BS EN ISO 17660 — Welding of Reinforcing Steel (Load-bearing and Non Load-bearing Welded Joints)

Welding — Welding of Reinforcing Steel — Part 1: Load-bearing Welded Joints; Part 2: Non Load-bearing Welded Joints (2006 Editions)

🏗️ BS EN ISO 17660 specifies requirements for welding of reinforcing steel used in concrete, and is the international standard for controlling reinforcing steel weld quality in construction. The series consists of two parts: Part 1 specifies requirements for load-bearing (structural) welded joints, while Part 2 specifies requirements for non load-bearing (non-structural) welded joints. The UK standards BS EN ISO 17660-1:2006 and BS EN ISO 17660-2:2006 are identical implementations of EN ISO 17660-1:2006 and EN ISO 17660-2:2006, prepared by BSI Technical Committee WEE/43 (Welding of steel for concrete reinforcement), replacing the withdrawn BS 7123.

Reinforcing steel welding is widely used in reinforced concrete structures for splicing bars, fixing intersection points (welded mesh), anchorage, and prefabricated element connections. Load-bearing joints transmit structural loads and require high weld strength and ductility; non load-bearing joints (such as welded mesh intersections) mainly provide positioning and construction functions, with relatively lower requirements. Weld quality directly affects structural safety, so systematic process requirements and inspection methods are essential.

💡 Reinforcing steel welding is a hidden structural safety element; load-bearing joints must guarantee adequate strength and ductility. BS EN ISO 17660 provides systematic joint classification, process requirements, and inspection and acceptance criteria, helping contractors and supervision bodies control weld quality.

1. Series Structure and Scope 📌

The series consists of two parts, both classified under ICS 25.160.10 (Welding processes). They were developed by ISO/TC 44 (Welding and allied processes), converted to European standards by CEN/TC 121 (Welding), and adopted as British Standards by BSI. They should be used in conjunction with the BS EN 1011 series (welding process recommendations) and national annexes.

StandardTitlePublishedJoint Type
BS EN ISO 17660-1:2006Welding — Welding of reinforcing steel — Part 1: Load-bearing welded jointsSep 2006Load-bearing (structural) joints
BS EN ISO 17660-2:2006Welding — Welding of reinforcing steel — Part 2: Non load-bearing welded jointsSep 2006Non load-bearing (non-structural) joints
⚠️ This series applies to welding of hot-rolled reinforcing steel, but the weldability of different steel grades (strength classes) and diameters varies. Before welding, confirm the chemical composition and weldability of the bars, and carry out welding procedure qualification where necessary.

2. Joint Types and Welding Processes 🔬

2.1 Load-bearing welded joints (Part 1)

Load-bearing welded joints transmit axial load in the bars. Common forms include flash butt welding, pressure gas welding, arc welding (lap, groove, and plate welding), and mechanical connections. The standard specifies welding process, weld dimensions, quality requirements, and inspection acceptance for load-bearing joints, and requires welding procedure qualification to verify joint strength and ductility through tensile and bending tests.

Key requirements for load-bearing joints include equal-strength matching of weld and base metal, conformity of weld dimensions (e.g., plate length, weld thickness), the structure and properties of the heat-affected zone, and the static and fatigue performance of the joint. The standard sets allowable limits for weld defects (porosity, slag, cracks, undercut).

2.2 Non load-bearing welded joints (Part 2)

Non load-bearing welded joints are mainly used for fixing intersection points of welded mesh and bar cages, and for positioning and construction connections that do not directly transmit primary structural loads. The standard specifies welding process and quality requirements, focusing on the firmness and consistency of intersection welds to prevent loosening during transport, concreting, and vibration.

Requirements for non load-bearing joints are relatively relaxed, but weld quality consistency must still be ensured to prevent false or detached welds. The standard specifies inspection methods such as visual inspection, hammer testing, or destructive testing to verify the reliability of intersection welds.

ComparisonPart 1 (Load-bearing)Part 2 (Non load-bearing)
Functional roleTransmit structural loadsPositioning, construction connection
Strength requirementEqual strength, higherRelatively lower
Procedure qualificationRequired (tensile/bending)Necessary (consistency verification)
Inspection focusWeld dimensions, defects, strengthWeld firmness, consistency
💡 Application points: load-bearing joints are key to structural safety and must strictly undergo procedure qualification and inspection; although non load-bearing joints do not transmit primary loads, poor welding may loosen during concreting and vibration, affecting the integrity of the bar cage and cover thickness.

3. Weld Quality Requirements and Inspection Methods 📏

The standard sets explicit quality requirements for reinforcing steel welded joints, including weld appearance (no cracks, no slag, no severe undercut), weld dimension deviations, and the mechanical properties of load-bearing joints (tensile strength, bending performance). Inspection methods include visual inspection, dimensional measurement, tensile testing, bend testing, and metallographic examination.

Load-bearing joints should be sampled for inspection, and full inspection performed where necessary; non load-bearing joints may use visual and hammer inspection. The standard specifies inspection lots, sample sizes, and acceptance criteria, and requires defective joints to be repaired or scrapped.

🚨 Reinforcing steel welding involves fire and electrical hazards: welding sparks can ignite combustibles, so fire-fighting equipment should be on site and combustibles cleared; welders should be certified, wear protective face shields and gloves, and ensure proper earthing to avoid electric shock.

4. Engineering Practice and Quality Control 🛠️

  • 🔍 Procedure qualification: before welding, carry out welding procedure qualification per the standard and project requirements, determining parameters (current, voltage, welding speed, preheat, post-heat), and issue a qualification report.
  • 📊 Welder qualification: welders should be trained, assessed, and certified, and their scope of work should match their qualification.
  • 📋 Process control: control welding parameters and bar-cleaning quality during welding; remove rust, oil, and mill scale before welding.
  • 🧾 Acceptance records: record the welding process, inspection methods, results, and acceptance decisions for weld joints, forming traceability documents.

5. Frequently Asked Questions ❓

❓ Q: How to distinguish load-bearing from non load-bearing joints?
A: Load-bearing joints transmit structural loads, such as bar splices and anchorage; non load-bearing joints are mainly for mesh intersections and construction connections that do not directly transmit primary loads. They follow Part 1 and Part 2 respectively.
❓ Q: Why is procedure qualification required for load-bearing joints?
A: Load-bearing joints carry structural loads, and their strength and ductility directly affect structural safety. Procedure qualification (tensile, bend tests) verifies the suitability of the welding process, ensuring joint performance meets design requirements.
❓ Q: What preparation is needed before welding reinforcing steel?
A: Remove rust, oil, mill scale, and moisture from the bar surface, check bar grade and weldability, set welding equipment per procedure-qualified parameters, and provide fire and safety protection.
❓ Q: What if a welded joint fails inspection?
A: Analyse the cause (e.g., improper parameters, poor bar weldability), repair or scrap the joint, and re-inspect per requirements; re-test mechanical and visual performance after repair.
🔒
正在加载下载地址,请稍候 10 秒

Leave a Reply