BS EN ISO 28721 — Glass-lined Apparatus for Process Plants Standard Series

Vitreous and Porcelain Enamels — Glass-lined Apparatus for Process Plants (ISO 28721 series)

🏭 BS EN ISO 28721 is the British Standard series adopted from the European Standard EN ISO 28721, corresponding to ISO 28721. It is the authoritative standard series for the quality and performance of glass-lined (glass-lining) apparatus for chemical process plants. The series specifies quality requirements for apparatus, components, appliances and accessories, the designation and specification of resistance to chemical attack and thermal shock, the determination of thermal-shock resistance, and requirements for glass-lined steel pipe fittings. It is widely used in the design, manufacture, inspection, and acceptance of glass-lined reactors, storage tanks, piping, and columns in the chemical, pharmaceutical, agrochemical, and food industries.

💡 Glass-lined apparatus is made by firing a glassy coating at high temperature onto a carbon-steel or stainless-steel substrate, combining the pressure-bearing and mechanical strength of metal with the corrosion resistance, non-adherence, and easy cleaning of glass. It is the preferred equipment for strongly corrosive chemical reactions and storage.

1. Series Structure and Scope 📌

The series is established under ICS 25.220.50 (Surface treatment — enamels) and 71.120.10 (Chemical plant) and maintained by UK Technical Committee STI/36 (Vitreous enamel coatings). The parts are complementary, forming a complete system from quality requirements to performance determination:

Standard PartSubjectMain Provisions
BS EN ISO 28721-1:2011Quality requirements for apparatus, components, appliances and accessoriesQuality, inspection, and acceptance requirements for glass-lined apparatus and its parts
BS EN ISO 28721-2:2015Designation and specification of resistance to chemical attack and thermal shockDesignation and specification of resistance-to-attack and thermal-shock classes
BS EN ISO 28721-3:2011Thermal shock resistanceDetermination of the thermal-shock resistance of glass-lined apparatus
BS EN ISO 28721-4:2015Glass-lined steel pipe and fittingsRequirements for flanged glass-lined steel pipes, fittings, and accessories
BS EN ISO 28721-5:2016Rating of resistance to chemical attack and thermal shockRating of apparatus and components for resistance to chemical attack and thermal shock
⚠️ This series applies to glass-lined apparatus for chemical process plants. Different parts address overall equipment quality, performance-class designation, and component requirements; select in light of the application, medium corrosivity, and operating temperature.

2. Quality Requirements and Performance Classes 🔧

The quality of glass-lined apparatus directly affects the safety and continuity of chemical production. The standard sets systematic quality requirements:

  • Coating quality: the glass layer should be uniform, dense, and free from bubbles, cracks, inclusions, and marked thickness variation; critical areas must be free from pinholes and spalling.
  • Chemical-attack class: after testing by the standard method, resistance to acidic and alkaline media is expressed by a class designation.
  • Thermal-shock resistance: the apparatus should withstand thermal shock over a defined temperature difference without cracking or spalling; the thermal-shock class is a key selection criterion.
  • Dimensions and form: flange sealing faces, nozzles, and other critical mating dimensions and form tolerances must meet the standard.
✅ The standard uses uniform test methods and class designations, making glass-lined apparatus from different suppliers comparable in chemical-attack and thermal-shock performance, providing a reliable basis for design selection and procurement acceptance.

3. Test Methods and Inspection Points 🔬

  • Chemical-attack test: per the corresponding ISO 28706 method, measure mass loss or attack of the glass layer in specified acid/alkali media at specified temperature and rate the corrosion class.
  • Thermal-shock test: transfer specimens or products at a defined temperature rapidly between hot and cold media, observing cracking or spalling to determine the thermal-shock class.
  • Visual and thickness inspection: visual and instrument detection of surface defects and thickness uniformity, with spark testing where necessary to reveal pinholes and defects.
  • Voltage/insulation test: spark/voltage testing of critical pressure and corrosion areas to ensure no conducting defects in the coating.
⚠️ Thermal-shock testing is among the most demanding performance evaluations for glass-lined apparatus. In service, avoid rapid cooling or heating of equipment under a temperature difference, and strictly control heating and cooling rates to prevent thermal stress from cracking the glass layer.

4. Engineering Practice and Applications 🛠️

  • Chemical reactors: core equipment for reactions in strong acids, alkalis, and corrosive organic media; the chemical-attack class must match medium corrosivity.
  • Storage and metering equipment: glass-lined storage tanks and metering vessels for corrosive liquids, ensuring medium purity and equipment life.
  • Glass-lined piping: flanged glass-lined steel pipes and fittings for conveying corrosive media; flange sealing and coating quality are key to leak-tightness and corrosion protection.
  • Pharmaceutical and food: smooth, non-adherent, easy-to-clean glass-lined surfaces meet the cleanliness and hygiene requirements of pharmaceutical and food processes.
🚨 Scan-version note: BS EN ISO 28721-4 (glass-lined steel pipe and fittings) and BS EN ISO 28721-5 (rating of resistance to chemical attack and thermal shock) are scanned files. Their content is summarized here from public-domain knowledge; the authoritative technical requirements are those of the official BSI published versions.

5. Frequently Asked Questions ❓

❓ Q: What is the thermal-shock resistance of glass-lined apparatus?
A: It is the ability of glass-lined apparatus to withstand sudden temperature changes without coating cracking or spalling, expressed as an allowable temperature difference or thermal-shock class. It is a key indicator of reliability under alternating hot-cold service.
❓ Q: How should the chemical-attack class be matched to the medium?
A: Match the chemical-attack class designation and medium reference tables to medium type (acid, alkali, salt, organic solvent), concentration, temperature, and operating conditions; verify by test where necessary.
❓ Q: What is the harm of pinholes in the glass lining?
A: Pinholes break coating density, allowing corrosive media to contact the metal substrate directly, causing substrate corrosion, medium contamination, and even perforation failure. Detect them promptly by spark testing and treat accordingly.
🔍 Q: What operating points should be observed when using glass-lined apparatus?
A: Strictly control heating and cooling rates to avoid thermal shock; prevent mechanical impact and sharp-object collision with the coating; regularly check coating integrity and flange sealing, and address defects promptly.
🔒