📄 BS ISO 5636 is the British Standard implementing the ISO 5636 series, which specifies methods for determining the air permeance of paper and board. Air permeance reflects the porosity of the fibre structure and is directly related to the breathability and filtration function of bags, cigarette paper, filter paper and packaging paper; it is also used to assess formation and structural uniformity. Parts 3 to 6 of the series give several methods based on different principles for the medium range of air permeance.
💡 The same sample gives different numeric results by different methods (Bendtsen, Sheffield, Gurley), with different units and ranges. The method must be matched to the paper grade, permeance level and upstream/downstream standard agreement, and must be stated in the report.
1. Series Overview and Scope 📌
The BS ISO 5636 series provides several methods for medium-range air permeance determination:
- Part 3 (Bendtsen method): a constant-pressure air stream passes through a defined sample area; permeance is expressed as flow rate (mL/min).
- Part 4 (Sheffield method): measures air flow rate at a defined pressure difference and expresses permeance in Sheffield units.
- Part 5 (Gurley method): measures the time for a defined volume of air to pass through the sample (Gurley seconds).
The methods differ in principle, apparatus and result expression, and suit different permeance levels of paper grades.
2. Series Structure and Key Points 📋
The series comprises four documents; the core readable parts are ISO 5636-3, 4 and 5, while Part 6 is a scanned version summarised here from public domain knowledge.
| Standard | Title | Main Content | Status |
| BS ISO 5636-3:2013 | Air permeance — Bendtsen method | Constant-pressure flow, permeance as flow rate | Readable |
| BS ISO 5636-4:2013 | Air permeance — Sheffield method | Flow rate at pressure difference, Sheffield units | Readable |
| BS ISO 5636-5:2013 | Air permeance — Gurley method | Time for a defined air volume (Gurley seconds) | Readable |
| BS ISO 5636-6:2015 | (Related permeance method, scanned) | Summarised from public domain knowledge | Scan |
⚠️ Part 6 of this series is a scanned version; the related technical content here is written from public domain knowledge. Consult the official BSI publication for clause details.
3. Key Technical Requirements 🔬
3.1 Principle and apparatus
Each method specifies the measuring principle, apparatus construction (pressure head, sample clamp, flow/time measuring device) and key dimensions. The Bendtsen method measures flow at constant pressure; the Sheffield method measures flow at a fixed pressure difference; the Gurley method records the time for a fixed air volume.
3.2 Sampling, conditioning and specimen preparation
The Standard specifies sampling, conditioning (standard temperature/humidity) and specimen preparation so specimens are in a consistent state. Paper moisture affects fibre porosity and permeance, so conditioning must be unified.
3.3 Result expression and conversion
Each method gives calculation and expression of results (flow, Sheffield units or Gurley seconds), with calibration and reference samples to ensure instrument accuracy. Conversion between methods requires the standard or reference samples.
🚨 Permeance results are sensitive to specimen clamping seal, pressure-difference setting and conditioning state. Poor clamping leaks, unstable pressure or incorrect conditioning distort the data — operate strictly per the Standard and calibrate the instrument regularly with reference samples.
4. Engineering Practice and Application 🛠️
- 🔍 Method matching: cigarette paper and filter paper (high permeance) often use the Gurley or Bendtsen method; packaging paper and light board often use Sheffield or Bendtsen. Choose by paper grade and supply agreement.
- 🔧 Quality control: permeance is a sensitive indicator of formation and structural uniformity, used for online and dispatch quality monitoring; abnormal variation suggests stock or forming problems.
- 📊 Functional evaluation: for filter, packaging and printing papers, combine permeance with pore size and ink absorption to evaluate function.
- 📋 Traceability: calibrate regularly with traceable reference samples, and retain instrument calibration records and test data.
4.4 Calibration, interlaboratory comparison and data management
Each permeance method is sensitive to instrument condition: pressure sensors, flow meters and timers drift with time, so calibrate regularly with traceable reference samples and join interlaboratory comparisons. Calibration reveals systematic deviation; comparison verifies consistent execution of the method. For production control, keep the method, operators and conditions fixed for longitudinal comparability; in release records note the method, conditioning and environment so abnormal variation can be traced. For exacting grades such as filter and cigarette paper, combine permeance with pore size and thickness rather than relying on a single indicator.
5. Frequently Asked Questions ❓
❓ Q: Why does the same sample give different values by different methods?
A: The methods differ in principle, pressure difference, sample area and unit (mL/min, Sheffield units, Gurley seconds); values are not directly comparable and need conversion by method and reference sample.
❓ Q: What is the significance of permeance for paper quality?
A: Permeance reflects pore structure and formation, affecting bag breathability, cigarette paper burn, filter paper filtration efficiency and printing ink absorption.
❓ Q: Why condition before testing?
A: Paper moisture varies with environment and affects fibre structure and pores; conditioning to a standard state (e.g. 23 °C/50 %RH) makes results comparable and reproducible.
🔍 Q: How to choose between Gurley and Bendtsen?
A: Gurley suits low permeance (dense paper); Bendtsen suits higher permeance (open paper, cigarette paper). Choose by paper grade and upstream/downstream standard.