๐ BS EN ISO 17072 is the British Standard series on the chemical determination of metal content in leather, developed by ISO/TC 120 (Leather) in collaboration with the IULTCS (International Union of Leather Technologists and Chemists Societies), with UK participation through Technical Committee TCI/69 (Footwear, leather and coated fabrics). During production, leather may acquire metal elements such as chromium, lead, cadmium and arsenic from tanning agents, dyes, auxiliaries and metal fittings; among these, hexavalent chromium, lead and cadmium are strictly regulated. The series specifies chemical methods for determining metal content in leather, in two parts: Part 1 covers extractable metals; Part 2 covers total metal content.
๐ก Extractable metals simulate the amount of metal a leather releases to human sweat or the environment during use; total metal content reflects all the metal contained in the leather itself. The two serve different regulatory-conformance purposes: extractable metals usually correspond to consumer-product safety limits, while total metal content corresponds to environmental and recycling assessment.
1. Overview of the Series ๐
Classified under ICS 59.140.30 (Leather and furs) and published in 2011, the series is the basic method standard for metal-content testing and regulatory-conformance assessment of leather and leather products (footwear, bags, garments, automotive interiors).
| Standard Number | Title | Object of Determination | Typical Use |
| BS EN ISO 17072-1:2011 | Leather โ Chemical determination of metal content โ Part 1: Extractable metals | Extractable (solubilised) metals | Consumer-product safety limit assessment |
| BS EN ISO 17072-2:2011 | Leather โ Chemical determination of metal content โ Part 2: Total metal content | Total metal content | Environmental, recycling and total-load assessment |
โ ๏ธ Leather samples are non-uniform and contain oil and moisture; sampling and pre-treatment greatly affect results. Sample, homogenise and control moisture per the prescribed method, and carry out blank and duplicate control batch by batch.
2. Structure and Technical Essentials ๐ง
Parts 1 (extractable metals) and 2 (total metal content) differ in sample pre-treatment and purpose: extractable metals are obtained by extraction with simulated acidic perspiration and similar media; total metal content requires complete digestion of the leather before measuring all metals.
| Comparison | Part 1 โ Extractable Metals | Part 2 โ Total Metal Content |
| Pre-treatment | Extraction (e.g., acidic perspiration) | Complete digestion (acid digestion etc.) |
| Object measured | Solubilised / bioavailable metals | All metals in the leather |
| Instruments | ICP-OES / ICP-MS / AAS | ICP-OES / ICP-MS / AAS |
| Purpose | Consumer-product hazardous-substance limits | Environmental and total-load control |
3. Key Technical Requirements: Extractable Metals ๐ฌ
Part 1 specifies the method for extractable metals, simulating the dissolution of metals from leather during use:
- Extraction medium: prepare the extraction medium as specified (e.g., simulated acidic perspiration) and extract the leather sample at the specified temperature and time.
- Sample preparation: cut/grind the leather sample to uniformity, weigh as prescribed, and control the effects of moisture and oil.
- Instrumental analysis: analyse the extract by ICP-OES, ICP-MS or AAS for the concentration of each metal after appropriate treatment.
- Expression of results: extractable metal content is expressed as the mass of the corresponding metal per kilogram of leather (or per gram of specimen), e.g., mg/kg.
โ
Extractable metal results are commonly used to assess whether leather products comply with consumer-product regulations (e.g., lead and cadmium limits in Annex XVII of EU REACH) and buyer technical specifications.
4. Key Technical Requirements: Total Metal Content ๐ฏ
Part 2 specifies the method for total metal content, requiring complete digestion of the leather to measure all metals present:
- Digestion: completely digest the leather sample with acids (e.g., nitric acid, hydrogen peroxide) so that all metals pass into solution.
- Instrumental analysis: measure the concentration of each metal in the appropriately diluted digest, correct for blank and calculate the total content on the sample mass.
- Quality control: verify digestion and determination accuracy using certified reference materials and spike recoveries; duplicate results should meet the tolerance.
- Expression of results: total metal content is expressed in mg/kg (dry basis or as-received per the Standard).
๐จ Leather digestion involves strong acids, high temperature and high pressure (microwave digestion). Work in a fume hood and wear protective equipment; determination of elements such as hexavalent chromium is sensitive to pre-treatment conditions, so avoid valence changes introduced by pre-treatment.
5. Engineering Practice and Applications ๐ ๏ธ
- ๐ Regulatory conformance: leather footwear, garments, bags and children’s products should be tested for extractable lead, cadmium, chromium, arsenic, cobalt and nickel to meet hazardous-substance limits at home and abroad.
- ๐ Supply-chain control: tanneries and brands should control metal sources in raw materials, chrome-tanning processes, dyes and auxiliaries, and establish batch testing systems.
- ๐ Testing and reporting: testing laboratories issue reports per this series, stating sample pre-treatment, method conditions and uncertainty for buyers and regulators.
- ๐งช Typical applications: metal-content testing and compliance assessment of leather shoes, garments, bags, belts, automotive seat leather and children’s leather products.
6. Frequently Asked Questions โ
โ Q: Why do extractable metal and total metal content results differ?
A: Extractable metals are those that can be dissolved under a specific extraction condition, representing the part that can come into contact with people or the environment; total metal content is the sum of all metals in the leather, including the non-extractable part. The purposes differ and the two should not be used interchangeably.
โ Q: Is it necessary to test chromium in all leather?
A: Leather is usually tanned with chrome tannage; trivalent chromium is a common tanning agent and is generally not restricted, whereas hexavalent chromium is toxic and strictly regulated. Testing should distinguish total, extractable and hexavalent forms and evaluate per the relevant standards and methods.
โ Q: Why does sampling strongly affect results?
A: Metal distribution in leather varies across positions (grain, flesh, finish layers) during production, and leather contains moisture and fat. The representativeness of sampling, homogenisation and moisture correction directly affect the comparability and accuracy of results.
๐ Q: How do you ensure reliable metal-testing data?
A: Use certified reference materials, spike recoveries, blank and duplicate control, calibrate instruments periodically, and take part in inter-laboratory comparisons and proficiency testing to ensure traceable, trustworthy results.