicable to both crimped and uncrimped fibers from tow, sliver, and yarns, this test method is essential for evaluating the dimensional…

D2099-14 – Standard Test Method Technical Guide

The ASTM D2099-14 (Reapproved 2023) standard specifies the test method for evaluating dynamic water resistance of shoe upper leather using the Maeser water penetration tester. This standard applies to all types of shoe upper leather except wet blue and measures…

D210-05 – Standard Test Method Technical Guide

🏭 Composition and Properties This specification covers the pigment commercially known as bone black, ivory black, or drop black. The dry pigment is manufactured by the calcination of bones and must be free from any admixture with other substances. It…