BS EN ISO 15614 — Specification and Qualification of Welding Procedures for Metallic Materials (Welding Procedure Test)

Specification and Qualification of Welding Procedures for Metallic Materials — Welding Procedure Test (ISO 15614 series)

🔩 The BS EN ISO 15614 series is the British Standard implementation of EN ISO 15614, which is identical to ISO 15614. It specifies methods and acceptance requirements for qualifying welding procedures by a welding procedure test, covering arc and gas welding of steels and nickel, electron and laser beam welding, and resistance spot, seam and projection welding. It is the core standard for quality control of pressure-containing and load-bearing welded structures such as boilers, pressure vessels, steel structures and pipelines.

💡 The core principle of 15614 is “test first, then produce”: by welding a representative test piece and examining its mechanical and metallurgical properties, it proves that the welding procedure can consistently produce acceptable joints, thereby ensuring batch production quality.

1. Series Overview 📌

The series is divided by welding process: Part 1 covers arc and gas welding of steels and nickel; Part 11 covers electron and laser beam welding; Part 12 covers resistance spot, seam and projection welding; the remaining parts (2, 5, 7, 8, 13, 14) cover aluminium, titanium, stainless steel, high-alloy steel and other processes. The UK committee is WEE/36 (Approval testing of welding procedures and welders), mirroring ISO/TC 44 “Welding and allied processes”.

⚠️ Parts 2, 5, 7, 8, 13 and 14 of this series are scanned versions; the related descriptions here are compiled from public domain knowledge of the standard’s field, and the authoritative text is the official BSI published version.

2. Series Structure and Technical Points 🧩

The series contains 9 standard documents, as shown below.

Standard No.EditionSubject (English title)
BS EN ISO 15614-12017Part 1: Arc and gas welding of steels and arc welding of nickel and nickel alloys
BS EN ISO 15614-112002Part 11: Electron and laser beam welding
BS EN ISO 15614-122014Part 12: Spot, seam and projection welding
BS EN ISO 15614-22005Part 2: Arc welding of aluminium and its alloys (scanned)
BS EN ISO 15614-52004Part 5: Arc welding of titanium and its alloys (scanned)
BS EN ISO 15614-72016Part 7: High-alloy steels (scanned)
BS EN ISO 15614-82016Part 8: Stainless steel (scanned)
BS EN ISO 15614-132012Part 13: Other welding processes (scanned)
BS EN ISO 15614-142013Part 14: Other welding processes (scanned)

BS EN ISO 15614-11:2002 is identical to ISO 15614-11:2001, with ICS 25.160.10.

3. Key Technical Requirements 🔧

3.1 Welding procedure test flow

The typical flow is: prepare a preliminary WPS (pWPS) → weld a representative test piece to the pWPS → examine the test piece by visual, non-destructive and destructive tests (tensile, bend, impact, hardness, macro/micro metallography) → assess against the standard acceptance criteria → if acceptable, issue the final WPS and qualification record.

3.2 Test items and acceptance

The parts specify corresponding test items and acceptance criteria: for example Part 1 specifies joint tensile, side/front bend, impact and hardness; Part 11 for high-energy beam welding specifies joint and heat-affected-zone examination; Part 12 for resistance welding specifies tensile-shear, cross-tension and nugget size.

3.3 Range of validity and substitution

The qualified range is limited by material group, thickness/diameter, welding position, groove geometry, welding consumables and parameter ranges; outside this range a new or supplementary qualification is required.

🚨 Welding procedure qualification must cover the actual production range. If the test piece does not represent the actual joint (for example thickness, material, position outside the qualified range), the qualification is invalid; never substitute a “similar qualification” for a real one.

4. Practical Engineering Application 🛠️

  • 🔍 Qualification planning: prepare a qualification plan by product structure and material, covering all representative joints.
  • 🔧 Test piece: a qualified welder welds to the pWPS, with process records and parameter monitoring.
  • 📊 Inspection and assessment: complete visual, non-destructive and destructive tests and judge against the standard acceptance criteria.
  • 📋 Documentation: issue the WPS, qualification records and welder qualifications, ensuring traceability.

5. Frequently Asked Questions ❓

❓ Q: How does 15614 relate to ISO 15609 (WPS preparation)?
A: ISO 15609 specifies the format and content of a Welding Procedure Specification (WPS); ISO 15614 specifies how to qualify that WPS by a welding procedure test. Together they form the complete procedure qualification system.
❓ Q: Why is a welding procedure test needed?
A: Welding quality depends strongly on material, process parameters and operator skill, so theoretical calculation alone cannot guarantee it. Testing a representative piece verifies mechanical and metallurgical properties, ensuring stable production joint quality.
❓ Q: How does qualification for electron/laser welding (Part 11) differ from arc welding (Part 1)?
A: High-energy beam welding has high energy density, low heat input and a narrow HAZ; the focus is on joint appearance, lack of fusion and HAZ microstructure, so test and acceptance requirements differ from arc welding.
🔍 Q: What variables must a qualification test piece cover?
A: It should cover material group, thickness/diameter range, welding position, groove type, welding consumables and key process parameter ranges; outside these, a new or supplementary qualification is needed.
🔒