BS EN ISO 18278 — Resistance Welding Weldability Standard Series (General Requirements and Spot Welding Evaluation Procedures)

Resistance Welding — Weldability — Part 1: General Requirements / Part 2: Evaluation Procedures for Spot Welding

🔧 BS EN ISO 18278 is the British Standard series for evaluating the weldability of metallic materials in resistance welding, superseding the withdrawn 2004 editions and falling under ICS 25.160.01 (Welding in general) and 25.160.10 (Welding processes). The series specifies the general requirements and concrete test procedures for evaluating weldability in resistance spot, seam, and projection welding, and is widely used in the automotive, appliance, and sheet-metal forming industries for welding process qualification, material selection, and quality control.

💡 The core purpose of weldability evaluation: before mass production, use standardised tests to establish the welding adaptability range (current window, electrode life, etc.) of a material under given welding parameters, avoiding welding defects and quality fluctuation in production.

1. Scope and General Framework 📌

The series was prepared by ISO/TC 44 (Welding and allied processes) in collaboration with CEN/TC 121 (Welding and allied processes), with UK participation through Technical Committee WEE/29 (Resistance welding). It consists of two parts that address the “principle” and “operation” levels of weldability evaluation:

Standard PartYearSubjectProcesses CoveredSupersession
BS EN ISO 18278-12015General requirements for evaluating weldability for resistance spot, seam, and projection welding of metallic materialsSpot, seam, projectionSupersedes BS EN ISO 18278-1:2004
BS EN ISO 18278-22016Evaluation procedures for weldability in spot weldingResistance spot weldingSupersedes BS EN ISO 18278-2:2004
⚠️ Weldability evaluation results are strongly affected by electrode material, machine characteristics, sheet-thickness combination, and surface condition. The specified test procedure must be carried out on equipment consistent with actual production conditions, otherwise conclusions may be distorted.

2. Series Structure and Technical Points 🔬

2.1 Part 1 General Requirements (BS EN ISO 18278-1:2015)

Part 1 specifies general principles and requirements for evaluating the weldability of metallic materials (including coated steels, galvanised sheet, stainless steel, aluminium and its alloys) in resistance spot, seam, and projection welding. It covers selection and condition of test materials, welding test apparatus and electrode requirements, definition of weldability indicators (such as weldable current range, critical diameter, electrode life, and tendency to spatter and shrinkage cavities), and requirements for assessing and reporting results. This part provides a common basis for comparing weldability between laboratories.

2.2 Part 2 Spot Welding Evaluation Procedures (BS EN ISO 18278-2:2016)

Part 2 gives detailed test procedures specifically for resistance spot welding, including:

  • layout and number of test welds;
  • determination of the welding current range (increasing current stepwise to obtain minimum and maximum current, forming the “weldability lobe”);
  • measurement and assessment of weld or nugget diameter;
  • electrode life testing and electrode wear evaluation;
  • specimen inspection: tensile-shear testing, peel (cross-tension) testing, and metallographic examination.
💡 The wider the weldability lobe, the less sensitive the material is to welding current variation and the more robust the process. This is one of the most important indicators of material weldability.

3. Key Technical Requirements 🔧

To ensure comparable and repeatable results, the standard imposes strict requirements on test conditions:

  • Equipment calibration: welding current, force, and time parameters must be calibrated regularly and verified before and after testing.
  • Electrode management: electrode face shape, material, and dressing condition directly affect nugget quality; electrode diameter and face finish must be controlled per specification.
  • Specimen preparation: specimen size, overlap length, surface cleanliness, and assembly gap must be standardised to avoid excessive gaps causing spatter.
  • Parameter recording: fully record current, electrode force, weld time, electrode diameter, sheet thickness, and material grade for reproducibility.
  • Result assessment: judge weld quality using criteria such as minimum nugget diameter, shear strength, and peel failure mode.
🚨 Resistance welding involves high current and high temperature; observe electrical safety rules to prevent electric shock and burns. Welding tests should be performed in a well-ventilated area and welding spatter removed promptly.

4. Engineering Practice and Application Guidance 🛠️

  • 🔍 New material introduction: before a new material or new coating grade enters production, perform spot welding weldability evaluation per Part 2 to establish the welding parameter window and electrode life.
  • 🔧 Process qualification: incorporate weldability evaluation results into the Welding Procedure Qualification Record (WPQR) as the basis for establishing production Welding Procedure Specifications (WPS).
  • 📊 Supplier management: comparative weldability testing of the same grade from different suppliers effectively screens materials and controls incoming quality variation.
  • 📋 Production monitoring: periodically sample-check electrode life and weld quality after production start-up, comparing against initial weldability results to detect process drift early.

5. Frequently Asked Questions ❓

❓ Q: How do Part 1 and Part 2 work together?
A: Part 1 gives the general principles and requirements for weldability evaluation, while Part 2 gives the concrete test procedure for spot welding. Both are used when evaluating spot weldability — Part 1 sets the “rules”, Part 2 sets the “steps”.
❓ Q: How does galvanised steel differ from uncoated steel in weldability?
A: The zinc coating lowers contact resistance and causes current shunting, typically narrowing the weldability lobe and shortening electrode life. Galvanised sheet therefore requires higher welding current and more frequent electrode dressing; always evaluate using material in the same condition as production.
❓ Q: What is the weldability lobe (current window)?
A: At a given electrode force and weld time, it is the range of welding current that produces welds meeting the minimum nugget diameter requirement. A too-narrow window indicates the material is sensitive to current fluctuation and has insufficient process margin.
❓ Q: Does the standard apply to aluminium and aluminium alloy spot welding?
A: The series is aimed at metallic materials, and aluminium alloys can also be evaluated by the procedure, but aluminium has high thermal and electrical conductivity and a significant surface oxide film; suitable electrodes and parameter strategies are needed, with particular attention to surface cleaning.
🔒