BS EN ISO 16482 — Binders for Paints and Varnishes Determination of the Non-volatile-matter Content of Aqueous Rosin-resin Dispersions Oven and Microwave Methods

Binders for Paints and Varnishes — Determination of the Non-volatile-matter Content of Aqueous Rosin-resin Dispersions — Oven and Microwave Methods (2016, ISO 16482:2013)

🧪 BS EN ISO 16482 is the British Standard series on the determination of the non-volatile-matter content of aqueous rosin-resin dispersions used as binders for paints and varnishes, developed by ISO/TC 35 (Paints and varnishes) and adopted as a European standard by CEN/TC 139, with UK participation through Technical Committee STI/3 (Paints, media and related products). Non-volatile-matter content (i.e., solids content) is a key indicator for assessing the quality of aqueous rosin-resin dispersions and for controlling paint formulations, directly affecting the solids content of the dried film and formulation cost. The series consists of two parts: Part 1 is the oven method; Part 2 is the microwave method.

💡 Non-volatile-matter content is determined by heating the dispersion to evaporate water and volatiles, expressing the residual solids as a percentage of the original sample mass. The oven method is classical and reliable; the microwave method is rapid. Both are suitable for quality control.

1. Overview of the Series 📌

Classified under ICS 87.040 (Paints and varnishes) and 87.060.20 (Paint binders). The ISO version was published in 2013 and renumbered as BS EN ISO 16482 in 2016 following a corrigendum, superseding BS ISO 16482:2013. The two parts provide the oven and microwave methods respectively.

Standard NumberTitleMethodApplication
BS EN ISO 16482-1:2016Binders for paints and varnishes — Determination of the non-volatile-matter content of aqueous rosin-resin dispersions — Part 1: Oven methodOven heating evaporationClassical laboratory quality control
BS EN ISO 16482-2:2016Binders for paints and varnishes — Determination of the non-volatile-matter content of aqueous rosin-resin dispersions — Part 2: Microwave methodMicrowave dryingRapid determination
⚠️ Non-volatile-matter content is affected by heating temperature, time and sample size. Determination must strictly follow the temperature and time specified by the Standard; otherwise incomplete volatilisation or resin degradation may cause deviation.

2. Structure and Technical Essentials 🔧

The oven and microwave methods share the same principle — heating to evaporate water and volatiles, then weighing the residual solids — differing only in the heating mode and operating flow:

  • Oven method (Part 1): a weighed dispersion sample is placed in an oven at the specified temperature (e.g., 125 °C), dried to constant mass, cooled and weighed.
  • Microwave method (Part 2): microwave radiation rapidly evaporates the water in the sample; drying time is short and determination is fast, suiting on-line or high-frequency inspection.
ComparisonPart 1 — OvenPart 2 — Microwave
Heating modeForced-convection ovenMicrowave radiation
Determination timeLonger (usually several hours)Short (minutes)
Result reliabilityClassical, stableRapid, requires calibration
Sample capacityBatch determination possibleSingle or few samples
UseArbitration and routine inspectionRapid process control

3. Key Technical Requirements: Principle and Operating Procedure 🔬

The Standard places clear requirements on sample weighing, heating conditions and result calculation:

  • Sample representativeness: stir the dispersion thoroughly before sampling to avoid non-uniform samples from settling or separation.
  • Weighing: weigh the specified mass of sample onto a flat dish using a balance of appropriate precision, recording the exact mass.
  • Heating/drying: for the oven method, dry at the specified temperature to constant mass (two successive weighings differing by no more than the specified limit); for the microwave method, dry according to the instrument programme to constant mass.
  • Result calculation: non-volatile matter (%) = (mass of residue after drying ÷ mass of sample) × 100%.
✅ It is recommended to run duplicate samples (usually at least two) in each batch; the difference between duplicates should be within the specified range. Where necessary, verify method accuracy using a reference sample of known solids content.

4. Key Technical Requirements: Equipment and Precautions 🎯

  • Oven: should maintain the specified temperature stably and have good ventilation to prevent steam condensing and refluxing inside.
  • Microwave drier: should be equipped with a moisture-determination function and calibrated per the manual; sample size should be appropriate to avoid uneven microwave heating.
  • Weighing dish: choose a temperature-resistant, chemically stable dish (e.g., aluminium or glass dish), kept clean and dry.
  • Cooling and weighing: after drying, cool the sample in a desiccator to room temperature before weighing to avoid moisture absorption giving high results.
🚨 Microwave heating of water-based dispersions may cause splashing or superheating. Use heat-resistant containers and control power and time; take care against burns during oven operation, and avoid direct contact when transferring hot samples into the desiccator.

5. Engineering Practice and Applications 🛠️

  • 🔍 Quality control: non-volatile-matter content is a core index in incoming inspection and process control of aqueous dispersions, directly affecting the solids content of paints and inks and cost accounting.
  • 📊 Formulation development: in formulation design, the addition of resin, pigments and additives is calculated from the non-volatile-matter content to ensure film performance.
  • 📋 Batch consistency: the non-volatile-matter content of different batches from the same supplier should remain stable; an out-of-range deviation should be investigated.
  • 🧪 Typical applications: solids-content inspection of rosin-resin dispersions (including modified rosin emulsions) in water-based printing inks, water-based paints, adhesives and overprint varnishes.

6. Frequently Asked Questions ❓

❓ Q: What is the difference between non-volatile-matter content and solids content?
A: In dispersion testing the two usually mean the same — the mass fraction of residual solids (resin, additives etc.) after evaporating water and volatiles. The Standard uses “non-volatile-matter content” as the formal term.
❓ Q: Can the results of the oven and microwave methods be used interchangeably?
A: The two methods share the same principle and should in principle give the same result, but the heating modes differ and may produce differences for certain easily oxidised or degraded systems. The oven method is usually the reference for arbitration; when using the microwave method, verify consistency by comparison tests.
❓ Q: Why cool and weigh in a desiccator after drying?
A: The dried residue absorbs moisture from the air, and weighing directly would give a high mass and a low solids result. Cooling to room temperature in a desiccator avoids moisture absorption and ensures accurate weighing.
🔍 Q: What is the permitted deviation for duplicate samples?
A: The Standard requires the difference between duplicate determinations to be within a specified range (the exact limit is given in the Standard text and laboratory QC requirements). Re-test and investigate if the permitted deviation is exceeded.
🔒