Physical Address
304 North Cardinal St.
Dorchester Center, MA 02124
Physical Address
304 North Cardinal St.
Dorchester Center, MA 02124
❤️ The BS EN ISO 25539 series specifies test methods and requirements for endovascular devices used in cardiovascular implants, making it an important medical device standard in interventional cardiology and vascular surgery. Published by BSI as the UK implementation of EN ISO 25539, the technical content is identical to ISO 25539 and was prepared by ISO/TC 150 (Implants for surgery) in collaboration with CEN/TC 285 (Non-active surgical implants), with UK participation entrusted to Technical Committee CH/150/2 (Cardiovascular implants). The series comprises three parts addressing endovascular prostheses, vascular stents and vena cava filters.
The series consists of three parts:
| Standard | Year | Title | Device |
|---|---|---|---|
| BS EN ISO 25539-1 | 2017 | Endovascular prostheses | Stent-grafts/vascular prostheses (e.g., EVAR aortic endoprostheses) |
| BS EN ISO 25539-2 | 2012 | Vascular stents | Bare-metal and drug-eluting stents, etc. |
| BS EN ISO 25539-3 | 2011 | Vena cava filters | Inferior vena cava filters |
All parts fall under ICS 11.040.40 (Surgical implants, prosthetics, orthotics). Part 1 supersedes BS EN ISO 25539-1:2009, Part 2 supersedes :2009, and Part 3 together with Parts 1 and 2 supersedes BS EN 12006-3:1998+A1:2009. The series specifies test requirements for endovascular devices in their intended use, covering materials, design, manufacture and labeling information, providing a basis for safety and effectiveness evaluation.
Part 1 (BS EN ISO 25539-1:2017) specifies test requirements for endovascular prostheses, including mechanical properties of stent-grafts and endovascular grafts (radial strength, flexibility, fatigue durability), delivery system performance, dimensions and marking, and biocompatibility evaluation. Endovascular prostheses are primarily used for endovascular repair of abdominal aortic aneurysms (EVAR) and thoracic aortic aneurysms (TEVAR).
This part emphasizes evaluating long-term durability in simulated physiological environments (pulsatile flow, fatigue loading) and provides methods for dimension measurement, radial force testing and delivery/deployment testing to ensure reliable device performance after implantation.
Part 2 (BS EN ISO 25539-2:2012) specifies test requirements for vascular stents, including radial strength, recoil, fatigue durability, drug-eluting performance (where applicable), delivery system and size labeling. Stents support narrowed or dissected vessels to restore blood flow and are core devices in coronary interventional treatment.
This part specifies performance requirements during stent compression, release and expansion, as well as in vitro-in vivo consistency evaluation methods, providing a basis for design verification and release testing of stent products.
Part 3 (BS EN ISO 25539-3:2011) specifies test requirements for vena cava filters. Filters are implanted in the inferior vena cava to intercept dislodged thrombi and prevent pulmonary embolism, for patients with contraindications to anticoagulation or failed anticoagulation therapy. This part specifies test methods for filter capture efficiency, thrombus capacity, deployment and retrieval (for retrievable types), materials and dimensions.
Filter geometry, positional stability and retrieval window are clinical concerns; this part provides unified methods for filter performance evaluation.