This review covers Batch 6 of the BS ISO single-file series, bringing together 150 independent International Standards (ISO) from BS ISO 8588 to BS ISO 10204. The batch spans quality management, road-vehicle dynamics, earth-moving machinery, aerospace, cranes, optics and photonics, iron-ore chemical analysis, water quality, ski equipment, hydraulic cylinders, essential oils and information and documentation.
This batch covers the continuous range BS ISO 8588 to BS ISO 10204. Clusters: 8588–8957 belong to sensory analysis, road-surface profiles, pallet loads, aerospace fluid vocabulary, GRP pipes, earth-moving machinery, plastics, air quality, mould tools, human biodynamics, ships, contamination monitoring, pneumatics, alpine skis, pulp microbiology, earth-moving machinery, aerospace solid-state remote power controllers, surgical implants, road-vehicle alternators, hard-coal froth flotation and essential oils; 8967–9138 belong to essential oils, carbon black, LNG sampling, dried milk, interior lighting, uranium, industrial wire cloth, nonwovens, stationary emissions, tyre rolling circumference, open-channel flow, brake fluids, motorcycles and abrasive grains; 9145–9336 belong to aerospace bolts, fuel gases, press dies, pulp chlorides, hydraulic motors, chain-saw noise, optical coatings, electromagnetic flow, earth-moving engines, gas-adsorption BET, abrasive sieving, zinc oxide and optical transfer function; 9344–9622 belong to microscope eyepieces, ductile iron, plastics wear, imaging glare, banking telecommunication, thermoplastic valves, textile floor coverings, tyre valves, ski bindings, high-strength cast steel, iron-ore water-soluble chloride, ski boots, earth-moving machinery, synchronous-belt conductivity, sulfide concentrates, aerospace nuts, acoustics and milk infrared spectroscopy; 9628–9869 belong to rolling bearings, metallic wire, aircraft tow bars, containers, direct-reduced iron, water quality, orthopaedic instruments, EDIFACT, drills, cellular-plastics burning, robot motion nomenclature, gas cylinders, road vehicles, hydrometry, building performance, essential oils, thermal insulation and ships; 9876–10204 belong to agricultural irrigation valves, crane training, crane manuals, aerospace hydraulic oil, crane information labels, connections, belt drives, composition cork, quality management, diesel smoke, hand-arm vibration, coal flocculants, hydraulic cylinder acceptance, environmental tests, plastic strain ratio, tarragon oil, reinforcement braided sleeves, plain bearings, aluminium-production carbon, stationary emissions, health informatics, interlibrary loan, tobacco vocabulary and iron-ore calcium/magnesium.
This batch has several large clusters. Quality management (10002, 10004, 10005, 10007, 10008, 10014, 10018) covers customer-complaint handling, customer-satisfaction monitoring, quality plans, configuration management, B2C e-commerce, financial and economic benefits, and people involvement and competence. Road vehicles (8854, 8855, 8856, 9128, 9129, 9815) covers alternators, vehicle-dynamics vocabulary, starter motors, brake-fluid symbols, moments of inertia and lateral stability. Earth-moving machinery (8643, 8811, 8812, 9249, 9533) covers backhoe-loader lowering devices, rollers, terminology, engine net power and travel alarms. Aerospace (8625-4, 8816, 9154, 9206, 9609, 9618, 9667, 9940) covers fluid vocabulary, solid-state remote power controllers, nickel-alloy bolts, constant-displacement hydraulic motors, hexagon nuts, tow bars and phosphate-ester hydraulic oil. Cranes (9926-3, 9928-1, 9942-1) covers tower-crane operator training, crane operating manuals and information labels. Optics and photonics (9211-4, 9334, 9335, 9336-1, 9358, 10109) covers optical coatings, optical transfer function, imaging glare and environmental-test selection. Iron-ore chemical analysis (9517, 9599, 9686, 10203, 10204) covers water-soluble chloride, moisture, direct-reduced iron C/S, calcium and magnesium.
BS ISO 10002:2014 provides guidance for handling customer complaints, a supporting standard for customer satisfaction within the ISO 9000 family. It specifies complaint-handling policy, receipt and recording, classification and investigation, decision and reply, feedback and notification, and complaint-handling personnel and confidentiality requirements, covering the complaint-handling process and improvement to help organisations enhance customer satisfaction and trust.
BS ISO 8855:2011 defines the vocabulary of road-vehicle dynamics and road-holding ability, the common terminology basis for vehicle-dynamics testing and simulation. It defines vehicle coordinate systems, centre of mass, wheelbase, track, slip angle, steering angle, understeer/oversteer, lateral acceleration and yaw rate, widely used in handling tests (e.g. ISO 4138, 7401) and chassis tuning.
BS ISO 9277:2010 specifies the gas-adsorption BET method for determining the specific surface area of solids, a fundamental standard in materials science and powder engineering. It specifies nitrogen adsorption, single-point and multi-point BET equations, relative pressure range, adsorption cross-sectional area and surface-area calculation — used to characterise catalysts, adsorbents, nanomaterials, cement and ceramic powders.
BS ISO 10086-2:2004 specifies a method for evaluating flocculants as filter aids in rotary vacuum filters for coal preparation, a key standard for selecting coal-slurry water-treatment reagents. It specifies flocculant preparation, slurry suspension preparation, filter-test apparatus, cake moisture and filtrate-turbidity evaluation — used by coal-preparation plants for flocculant procurement and performance evaluation.
BS ISO 10113:2006 specifies the determination of the plastic strain ratio (r-value, anisotropy index) of metallic sheet and strip, a base standard for evaluating the formability of automotive stamping steel. It specifies uniaxial tensile testing, longitudinal/transverse/45° sampling, width and thickness strain measurement at a specified strain, and r-value and Δr calculation — used to evaluate deep-drawing performance and formability.
This batch supports practice across many fields. Quality management uses 10002, 10005 and 10007 for complaint handling, quality plans and configuration management; vehicle engineering uses 8855 and 9815 for handling and lateral-stability tests; materials characterisation uses 9277 for surface area and 10113 for stamping-steel formability; coal preparation uses 10086-2 for flocculant evaluation; optical design uses 9334–9336 for lens transfer function; water environment uses 9696, 9697 and 10200 for activity monitoring; mining uses 9517, 9599 and 10203 for iron-ore chemical analysis; hydraulic systems use 10100 for cylinder acceptance tests; health informatics uses 10159 for web-access manifests; cranes use 9928-1 for operating manuals. Users should follow the current official BSI edition.
The table below lists all 150 single-file BS ISO standards in this batch, in numerical order, with standard number and title.
| Standard | Title |
|---|---|
| BS ISO 08588:2017 | S e n s o r y a n a l y s i s M e t h o d o l o g y A n o t A t e s t B S I S O B S I S t a n d a r d s P u b l i c a t i o n N a t i o n a l f o re w o rd T h i s B r i t i s h S t a n d a r d i s t h e U K i m p l e m e n t a t i o n o f I S O I t s u p e r s e d e s B S w h i c h i s w i t h d r a w n T h e U K p a r t i c i p a t i o n i n i t s p r e p a r a t i o n w a s e n t r u s t e d t o T e c h n i c a l C o m m i t t e e A W S e n s o r y a n a l y s i s A l i s t o f o r g a n i z a t i o n s r e p r e s e n t e d o n t h i s c o m m i t t e e c a n b e o b t a i n e d o n r e q u e s t t o i t s s e c r e t a r y T h i s p u b l i c a t i o n d o e s n o t p u r p o r t t o i n c l u d e a l l t h e n e c e s s a r y p r o v i s i o n s o f a c o n t r a c t U s e r s a r e r e s p o n s i b l e f o r i t s c o r r e c t a p p l i c a t i o n T h e B r i t i s h S t a n d a r d s I n s t i t u t i o n P u b l i s h e d b y B S I S t a n d a r d s L i m i t e d I S B N I C S C o m p l i a n c e w i t h a B r i t i s h S t a n d a r d c a n n o t c o n f e r i m m u n i t y f r o m l e g a l o b l i g a t i o n s T h i s B r i t i s h S t a n d a r d w a s p u b l i s h e d u n d e r t h e a u t h o r i t y o f t h e S t a n d a r d s P o l i c y a n d S t r a t e g y C o m m i t t e e o n J u l y A m e n d m e n t s / c o r r i g e n d a i s s u e d s i n c e p u b l i c a t i o n D a t e T e x t a f f e c t e d B RI T I S H S T A N D A RD B S I S O I S O S e n s o r y a n a l ys i s M e t h o d o l o g y A n o t A t e s t A n a ly se se n so r ie lle M t h o d o lo g ie E ssa i A n o n A I N T E R N A T I O N A L S T A N D A R D I S O S e c o n d e d i ti o n R e f e r e n c e n u m b e r I S O E B S I S O I S O E i i I S O A l l r i gh ts re s e r v e d C O P YRI G H T P R O T E C T E D D O C U M E N T I S O P u b l i s h e d i n S w i t z e r l a n d A l l r i g h ts r e s e r v e d U n l e s s o th e r w i s e s p e c i f i e d n o p a r t o f th i s p u b l i c a ti o n m a y b e r e p r o d u c e d o r u ti l i z e d o th e r w i s e i n a n y f o r m o r b y a n y m e a n s e l e c t r o n i c o r m e c h a n i c a l i n c l u d i n g p h o t o c o p yi n g o r p o s ti n g o n th e i n t e r n e t o r a n i n tra n e t w i t h o u t p r i o r wr i tt e n p e r m i s s i o n P e r m i s s i o n c a n b e re q u e s t e d f ro m e i t h e r I S O a t th e a d d r e s s b e l o w o r I S O s m e m b e r b o d y i n th e c o u n t r y o f t h e r e q u e s t e r I S O c o p yr i g h t o f f i c e C h d e B l a n d o n n e t C P C H V e r n i e r G e n e v a S w i tz e r l a n d T e l Fa x c o p yr i g h i s o o r g www i s o o r g B S I S O I S O E F o re w o rd |
| BS ISO 08608:2016 | BS ISO 8608:2016 Mechanical vibration — Road surface profiles — Reporting of measured data |
| BS ISO 08611-3:2011 | BS ISO 8611-3:2011 Pallets for materials handling Part 3: Maximum working loads |
| BS ISO 08622:1998 | BS ISO 08622 |
| BS ISO 08625-4:2011 | BS ISO 8625-4:2011 Aerospace — Fluid systems — Vocabulary Part 4: General terms and definitions relating to control/actuation systems |
| BS ISO 08639:2016 | BS ISO 8639:2016 Glass-reinforced thermosetting plastics (GRP) pipes and fittings — Test methods for leaktightness and proof of structural design of flexible joints |
| BS ISO 08643:2017 | BS ISO 8643:2017 Earth-moving machinery backhoe loader lowering control device — Requirements and tests |
| BS ISO 08660:2002 | BS ISO Plastics — Determination of permanganate absorption number of caprolactam — Spectrometric method |
| BS ISO 08672:2014 | BS ISO 8672:2014 Air quality — Determination of the number concentration of airborne inorganic fibres by phase contrast optical microscopy — Membrane filter method |
| BS ISO 08693:2011 | BS ISO 8693:2011 Tools for moulding — Flat ejector pins |
| BS ISO 08694:2011 | BS ISO 8694:2011 Tools for moulding — Shouldered ejector pins |
| BS ISO 08695:2010 | BS ISO 8695:2010 Tools for pressing — Punches terminology |
| BS ISO 08697:1999 | BS ISO 08697 |
| BS ISO 08710:2010 | BS ISO 08710 |
| BS ISO 08727:1997 | BS ISO Mechanical vibration and shock — Human exposure — Biodynamic coordinate systems BS ISO A1:2015 Amendments/corrigenda issued since publication Date Comments Implementation of ISO amendment 1:2015 |
| BS ISO 08728:2014 | BS ISO 8728:2014 Ships and marine technology |
| BS ISO 08769:2016 | BS ISO 8769:2016 Reference sources — Calibration of surface contamination monitors — Alpha-, beta- and photon emitters |
| BS ISO 08778:2003 | BS ISO Pneumatic fluid power — Standard reference atmosphere |
| BS ISO 08779:2010 | BS ISO 08779 |
| BS ISO 08783:2015 | BS ISO 8783:2015 Alpine skis — Guidelines for conducting slope performance tests |
| BS ISO 08784-1:2014 | BS ISO 8784-1:2014 Pulp, paper and board — Microbiological examination Part 1: Enumeration of bacteria and bacterial spores based on disintegration |
| BS ISO 08811:2000 | BS ISO 8811:2000 Earth-moving machinery — Rollers and landfill compactors specifications |
| BS ISO 08812:2016 | BS ISO 8812:2016 Earth-moving machinery Terminology and commercial specifications |
| BS ISO 08816:1993 | General requirements UDC 629.7.064.5:621.316.57 BS ISO 8816:1993 Aircraft – Solid-state remote power controllers |
| BS ISO 08828:2014 | BS ISO 8828:2014 Implants for surgery — Guidance on care and handling of orthopaedic implants |
| BS ISO 08829-1:2009 | BS ISO 08829 |
| BS ISO 08843:2005 | BS ISO 08843 |
| BS ISO 08854:2012 | BS ISO 8854:2012 Road vehicles — Alternators with regulators — Test methods and general requirements |
| BS ISO 08855:2011 | BS ISO 8855:2011 Road vehicles — Vehicle dynamics and road-holding ability — Vocabulary |
| BS ISO 08856:2014 | BS ISO 8856:2014 Road vehicles — Electrical performance of starter motors requirements |
| BS ISO 08858-3:2004 | BS ISO Hard coal — Froth flotation testing — Part 3: Release evaluation |
| BS ISO 08896:2016 | BS ISO 8896:2016 Essential oil of caraway (Carum carvi L.) |
| BS ISO 08897:2010 | BS ISO 08897 |
| BS ISO 08899:2003 | BS ISO Oil of lemon petitgrain |
| BS ISO 08900:2005 | EHUJDPLD 5LVVR HW Confirmed May 2009 LQWHUHVWV LQIRUPHG PRQLWRU UHODWHG LQWHUQDWLRQDO DQG (XURSHDQ GHYHORSPHQWV DQG BS ISO 8900:2005 LL LLL G |
| BS ISO 08902:2009 | BS ISO 08902 |
| BS ISO 08942:2010 | BS ISO 8942:2010 Rubber compounding ingredients — Carbon black — Determination of individual pellet crushing strength |
| BS ISO 08943:2007 | BS ISO Refrigerated light hydrocarbon fluids — Sampling of liquefied natural gas — Continuous and intermittent methods |
| BS ISO 08967:2005 | BS ISO Dried milk and dried milk products — Determination of bulk density |
| BS ISO 08995:2002 | BS ISO Lighting of indoor work places |
| BS ISO 09000-2:1997 | BS ISO 09000 |
| BS ISO 09005:2007 | BS ISO 9005:2007 Nuclear energy — Uranium dioxide powder and sintered pellets — Determination of oxygen/uranium atomic ratio by the amperometric method |
| BS ISO 09044:2016 | BS ISO 9044:2016 Industrial woven wire cloth tests |
| BS ISO 09057:1991 | BS ISO 09057 |
| BS ISO 09073-11:2002 | BS ISO Textiles — Test methods for nonwovens — Part 11: Run-off |
| BS ISO 09096:2003 | BS ISO Stationary source emissions — Manual determination of mass concentration of particulate matter |
| BS ISO 09112:2008 | BS ISO Truck and bus tyres — Methods of measuring tyre rolling circumference — Loaded new tyres |
| BS ISO 09123:2001 | BS ISO Measurement of liquid flow in open channels — Stage-fall-discharge relationships |
| BS ISO 09128:2006 | BS ISO Road vehicles — Graphical symbols to designate brake fluid types |
| BS ISO 09129:2008 | BS ISO Motorcycles — Measurement methods for moments of inertia |
| BS ISO 09138:2015 | BS ISO 9138:2015 Abrasive grains — Sampling and splitting |
| BS ISO 09154:2016 | BS ISO 9154:2016 Aerospace — Bolts, with MJ threads, made of heat-resistant nickel-based alloy, strength class 1 550 MPa — Procurement specification |
| BS ISO 09162:2013 | BS ISO 9162:2013 Petroleum products — Fuels gases — Specifications |
| BS ISO 09183-2:2011 | BS ISO 9183-2:2011 Tools for pressing — Wear plates for press dies Part 2: Type B |
| BS ISO 09197:2016 | BS ISO 9197:2016 Paper, board and pulps — Determination of water-soluble chlorides |
| BS ISO 09206:2016 | BS ISO 9206:2016 Aerospace series — Constant displacement hydraulic motors |
| BS ISO 09207:1995 | BS ISO Implementation of ISO 9207:1995 Manually portable chain-saws with internal combustion engine — Determination of sound power levels — Engineering method |
| BS ISO 09211-4:2012 | BS ISO 9211-4:2012 Optics and photonics — Optical coatings Part 4: Specific test methods |
| BS ISO 09213:2004 | BS ISO Measurement of total discharge in open channels — Electromagnetic method using a full-channel-width coil |
| BS ISO 09244:2008 | BS ISO 09244 |
| BS ISO 09249:2007 | BS ISO 9249:2007 Earth-moving machinery — Engine test code — Net power |
| BS ISO 09277:2010 | BS ISO 9277:2010 Determination of the specific surface area of solids by gas adsorption — BET method |
| BS ISO 09284:2013 | BS ISO 9284:2013 Abrasive grains — Test-sieving machines |
| BS ISO 09286:1997 | BS ISO 09286 |
| BS ISO 09298:2017 | BS ISO 9298:2017 Rubber compounding ingredients — Zinc oxide — Test methods |
| BS ISO 09334:2012 | BS ISO 9334:2012 Optics and photonics — Optical transfer function — Definitions and mathematical relationships |
| BS ISO 09335:2012 | BS ISO 9335:2012 Optics and photonics — Optical transfer function — Principles and procedures of measurement |
| BS ISO 09336-1:2010 | BS ISO 9336-1:2010 Optics and photonics — Optical transfer function — Application Part 1: Interchangeable lenses for 35 mm still cameras |
| BS ISO 09344:2016 | BS ISO 9344:2016 Microscopes — Graticules for eyepieces |
| BS ISO 09349:2017 | BS ISO 9349:2017 Ductile iron pipes, fittings, accessories and their joints — Thermal preinsulated products |
| BS ISO 09352:2012 | BS ISO 9352:2012 Plastics — Determination of resistance to wear by abrasive wheels |
| BS ISO 09358:1994 | BS ISO Implementation of ISO 9358:1994 Optics and optical instruments — Veiling glare of image-forming systems — Definitions and methods of measurement |
| BS ISO 09362:2014 | BS ISO 9362:2014 Banking — Banking telecommunication messages |
| BS ISO 09393-1:2004 | BS ISO Thermoplastics valves for industrial applications — Pressure test methods and requirements — Part 1: General |
| BS ISO 09403:2000 | BS ISO 09403 |
| BS ISO 09405:2015 | BS ISO 9405:2015 Textile floor coverings — Assessment of changes in appearance |
| BS ISO 09413:2012 | Tyre valves — Dimensions and designation |
| BS ISO 09416:2009 | BS ISO 09416 |
| BS ISO 09462:2014 | BS ISO 9462:2014 Alpine ski-bindings — Requirements and test methods |
| BS ISO 09465:2012 | BS ISO 9465:2012 Alpine ski-bindings — Lateral release under impact loading |
| BS ISO 09477:2015 | BS ISO 9477:2015 High strength cast steels for general engineering and structural purposes |
| BS ISO 09517:2007 | BS ISO Iron ores — Determination of water-soluble chloride — Ion-selective electrode method |
| BS ISO 09523:2015 | BS ISO 9523:2015 Touring ski-boots for adults bindings — Requirements and test methods |
| BS ISO 09533:2010 | BS ISO 9533:2010 Earth-moving machinery — Machine-mounted audible travel alarms and forward horns — Test methods and performance criteria |
| BS ISO 09563:2015 | BS ISO 9563:2015 Belt drives — Electrical conductivity of antistatic endless synchronous belts — Characteristics and test method |
| BS ISO 09568:1993 | BS ISO 09568 |
| BS ISO 09599:2015 | BS ISO 9599:2015 Copper, lead, zinc and nickel sulfide concentrates — Determination of hygroscopic moisture content of the analysis sample — Gravimetric method |
| BS ISO 09609:2016 | BS ISO 9609:2016 Aerospace — Nuts, hexagonal, plain, reduced height, normal across flats, with MJ threads, classifications: Dimensions |
| BS ISO 09611:1996 | BS ISO Implementation of ISO 9611:1996 Acoustics — Characterization of sources of structure-borne sound with respect to sound radiation from connected structures — Measurement of velocity at the contact points of machinery when resiliently mounted |
| BS ISO 09618:2016 | BS ISO 9618:2016 Aerospace — Nuts, hexagonal, slotted (castellated), reduced height, normal across flats, with MJ threads, classifications: 450 MPa (at ambient Dimensions |
| BS ISO 09622:2013 | BS ISO 9622:2013 Milk and liquid milk products application of mid-infrared spectrometry |
| BS ISO 09628:2006 | BS ISO Rolling bearings — Insert bearings and eccentric locking collars — Boundary dimensions and tolerances February 2007 |
| BS ISO 09644:2008 | BS ISO 09644 |
| BS ISO 09649:2016 | BS ISO 9649:2016 Metallic materials — Wire — Reverse torsion test |
| BS ISO 09650-3:2009 | BS ISO 09650 |
| BS ISO 09667:2016 | BS ISO 9667:2016 Aircraft ground support equipment — Tow bars |
| BS ISO 09669:1990 | BS ISO Amendment 1:1992) Implementation of ISO 9669:1990 Series 1 freight containers — Interface connections for tank containers UDC 621.869.88:621.642.06:621.643.412 |
| BS ISO 09686:2006 | BS ISO Direct reduced iron — Determination of carbon and/or sulfur — High-frequency combustion method with infrared measurement |
| BS ISO 09696:2007 | BS ISO Water quality — Measurement of gross alpha activity in non-saline water — Thick source method |
| BS ISO 09697:2015 | BS ISO 9697:2015 Water quality — Gross beta activity in non-saline water — Test method using thick source |
| BS ISO 09707:2008 | BS ISO 09707 |
| BS ISO 09714-1:2012 | BS ISO 9714-1:2012 Orthopaedic drilling instruments Part 1: Drill bits, taps and countersink cutters |
| BS ISO 09735-10:2014 | BS ISO 9735-10:2014 Electronic data interchange for administration, commerce and transport (EDIFACT) — Application level syntax rules Syntax release number: 2) Part 10: Syntax service directories |
| BS ISO 09766:2012 | BS ISO 9766:2012 Drills with indexable inserts parallel flat |
| BS ISO 09772:2012 | BS ISO 9772:2012 Cellular plastics — Determination of horizontal burning characteristics of small specimens subjected to a small flame |
| BS ISO 09787:2013 | BS ISO 9787:2013 Robots and robotic devices motion nomenclatures |
| BS ISO 09809-4:2014 | BS ISO 9809-4:2014 Gas cylinders — Refillable seamless steel gas cylinders testing Part 4: Stainless steel cylinders with an Rm value of less than 1 100 MPa |
| BS ISO 09815:2010 | BS ISO 9815:2010 Road vehicles — Passenger- car and trailer combinations — Lateral stability test |
| BS ISO 09825:2005 | BS ISO amendment no. 1 Hydrometry — Field measurement of discharge in large rivers and rivers in flood |
| BS ISO 09836:2011 | Performance standards in building — Definition and calculation of area and space indicators BS ISO 9836:2011 January 2013 |
| BS ISO 09838:2015 | BS ISO 9838:2015 Alpine and touring ski-bindings tests |
| BS ISO 09841:2013 | BS ISO 9841:2013 Essential oil of hyssop officinalis) |
| BS ISO 09843:2002 | BS ISO Oil of cedarwood, Chinese type Endlicher) |
| BS ISO 09844:2006 | BS ISO Oil of bitter orange |
| BS ISO 09849:2000 | BS ISO 09849 |
| BS ISO 09869-1:2014 | BS ISO 9869-1:2014 Thermal insulation — Building elements — In- situ measurement of thermal resistance and thermal transmittance Part 1: Heat flow meter method |
| BS ISO 09876:2015 | BS ISO 9876:2015 Ships and marine technology for meteorological charts |
| BS ISO 09911:2006 | BS ISO Agricultural irrigation equipment — Manually operated small plastics valves |
| BS ISO 09926-3:2016 | BS ISO 9926-3:2016 Cranes — Training of operators Part 3: Tower cranes |
| BS ISO 09928-1:2015 | BS ISO 9928-1:2015 Cranes — Crane operating manual Part 1: General |
| BS ISO 09940:2015 | BS ISO 9940:2015 Aerospace series — Fluid, hydraulic, phosphate ester- base, fire resistant — Technical specification |
| BS ISO 09942-1:2015 | BS ISO 9942-1:2015 Cranes — Information labels Part 1: General |
| BS ISO 09974-4:2016 | BS ISO 9974-4:2016 Connections for general use and fluid power — Ports and stud ends with ISO 261 threads with elastomeric or metal-to- metal sealing Part 4: Dimensions, design, test methods and requirements for external hex and internal hex port plugs |
| BS ISO 09980:2012 | BS ISO 9980:2012 Belt drives — Grooved pulleys for V-belts (system based on effective width) — Geometrical inspection of grooves |
| BS ISO 09986:2014 | BS ISO 9986:2014 Composition cork for shoe outsoles |
| BS ISO 10002:2014 | BS ISO 10002:2014 Quality management — Customer satisfaction — Guidelines for complaints handling in organizations |
| BS ISO 10004:2012 | Quality management — Customer satisfaction — Guidelines for monitoring and measuring |
| BS ISO 10005:2005 | BS ISO Quality management systems — Guidelines for quality plans |
| BS ISO 10007:2017 | B S I S t a n d a r d s P u b l i c a t i o n Q u a l i t y m a n a g e m e n t G u i d e l i n e s f o r c o n f i g u ra t i o n m a n a g e m e n t B S I S O N a t i o n a l f o re w o rd T h i s B r i t i s h S t a n d a r d i s t h e U K i m p l e m e n t a t i o n o f I S O I t s u p e r s e d e s B S I S O w h i c h i s w i t h d r a w n T h e U K p a r t i c i p a t i o n i n i t s p r e p a r a t i o n w a s e n t r u s t e d b y T e c h n i c a l C o m m i t t e e Q S / Q u a l i t y m a n a g e m e n t a n d q u a l i t y a s s u r a n c e p r o c e d u r e s t o S u b c o m m i t t e e Q S / Q u a l i t y M a n a g e m e n t S y s t e m S t a n d a r d s A l i s t o f o r g a n i z a t i o n s r e p r e s e n t e d o n t h i s s u b c o m m i t t e e c a n b e o b t a i n e d o n r e q u e s t t o i t s s e c r e t a r y T h i s p u b l i c a t i o n d o e s n o t p u r p o r t t o i n c l u d e a l l t h e n e c e s s a r y p r o v i s i o n s o f a c o n t r a c t U s e r s a r e r e s p o n s i b l e f o r i t s c o r r e c t a p p l i c a t i o n I S B N I C S C o m p l i a n c e w i t h a B r i t i s h S t a n d a r d c a n n o t c o n f e r i m m u n i t y f r o m l e g a l o b l i g a t i o n s T h i s B r i t i s h S t a n d a r d w a s p u b l i s h e d u n d e r t h e a u t h o r i t y o f t h e S t a n d a r d s P o l i c y a n d S t r a t e g y C o m m i t t e e o n A p r i l A m e n d m e n t s / c o r r i g e n d a i s s u e d s i n c e p u b l i c a t i o n D a t e T e x t a f f e c t e d B RI T I S H S T A N D A RD B S I S O I S O Q u a l i t y m a n a g e m e n t G u i d e l i n e s f o r c o n f i g u ra t i o n m a n a g e m e n t M a n a g e m e n t d e la q u a l it L ig n e s d ir e ct r ice s p o u r la g e st io n d e la co n f ig u r a t io n I N T E R N A T I O N A L S T A N D A R D I S O T h i r d e d i ti o n R e f e re n c e n u m b e r I S O E B S I S O I S O E i i I S O A l l r i gh ts re s e r v e d C O P YRI G H T P R O T E C T E D D O C U M E N T I S O P u b l i s h e d i n S w i t z e r l a n d A l l r i g h ts r e s e r v e d U n l e s s o th e r w i s e s p e c i f i e d n o p a r t o f th i s p u b l i c a ti o n m a y b e r e p r o d u c e d o r u ti l i z e d o th e r w i s e i n a n y f o r m o r b y a n y m e a n s e l e c tr o n i c o r m e c h a n i c a l i n c l u d i n g p h o t o c o p yi n g o r p o s t i n g o n th e i n t e r n e t o r a n i n t r a n e t , wi th o u t p r i o r wr i tt e n p e r m i s s i o n P e r m i s s i o n c a n b e re q u e s t e d f ro m e i th e r I S O a t t h e a d d r e s s b e l o w o r I S O s m e m b e r b o d y i n th e c o u n tr y o f t h e r e q u e s t e r I S O c o p yr i g h t o f f i c e C h d e B l a n d o n n e t C P C H V e r n i e r G e n e v a S wi tz e r l a n d T e l Fa x c o p yr i g h i s o o r g www i s o o r g B S I S O I S O E F o re w o rd |
| BS ISO 10008:2013 | BS ISO 10008:2013 Quality management — Customer satisfaction — Guidelines for business-to-consumer electronic commerce transactions |
| BS ISO 10014:2006 | BS ISO Quality management — Guidelines for realizing financial and economic benefits |
| BS ISO 10018:2012 | Quality management — Guidelines on people involvement and competence |
| BS ISO 10050:2005 | BS ISO 10050 |
| BS ISO 10054:1998 | BS ISO Internal combustion compression-ignition engines — Measurement apparatus for smoke from engines operating under steady-state conditions — Filter type smokemeter |
| BS ISO 10068:2012 | BS ISO 10068:2012 Mechanical vibration and shock the human hand-arm system at the driving point |
| BS ISO 10086-2:2004 | BS ISO Coal — Methods for evaluating flocculants for use in coal preparation — Part 2: Flocculants as filter aids in rotary vacuum filtration systems |
| BS ISO 10100:2001 | BS ISO Hydraulic fluid power — Cylinders — Acceptance tests BS ISO |
| BS ISO 10109:2015 | BS ISO 10109:2015 Optics and photonics — Guidance for the selection of environmental tests |
| BS ISO 10113:2006 | BS ISO Metallic materials — Sheet and strip — Determination of plastic strain ratio |
| BS ISO 10115:2013 | Essential oil of tarragon |
| BS ISO 10122:2014 | BS ISO 10122:2014 Reinforcement materials — Tubular braided sleeves — Basis for a specification |
| BS ISO 10129:2017 | B S I S t a n d a r d s P u b l i c a t i o n P l a i n b e a r i n g s T e s t i n g o f b e a r i n g m e t a l s R e s i s t a n c e t o c o r ro s i o n b y l u b r i c a n t s u n d e r s t a t i c c o n d i t i o n s B S I S O N a t i o n a l f o re w o rd T h i s B r i t i s h S t a n d a r d i s t h e U K i m p l e m e n t a t i o n o f I S O I t s u p e r s e d e s B S I S O w h i c h i s w i t h d r a w n T h e U K p a r t i c i p a t i o n i n i t s p r e p a r a t i o n w a s e n t r u s t e d t o T e c h n i c a l C o m m i t t e e M C E P l a i n b e a r i n g s A l i s t o f o r g a n i z a t i o n s r e p r e s e n t e d o n t h i s c o m m i t t e e c a n b e o b t a i n e d o n r e q u e s t t o i t s s e c r e t a r y T h i s p u b l i c a t i o n d o e s n o t p u r p o r t t o i n c l u d e a l l t h e n e c e s s a r y p r o v i s i o n s o f a c o n t r a c t U s e r s a r e r e s p o n s i b l e f o r i t s c o r r e c t a p p l i c a t i o n I S B N I C S C o m p l i a n c e w i t h a B r i t i s h S t a n d a r d c a n n o t c o n f e r i m m u n i t y f r o m l e g a l o b l i g a t i o n s T h i s B r i t i s h S t a n d a r d w a s p u b l i s h e d u n d e r t h e a u t h o r i t y o f t h e S t a n d a r d s P o l i c y a n d S t r a t e g y C o m m i t t e e o n M a y A m e n d m e n t s / c o r r i g e n d a i s s u e d s i n c e p u b l i c a t i o n D a t e T e x t a f f e c t e d B RI T I S H S T A N D A RD B S I S O I S O P l a i n b e a r i n g s T e s t i n g o f b e a r i n g m e t a l s R e s i s t a n c e t o c o r ro s i o n b y l u b r i c a n t s u n d e r s t a t i c c o n d i t i o n s P a l ie r s l isse s E ssa i d e s m a t r ia u x a n t if r ict io n Ré sist a n c e la c o r r o sio n p a r d e s l u b r if ia n t s d a n s d e s c o n d it io n s st a t iq u e s I N T E R N A T I O N A L S T A N D A R D I S O S e c o n d e d i ti o n R e f e r e n c e n u m b e r I S O E B S I S O I S O E i i I S O A l l r i gh ts re s e r v e d C O P YRI G H T P R O T E C T E D D O C U M E N T I S O P u b l i s h e d i n S w i t z e r l a n d A l l r i g h ts r e s e r v e d U n l e s s o th e r w i s e s p e c i f i e d n o p a r t o f th i s p u b l i c a ti o n m a y b e r e p r o d u c e d o r u ti l i z e d o th e r w i s e i n a n y f o r m o r b y a n y m e a n s e l e c t r o n i c o r m e c h a n i c a l i n c l u d i n g p h o t o c o p yi n g o r p o s ti n g o n th e i n t e r n e t o r a n i n tra n e t w i t h o u t p r i o r wr i tt e n p e r m i s s i o n P e r m i s s i o n c a n b e re q u e s t e d f ro m e i t h e r I S O a t th e a d d r e s s b e l o w o r I S O s m e m b e r b o d y i n th e c o u n tr y o f t h e r e q u e s t e r I S O c o p yr i g h t o f f i c e C h d e B l a n d o n n e t C P C H V e r n i e r G e n e v a S wi tz e r l a n d T e l Fa x c o p yr i g h i s o o r g www i s o o r g B S I S O I S O E F o re w o rd |
| BS ISO 10130:2009 | BS ISO 10130 |
| BS ISO 10143:2014 | BS ISO 10143:2014 Carbonaceous materials for the production of aluminium — Calcined coke for electrodes — Determination of the electrical resistivity of granules |
| BS ISO 10155:1995 | BS ISO Implementation of ISO 10155:1995 Stationary source emissions — Automated monitoring of mass concentrations of particles — Performance characteristics, test methods and specifications |
| BS ISO 10159:2011 | BS ISO 10159:2011 Health informatics — Messages and communication — Web access reference manifest |
| BS ISO 10160:2015 | BS ISO 10160:2015 Information and documentation — Open Systems Interconnection — Interlibrary Loan Application Service Definition |
| BS ISO 10185:2004 | BS ISO Tobacco and tobacco products — Vocabulary CONFIRMED FEBRUARY 2008 |
| BS ISO 10203:2017 | BS ISO 10203:2017 Iron ores — Determination of calcium — Flame atomic absorption spectrometric method |
| BS ISO 10204:2015 | BS ISO 10204:2015 Iron ores — Determination of magnesium — Flame atomic absorption spectrometric method |