🛣️ BS EN ISO 13473 is the British Standard (BSI) series that adopts the European Standard, itself identical to an International Standard, for characterization of pavement texture by use of surface profiles. The series specifies methods for characterizing pavement texture from measured surface profiles, including Part 1 for determination of Mean Profile Depth (MPD) and Part 5 for determination of megatexture. Pavement texture directly affects tyre–pavement friction, noise, drainage, and ride comfort, making it a key indicator in road engineering and traffic safety. The technical content was prepared by ISO/TC 43 “Acoustics” and relevant subcommittees, and introduced into the British Standards system by BSI.
The series covers ICS 17.140.30 (Noise) and 93.080.20 (Road materials and pavements), with two relevant parts in this batch:
| Standard | Title | Main Content |
|---|---|---|
| BS EN ISO 13473-1:2004 | Characterization of pavement texture by use of surface profiles — Part 1: Determination of Mean Profile Depth | Specifies determination of pavement mean profile depth from surface profiles |
| BS EN ISO 13473-5:2009 | Characterization of pavement texture by use of surface profiles — Part 5: Determination of megatexture | Specifies determination of pavement megatexture (large-scale texture) |
Part 1 was published in 2004, technically identical to ISO 13473-1:1997; Part 5 was published in 2009, renumbered from BS ISO 13473-5:2009 to BS EN ISO 13473-5:2009 by the 2010 corrigendum. In the UK, technical responsibility is vested in subcommittee B/510/5, Surface characteristics, under B/510 (Road materials).
Part 1 specifies determination of the mean profile depth of pavement macrotexture from surface profiles (surface height variation with distance). MPD is calculated by dividing the texture profile along the measuring line into segments; within each segment, the difference between the highest point and the mean line of the segment is averaged. This parameter corresponds to the texture depth measured by the sand-patch method (ETD) and is a key parameter for evaluating skid resistance and drainage.
In measurement, a high-resolution non-contact (e.g., laser) or contact profilometer collects surface-height data along the pavement line; after filtering to remove noise and slope effects, MPD is computed per the standard’s segmentation. Measurement should cover representative sections and consider traffic direction.
Part 5 specifies determination of pavement megatexture. Megatexture refers to surface irregularities of larger wavelength (typically on the order of 50 mm to 500 mm), affecting tyre–pavement noise, vehicle vibration, and drainage. Unlike macrotexture, megatexture concerns larger-scale surface undulation.
Megatexture is also determined from surface-profile measurements, characterized by analysing profile undulation within a larger wavelength range. The Standard specifies measurement equipment, filtering range, data processing, and reporting to ensure comparability between laboratories.
| Texture Scale | Typical Wavelength | Primary Effect |
|---|---|---|
| Microtexture | less than 0.5 mm | Tyre–pavement micro-adhesion, wet/dry friction |
| Macrotexture | 0.5–50 mm | Drainage, skid resistance, tyre noise |
| Megatexture | about 50–500 mm | Noise, vibration, drainage, comfort |