🧵 BS EN ISO 16396 is the British Standard series on polyamide (PA, commonly known as nylon) moulding and extrusion materials, developed by ISO/TC 61 (Plastics) with CEN/TC 249 (Plastics), with UK participation through Technical Committee PRI/82 (Thermoplastic materials). It supersedes the earlier BS EN ISO 1874 series and is the current standard system for the designation, specification and property determination of PA moulding and extrusion materials. The series consists of two parts: Part 1 specifies the designation system, marking of products and basis for specifications; Part 2 specifies the preparation of test specimens and determination of properties. PA offers excellent mechanical properties, wear resistance and chemical resistance, and is widely used in automotive, electrical/electronic, machinery and consumer products.
💡 A unified designation system makes the grade, composition and key properties of a PA material immediately clear, providing a common language between suppliers, processors and end users; standardised specimen preparation and property determination are the prerequisite for comparable data.
1. Overview of the Series 📌
Classified under ICS 83.080.20 (Thermoplastic materials). Part 1 (2015) supersedes BS EN ISO 1874-1:2010; Part 2 (2017) supersedes BS EN ISO 1874-2:2012. The two parts cover the “material identification/specification” and “property determination” stages respectively.
| Standard Number | Title | Core Content | Status |
| BS EN ISO 16396-1:2015 | Plastics — Polyamide (PA) moulding and extrusion materials — Part 1: Designation system, marking of products and basis for specifications | PA designation, grade data blocks and specification clauses | Supersedes ISO 1874-1:2010 |
| BS EN ISO 16396-2:2017 | Plastics — Polyamide (PA) moulding and extrusion materials — Part 2: Preparation of test specimens and determination of properties | Specimen preparation, conditioning and property determination | Supersedes ISO 1874-2:2012 |
⚠️ PA is a hygroscopic material; moisture content significantly affects both injection moulding and mechanical properties. Moisture must be controlled in designation, storage and testing, and specimen conditioning and test environment strongly influence results.
2. Structure and Technical Essentials 🔧
Part 1 (designation and specification) and Part 2 (specimens and properties) work together: the designation system defines “what the material is and how its properties are denoted”, while specimen preparation and property determination provide the methods for obtaining those property data.
| Comparison | Part 1 — Designation & Specification | Part 2 — Specimens & Properties |
| Nature of content | Designation and specification clauses | Test methods |
| Core content | Grade data blocks, PA type definition | Injection/compression specimens, conditioning |
| Property data | Indices referenced by specifications | Tensile, impact, melt flow rate determination |
| Purpose | Material selection and procurement | Quality inspection and performance evaluation |
3. Key Technical Requirements: Designation System and Basis for Specifications 🔬
Part 1 specifies the designation rules and basis for specification clauses for PA materials. A designation normally consists of the standard number and data blocks containing material type, filler/reinforcement and key property data:
- PA type: e.g., PA6, PA66, PA11, PA12, PA46 and copolymers; the designation should state the type and composition.
- Data blocks: the designation may contain data blocks specifying the type and content of filler/reinforcement (e.g., GF30 for 30% glass-fibre reinforcement) and information such as melt volume-flow rate (MVR).
- Specification clauses: provide the basis for drafting specifications so that parties can agree material requirements using uniform designations and property indices.
- Product marking: define the marking content of materials, articles and packaging to ensure traceability.
✅ Marking plastic products with the material identifier (e.g., “>PA6-GF30<“) per ISO 11469 and similar requirements facilitates sorting for recycling and material traceability, an important marking practice in sustainable design.
4. Key Technical Requirements: Preparation of Test Specimens and Determination of Properties 🎯
Part 2 specifies the preparation of PA test specimens and the property-determination requirements — the key to comparable data:
- Specimen preparation: prescribes the moulding conditions for injection or compression specimens (melt temperature, mould temperature, injection pressure etc.) so that specimens produced in different laboratories are comparable.
- Conditioning: hygroscopic PA materials should be conditioned under defined conditions (e.g., specified temperature and relative humidity) before testing, with the moisture content in the specified range.
- Property determination: determine tensile properties, flexural properties, impact properties (Charpy/Izod), melt volume-flow rate (MVR) and other indices, using the corresponding ISO test methods.
- Test environment: determination should be performed under the specified laboratory environment (temperature, humidity) to ensure reproducibility.
🚨 PA injection moulding involves high temperatures (melt temperatures often above 240 °C) and high pressures. Follow injection-moulding machine safety rules and protect against burns; be aware of low-molecular-weight emissions during drying and processing and take personnel precautions.
5. Engineering Practice and Applications 🛠️
- 🔍 Material selection: choose PA type and reinforcement level according to the service conditions (temperature, load, chemical media) and processing method, checking designations and property data.
- 📊 Incoming inspection: sample PA pellets for MVR, moisture content and key properties, verifying grade marking and specification conformance.
- 📋 Processing control: dry adequately before moulding (control moisture content), set appropriate melt and mould temperatures, and avoid degradation and part defects.
- 🧪 Typical applications: automotive (intake manifolds, gears, clips), electrical/electronic (connectors, coil bobbins), machinery (bearings, gears, pulleys) and consumer products (zippers, sporting goods).
6. Frequently Asked Questions ❓
❓ Q: What is the difference between PA6 and PA66?
A: PA6 and PA66 are the two most common PA types, differing slightly in chemical structure, moisture absorption and crystallisation temperature. PA66 generally has a higher melting point and greater rigidity; PA6 offers a wider processing window and often lower cost. Check the material’s specification data for the exact properties.
❓ Q: What does a data block such as GF30 in the designation mean?
A: The data block usually gives the type and content of filler/reinforcement — GF30 means 30% glass-fibre reinforcement. Designations also often include MVR and other information, helping to distinguish grades and select the appropriate processing and performance.
❓ Q: Why must PA specimens be conditioned before testing?
A: PA absorbs moisture strongly, and moisture content affects mechanical properties and dimensions. Without conditioning, properties measured in different environments are not comparable. The Standard specifies conditioning to equilibrium moisture at defined temperature and humidity before testing.
🔍 Q: Why is drying required before processing PA?
A: Moisture in PA hydrolyses and degrades the polymer during high-temperature moulding, causing property loss and part defects (silver streaking, bubbling). Drying to a specified moisture content (usually below 0.2%) is a necessary step before PA moulding.