BS EN ISO 15877 — Plastics Piping Systems for Hot and Cold Water Installations: Chlorinated Poly(Vinyl Chloride) (PVC-C)

General requirements, pipes, fittings and fitness for purpose of the system
📄 Scanned-version note: Part 5 of this series (BS EN ISO 15877-5:2009+A1:2010) is a scanned document (not machine-readable). This article summarises it from public domain knowledge of the standard’s subject area; the authoritative clauses are those in the BSI published version.

🚰 BS EN ISO 15877 is the British Standard series adopted by BSI from the European standard EN ISO 15877, specifying the requirements for chlorinated poly(vinyl chloride) (PVC-C) plastics piping systems for hot and cold water installations in buildings. Prepared by ISO/TC 138 together with CEN/TC 155 and entrusted in the UK to Technical Committee PRI/88/2 (Plastics piping for pressure applications), the series is classified under ICS 23.040.01, 23.040.20, 23.040.45 and 91.140.60. By chlorination, PVC-C (commonly CPVC) enhances the heat resistance of PVC, giving high-temperature tolerance, flame retardancy, chemical resistance and good hygiene, and is widely used for hot water, potable water, fire-protection and chemical piping systems.

⚠️ UK National foreword: The UK Committee emphasises that compliance with this standard does not necessarily mean products are fit for non-potable hot-water pipes, nor that all performance requirements of an actual UK pipework application are covered. The normal maximum cold-water supply pressure in the UK is 12.5 bar, a pressure that some application classes in this standard do not meet; the predominant UK jointing method is push-fit, while this standard defines mechanical fittings only in general terms; and there is a disparity between the malfunction temperature (100 °C) in Table 1 of Part 1 and boiler malfunction temperatures (110 °C). Current UK practice should consult BS 7291-1 and select systems to BS 7291 Class S; this series does not replace BS 7291 parts 1, 2 and 3.
💡 PVC-C is “heat-resistant PVC”: chlorination raises the chlorine content, significantly increasing the Vicat softening temperature and long-term heat-creep capability, enabling use in hot-water systems.

1. Series Structure and Scope 📌

This batch covers four parts of the 2009 edition (with A1:2010 amendments):

Part StandardThemeICSMain Content
BS EN ISO 15877-1:2009+A1:2010General23.040.01; 91.140.60Terminology, materials, design basis and overall requirements
BS EN ISO 15877-2:2009+A1:2010Pipes23.040.20; 91.140.60Dimensions, performance and testing of PVC-C pipes
BS EN ISO 15877-3:2009+A1:2010Fittings23.040.45; 91.140.60Dimensions, performance and testing of PVC-C fittings
BS EN ISO 15877-5:2009+A1:2010 (scanned)Fitness for purpose of the system23.040.01; 91.140.60Fitness-for-purpose testing of the pipe-fitting-joint combination system
⚠️ Before selecting this standard, verify the system service conditions (in particular UK cold-water pressure of 12.5 bar and heating malfunction temperatures), and where necessary assess to BS 7291 Class S.

2. Technical Requirements of Each Part 🔧

2.1 Part 1: General

Part 1 specifies the terminology, material requirements and design basis of PVC-C piping systems: it defines the material grade, minimum required strength (MRS) and design coefficient, gives the design pressure-temperature-life relationship and the application classes (including the Table 1 malfunction temperatures), and sets out the overall requirements for pipes, fittings and systems. Amendment A1:2010 modified a number of clauses.

2.2 Part 2: Pipes

Part 2 specifies the dimension series (outside diameter, wall thickness and SDR), tolerances, appearance, mechanical properties (hydrostatic strength, impact toughness) and hygienic requirements of PVC-C pipes, together with test methods. PVC-C pipe is relatively rigid and is mainly joined by solvent-cement bonding or mechanical joints.

2.3 Part 3: Fittings

Part 3 specifies the dimensions, performance and test requirements of PVC-C fittings, including socket dimensions, wall thickness, hydrostatic strength, bonding quality and sealing requirements, ensuring that fittings match the pipes in performance after jointing.

2.4 Part 5: Fitness for Purpose of the System

Part 5 specifies system-level fitness-for-purpose tests for the pipe-fitting-joint combination, including internal-pressure tests, thermal-cycle tests, flexural and sealing tests, evaluating the reliability of the complete combination under long-term operating conditions. (Scanned version, compiled from public domain knowledge)

✅ PVC-C system jointing is dominated by solvent bonding and mechanical joints; cleanliness of the bonding surfaces, adhesive application and curing-time control are the keys to long-term leak-free joints.

3. Key Technical Requirements and Acceptance Points 🧪

  • Material grade: verify the PVC-C material MRS and design stress, and select by application class and temperature.
  • Wall-thickness design: determine wall thickness by SDR and design pressure, allowing for strength reduction at elevated temperature.
  • Joint quality: solvent cement should be matched to the pipe material; control the amount applied, full insertion and curing time.
  • Thermal expansion compensation: PVC-C has a comparatively high coefficient of thermal expansion; straight runs should include compensators or expansion loops to avoid thermal pull-out and cracking.
  • Fire and hygiene: PVC-C is flame-retardant, suiting high fire-safety locations; potable-water systems must meet hygienic requirements.

4. Engineering Practice 🛠️

  • 🔍 System selection: choose the PVC-C pipe series and fittings according to temperature, pressure and life, verifying suitability for UK Class S requirements.
  • 🔧 Installation: strictly control the solvent-bonding process and curing time; arrange expansion compensation and supports correctly.
  • 📊 Pressure testing: after installation, perform a hydrostatic test, determining test pressure and holding time per the specification.
  • 📋 Acceptance and maintenance: verify material certificates and hygienic approval; in service, avoid over-temperature, overpressure and impact damage.

5. Frequently Asked Questions ❓

❓ Q: What is the difference between PVC-C and ordinary PVC-U?
A: PVC-C is chlorinated to improve heat resistance, giving markedly higher Vicat softening temperature and long-term heat performance than PVC-U, so it can be used for hot-water systems; PVC-U is mainly used for cold water, drainage and chemicals.
❓ Q: How are PVC-C pipes mainly joined?
A: Chiefly by solvent-cement socket bonding, or by mechanical (press/clamp) joints. Bonding is sensitive to construction technique; adhesive application, insertion and curing must be controlled.
❓ Q: Why does the UK particularly note the BS 7291 series?
A: The UK maximum cold-water supply pressure of 12.5 bar and boiler malfunction temperatures of 110 °C exceed the applicable conditions of some application classes in this series; UK tradition uses systems certified to BS 7291 Class S, and this series does not replace BS 7291 parts 1, 2 and 3.
❓ Q: Why does a PVC-C system need thermal expansion compensation?
A: PVC-C’s coefficient of thermal expansion is several times that of steel; temperature change produces significant thermal elongation. Without compensation, joints can be pulled apart or fittings crack, so compensators, expansion loops or correctly arranged supports are required.
🔒
正在加载下载地址,请稍候 10 秒

Leave a Reply

Your email address will not be published. Required fields are marked *