BS EN ISO 17636 — Non-destructive Testing of Welds Radiographic Testing (Film and Digital Detector Techniques)

Non-destructive Testing of Welds — Radiographic Testing — Part 1: X- and Gamma-ray Techniques with Film; Part 2: X- and Gamma-ray Techniques with Digital Detectors (2013 Editions)

📷 BS EN ISO 17636 specifies methods for radiographic testing of welds, one of the core standards in the non-destructive testing (NDT) of welded joints. The series consists of two parts: Part 1 covers X- and gamma-ray techniques with film, while Part 2 covers X- and gamma-ray techniques with digital detectors; together they replace the withdrawn BS EN 1435:1997. The UK standards BS EN ISO 17636-1:2013 and BS EN ISO 17636-2:2013 are identical implementations of EN ISO 17636-1:2013 and EN ISO 17636-2:2013, prepared by BSI Technical Committee WEE/46 (Non-destructive testing).

Radiographic testing uses X-rays or gamma rays emitted from a source to pass through the welded joint. Since internal defects (porosity, slag inclusions, lack of fusion, cracks) attenuate radiation differently from the base material, they produce distinct images on film or a digital detector, enabling the detection of internal weld defects. The method is particularly sensitive to volumetric defects (porosity, slag) and is widely used for welds in pressure vessels, boilers, and pipelines.

💡 Film technique is mature and provides direct-view images, widely used in traditional testing; digital detector technique (DR) requires no film or darkroom, offers fast imaging, and allows digital storage and transmission, and is increasingly mainstream. Both follow similar principles for source selection, geometry, and image-quality requirements.

1. Series Structure and Scope 📌

The series consists of two parts, both classified under ICS 25.160.40 (Welded joints). They were developed by ISO/TC 44 (Welding and allied processes), converted to European standards by CEN/TC 121 (Welding), and adopted as British Standards by BSI.

StandardTitlePublishedImaging Mode
BS EN ISO 17636-1:2013NDT of welds — Radiographic testing — Part 1: X- and gamma-ray techniques with filmJan 2013Film imaging (conventional radiography)
BS EN ISO 17636-2:2013NDT of welds — Radiographic testing — Part 2: X- and gamma-ray techniques with digital detectorsJan 2013Digital detector imaging (DR)
⚠️ This series applies to radiographic testing of fusion welds in metallic materials, but for different materials (steel, aluminium, titanium) and wall thicknesses, the radiation energy, exposure parameters, and image-quality requirements differ. The appropriate source and technique class must be chosen before testing according to material and thickness.

2. Testing Principles and Technique Classes 🔬

2.1 Testing principle and source selection

Radiographic testing uses radiation from an X-ray unit or gamma-ray source (e.g., Ir-192, Se-75, Co-60) to penetrate the welded joint. The difference in attenuation between defects and base material produces an image, and the type and size of defects are determined by observing the defect images (density differences). The type and energy of the source should be selected according to the thickness and density of the material to ensure adequate penetration and image contrast.

Attention should be paid to geometric unsharpness (determined by source focal-spot size and focal distance) and the effect of scattered radiation, controlled by increasing focal distance and using filters and lead shielding. The standard specifies the source-to-object distance, beam direction, and film/detector position.

2.2 Technique classes

The standard specifies two technique classes (A and B): Class A is the basic technique, while Class B is the improved technique (higher sensitivity). Class B generally requires a smaller source size, a larger focal distance, or stricter image-quality requirements to achieve higher detection sensitivity. The choice of technique class should be based on the importance of the weld and the acceptance requirements.

ComparisonPart 1 (Film technique)Part 2 (Digital detector technique)
Imaging mediumRadiographic film (darkroom processing)Digital detector (real-time/static imaging)
Image recordingFilm (long-term archiving)Digital image (storage and transmission)
Image-quality evaluationIQI (wire/hole type) + densityIQI + grey level and contrast
Typical useTraditional testing, site inspectionHigh-efficiency testing, digital management
💡 Technical points: to ensure detection sensitivity, use an appropriate image quality indicator (IQI) placed on the source side and evaluate the image quality index per the standard; the film density or digital image grey level must lie within the range specified in the standard, otherwise the exposure parameters should be adjusted.

3. Image Quality Requirements and Evaluation 📏

The standard sets explicit requirements for image quality, including the image quality index of the IQI, the density or grey-level range of the film/digital image, and limits on geometric unsharpness. The IQI is typically of the wire or hole type, placed on the source side; the image quality index evaluated after testing must meet the class requirement specified in the standard.

Image-quality evaluation also includes checking sharpness and contrast and avoiding artefacts (scratches, static marks, light leaks, uneven development) that could hinder defect interpretation. Digital detector technique also requires detector calibration (e.g., dark-field and gain correction) to remove pixel non-uniformity and dead pixels.

🚨 Radiographic testing involves ionising radiation: strictly follow radiation protection requirements, control the testing area, post warning signs, and use personal dosimeters. Expose only when personnel safety is assured. Testing personnel should be qualified and trained in radiation safety.

4. Engineering Practice and Quality Control 🛠️

  • 🔍 Procedure qualification: before testing, prepare a test procedure sheet per the standard specifying the source, exposure parameters, geometry, and image-quality requirements, and validate the procedure.
  • 📊 Image-quality control: place an IQI on every film/image and evaluate the image quality index; re-shoot unacceptable images.
  • 📋 Defect evaluation: evaluate defect type, size, and class per the relevant acceptance standard (e.g., ISO 5817, ISO 10675) and issue a test report.
  • 🧾 Records and reporting: reports should state the test standard, technique class, source, exposure parameters, image-quality results, defect evaluation, and tester qualification.

5. Frequently Asked Questions ❓

❓ Q: Why is the IQI placed on the source side?
A: Placing the IQI on the source side reflects the actual sensitivity of the system at the workpiece thickness and represents the most unfavourable position for image quality, giving a truer assessment of detection capability.
❓ Q: How to choose between film and digital detector techniques?
A: Film technique suits traditional site inspection and long-term archiving; digital detector technique suits high-efficiency testing, digital management, and remote interpretation, considering investment and testing cost.
❓ Q: What is the difference between Classes A and B?
A: Class B is the improved technique requiring higher sensitivity (smaller image quality index), typically a smaller focal spot, larger focal distance, or stricter exposure parameters; it is used for important pressure-bearing welds.
❓ Q: Can radiography detect all defects?
A: Radiography is sensitive to volumetric defects (porosity, slag); detection of planar defects (cracks, lack of fusion) depends heavily on the radiation direction. Complementary NDT methods such as ultrasonics should be used where necessary.
🔒