BS EN ISO 1518 — Paints and Varnishes Determination of Scratch Resistance Series

Standard Series (Part 1: Constant-Loading Method & Part 2: Variable-Loading Method)

✏️ BS EN ISO 1518 is the BSI-published series adopting the European Standard EN ISO 1518, identical to ISO 1518. It specifies methods for determining the scratch resistance of paints and varnishes — the ability of a coating to resist scratching by a hard object without producing a visible scratch. Scratch resistance is an important quality indicator for many decorative and functional coatings, from automotive topcoats and appliance housings to wood coatings and coil coatings, directly affecting product appearance retention and service life. The series has two parts: Part 1, the constant-loading method (scratch under a fixed load and judge whether a scratch forms), and Part 2, the variable-loading method (continuously increasing load to find the “critical scratch load”). The series supersedes the former BS EN ISO 1518:2001 and BS EN ISO 12137-2:2006.

💡 BSI Technical Committee STI/10 (Test Methods for Paints) manages UK participation, aligned with ISO/TC 35 (Paints and Varnishes) and CEN/TC 139.

1. Series Overview and Scope 🎯

The basic scratch test: a stylus of defined hardness and shape (a loaded needle or pen) is drawn at uniform speed across the coating surface, and the surface is then inspected for visible scratching. The two methods answer two engineering questions: the constant-loading method asks “does the coating resist scratching at the specified service load?”, and the variable-loading method asks “at what load does the coating begin to be scratched?”. The series is classified under ICS 87.040 (paints and varnishes).

StandardTitleMain Content
BS EN ISO 1518-1:2011Paints and varnishes — Determination of scratch resistance — Part 1: Constant-loading methodScratching under a selected constant load and judging whether a visible scratch appears
BS EN ISO 1518-2:2011Paints and varnishes — Determination of scratch resistance — Part 2: Variable-loading methodContinuously increasing load to determine the critical load at which scratching begins
⚠️ Scratch judgement relies on the definition of a “visible” scratch: different lighting, viewing angles and inspectors can disagree. Test under standardised illumination and viewing conditions, performed by trained personnel.

2. Part 1: Constant-Loading Method 🎚️

BS EN ISO 1518-1:2011 specifies the constant-load scratch test:

  • Stylus: a stylus (pen or needle type) of specified shape and hardness, with consistent scratch angle and travel direction.
  • Load application: a selected load is applied to the stylus (per product specification or mutual agreement).
  • Scratch procedure: a scratch of specified length is drawn at uniform speed over the cured coating surface.
  • Judgement: visual inspection determines whether the scratch is continuously visible, giving “coating scratched / not scratched”.
💡 The constant-loading method suits pass/fail quality control: set the load to the product requirement (e.g. 2 N), scratch and judge — simple and fast.

3. Part 2: Variable-Loading Method 📈

BS EN ISO 1518-2:2011 specifies the scratch test with continuously increasing load:

  • Load gradient: the load rises continuously (or in steps) from low to high during scratching.
  • Critical load determination: the point where the scratch becomes continuously visible identifies the “critical scratch load”.
  • Result expression: the critical load (newtons) is a quantitative indicator of scratch resistance — the higher, the better.
  • Scope: better suited to quantitative comparison and specification between materials/formulations.
🚨 The variable-loading test is more sensitive to stylus wear, surface cleanliness and travel speed. Check the stylus tip before and after, and keep the surface free of particles, or the critical-load data will be distorted.

4. Key Technical Points 🔍

TopicPart 1 (Constant Load)Part 2 (Variable Load)
Loading modeConstant loadContinuously increasing load
Result formScratched / not scratchedCritical load (N)
Typical usePass/fail, production inspectionMaterial comparison, R&D, specification
SpeedFastSlower (requires reading the critical point)
EquipmentSimpleRequires a load-gradient mechanism

5. Engineering Practice 🛠️

  • Formulation development: use the variable-loading method to compare critical scratch loads of different resin, crosslinker and additive systems, balancing hardness and toughness.
  • Quality control: include the constant-loading method in production sampling to quickly screen batches that fail scratch requirements.
  • Product specification: define a minimum critical load or a pass criterion at a specified load in technical specifications.
  • Field failure analysis: retest parts with scratched surfaces in service and, combined with scratch morphology, judge whether the coating is too soft or contamination is the cause.

6. FAQ ❓

❓ Are scratch resistance and hardness the same thing?
Answer: Not exactly. Hardness (e.g. pencil hardness, pendulum hardness) reflects resistance to indentation; scratch resistance is more influenced by coating toughness, friction behaviour and stylus geometry. They correlate but are not interchangeable.
❓ Why do different methods give different results for the same coating?
Answer: Stylus shape, load, speed and judgement criteria all affect results. The constant-loading method gives a qualitative pass/fail; the variable-loading method gives a quantitative critical load — they answer different questions.
❓ Is there an objective criterion for judging scratches visually?
Answer: The standard prescribes uniform observation conditions and judgement rules, but some subjectivity remains. Magnifiers, defined lighting and multi-person review reduce misjudgement; combine with microscopy when needed.
❓ Does film thickness affect the results?
Answer: Yes. Very thin coatings tend to deform with the substrate, and scratches reach the substrate more easily; compare at similar dry-film thickness.
❓ How does this series differ from abrasion tests (e.g. falling-sand, Taber)?
Answer: This series targets scratch resistance to a single scratch producing a visible mark; abrasion tests evaluate mass loss or appearance change under repeated wear. Choose the test matching the dominant in-service damage mode.
🔒
正在加载下载地址,请稍候 10 秒

Leave a Reply

Your email address will not be published. Required fields are marked *