🧵 BS EN ISO 13934 is the British Standard (BSI) series that adopts the European Standard, itself identical to an International Standard, for determination of the tensile properties of fabrics. The series specifies two methods: Part 1 uses the strip method to determine maximum force and elongation at maximum force; Part 2 uses the grab method to determine maximum force. Tensile properties (breaking force and elongation) are among the most important mechanical properties of fabrics, widely used to evaluate the strength and toughness of woven, knitted, and nonwoven fabrics and in quality acceptance. The technical content was jointly prepared by ISO/TC 38 “Textiles” and CEN/TC 248, and introduced into the British Standards system by BSI.
The series covers ICS 59.080.30 (Textile testing) and has two parts:
| Standard | Title | Main Content |
|---|---|---|
| BS EN ISO 13934-1:2013 | Textiles — Tensile properties of fabrics — Part 1: Determination of maximum force and elongation at maximum force using the strip method | Determines fabric maximum force and elongation at maximum force by the strip method |
| BS EN ISO 13934-2:2014 | Textiles — Tensile properties of fabrics — Part 2: Determination of maximum force using the grab method | Determines fabric maximum force by the grab method |
Part 1 was published in 2013, superseding BS EN ISO 13934-1:1999; Part 2 was published in 2014, superseding BS EN ISO 13934-2:1999. In the UK, technical responsibility is vested in committee TCI/24, Physical testing of textiles.
Part 1 specifies determination of fabric maximum force and elongation at maximum force at a constant rate of extension. The strip method uses a full-width strip specimen of specified width, stretched along its length at a specified gauge length and extension rate to rupture, recording maximum force (breaking force) and the corresponding elongation.
Specimen preparation and conditioning significantly affect results: specimens should be conditioned in a standard atmosphere (typically 20 °C, 65% RH) and sampled separately in warp and weft directions; strip width, gauge length, and extension rate follow the Standard. A sufficient number of tests (typically 5 per direction) should be averaged.
Part 2 specifies determination of fabric maximum force by the grab method. The grab method clamps only the central part of the specimen (typically smaller clamp width); the edges are free, closer to the local tensile loading in actual use. The measured force is usually lower than the strip method, because only the clamped region carries the main load.
| Method | Clamping | Measured | Typical Use |
|---|---|---|---|
| Strip method (Part 1) | Full width | Maximum force, elongation at max force | Overall fabric strength/elongation |
| Grab method (Part 2) | Partial (central) | Maximum force | Local strength evaluation |
The grab method also requires standard conditioning, separate warp/weft sampling, and sufficient repetition, reporting mean maximum force and coefficient of variation. Because clamping differs, grab and strip results are not directly comparable; choose based on the fabric’s actual use and acceptance requirement.
Fabric tensile-property determination is widely used in textiles, apparel, home textiles, and technical textiles: