BS EN ISO 12625 — Tissue Paper and Tissue Products Test Methods Standard Series

Tissue Paper and Tissue Products — Test Methods (UK implementation of EN ISO 12625)

📐 BS EN ISO 12625 is the UK implementation of ISO 12625 / EN ISO 12625, the test-method series specialised for tissue paper and tissue products, overseen in the UK by BSI Technical Committee PAI/11 (Methods of test for paper, board and pulps). Because tissue has low grammage, high flexibility and strong absorbency, the series provides dedicated methods for thickness and bulk, grammage, tensile strength, wet strength, burst strength, absorbency and optical properties. It is the standardisation and quality-control basis for the toilet-tissue, facial-tissue, kitchen-towel and napkin industries. The complete set comprises 11 documents.

⚠️ Scanned version, written from public domain knowledge: the source material for this series is scanned (SCAN>0); the technical content below is summarised from publicly known information in the field, and the authoritative text is the official BSI publication.
💡 Tissue grammage is far below ordinary paper (typically 12–45 g/m²), and the fibre network is loose, porous and surface-weak. Many tests (tensile, burst, absorbency) therefore differ from the general paper standards (ISO 1924/2758/8787) in equipment and handling details — the dedicated 12625 methods must be used.

1. Scope and General Overview 📌

Tissue paper is a low-grammage, flexible paper made from pulp (virgin, recycled or blends) and its products (toilet rolls, boxed facial tissue, kitchen rolls, napkins, pocket tissues). ISO 12625 provides unified test methods for its physical and optical properties, ensuring comparable data across manufacturers and laboratories, and supporting product standards and market surveillance.

The series is organised by target: basic properties (Part 1 terms, Part 3 thickness/bulk, Part 6 grammage); mechanical properties (Part 4 dry tensile and stretch, Part 5 wet tensile, Part 11 wet ball burst, Part 9 ball burst); absorbency (Part 8 water-absorption time); and optical properties (Part 7 scattering/absorption coefficients, Part 15 brightness and colour, Part 16 opacity). Each part specifies sampling, conditioning, apparatus and result expression.

2. Series Structure and Technical Content 🔧

The table below summarises the 11 parts of BS EN ISO 12625 and their test targets. Each part corresponds to ISO 12625 and is referenced by part number in industry literature.

PartSubjectTest object and highlights
BS EN ISO 12625-1 (2011)Terms and general guidanceTerminology and general sampling guidance for tissue and products
BS EN ISO 12625-3 (2014)Thickness, bulking thickness and apparent bulk densityThickness at specified pressure (single/multi-ply) and bulk calculation
BS EN ISO 12625-4 (2016)Tensile strength, stretch at max force and TEADry tensile properties including tensile energy absorption
BS EN ISO 12625-5 (2016)Wet tensile strengthWet tensile after moistening (wet-wipe indicator)
BS EN ISO 12625-6 (2016)GrammageMass per unit area determination
BS EN ISO 12625-7 (2014)Optical — light scattering and absorption coefficientsKubelka-Munk parameters (drive opacity and brightness)
BS EN ISO 12625-8 (2010)Water absorption time (basket immersion)Time to complete water absorption under specified conditions
BS EN ISO 12625-9 (2015)Ball burst strengthDry ball-penetration burst strength
BS EN ISO 12625-11 (2012)Wet ball burst strengthBall-penetration burst strength after moistening
BS EN ISO 12625-15 (2015)Optical — brightness and colour (C/2°)ISO brightness and colour under D65/2° and C/2° conditions
BS EN ISO 12625-16 (2015)Optical — opacityOpacity of the sheet
💡 Many tissue properties are directional: machine-direction (MD) and cross-direction (CD) tensile differ significantly; for multi-ply products (2- or 3-ply embossed toilet tissue), thickness and strength must be measured per combined plies or per single ply as specified. Always state conditions and ply count in reports.

3. Key Technical Requirements 🔥

Key technical requirements across the series include:

  • Conditioning: all tests condition specimens in the specified atmosphere (conventionally 23 °C / 50% RH) and test under the same conditions to guarantee comparability.
  • Specimen preparation: sampling position, strip width/length and the separation of plies for multi-ply samples are specified, avoiding edge effects and emboss/crease influence.
  • Apparatus and grips: tensile tests use a precision tensile tester with specified gauge length and speed; burst uses a ball-burst device, distinct from the flat (Mullen) rupture method for board.
  • Absorbency test: Part 8 basket-immersion measures the time for a specimen of specified size to complete upward water absorption — a common “absorbency” indicator for kitchen towels.
  • Optical measurement: Parts 7/15/16 use standard illuminants (D65 or C) and geometry to measure brightness, colour, opacity and scattering/absorption coefficients, with strict light-source and viewing-geometry requirements.
🚨 Wet-state tests demand strict control of the moistening condition: immersion time, water temperature and specimen state significantly change wet-strength results; tissue is easily torn when wet, so manipulation (edge rolling, suspension) also biases results. Strictly follow the wetting and clamping steps of Parts 5/11 and record them.

4. Engineering Practice 🛠️

  • 🔍 Quality control: on the production line, grammage (Part 6) and thickness (Part 3) monitor basis-weight stability; dry/wet tensile balancing achieves “strong enough, not wasteful” strength design.
  • 🔧 New product development: use the strength (Parts 4/5/9/11) and absorbency (Part 8) indices to evaluate pulp type, embossing, creping and wet-strength additive recipes, iterating quickly.
  • 📊 Competitive benchmarking: industry tests (towel strength and absorbency) use the unified 12625 methods so conclusions remain traceable and comparable.
  • 📋 Compliance and market surveillance: third-party reports per 12625 support acceptance and surveillance of key indices required by product standards (e.g. toilet-tissue EN requirements).

5. Frequently Asked Questions ❓

❓ Q: How do 12625 and the general paper standards (ISO 1924, ISO 536) relate?
A: 12625 is the dedicated series for tissue characteristics; it revises and replaces the application of general standards to tissue (e.g. dedicated tensile and grammage editions) and adds wet-state and absorbency methods not in the general standards.
❓ Q: Why does wet tensile strength (Part 5) matter?
A: Wet strength determines the experience of wet wipes, flushable wipes and “does-not-break-when-wet” products; it is produced by adding wet-strength resins to the pulp and is the key indicator distinguishing dry-strength from wet-strength papers.
❓ Q: What is the difference between ball burst and the traditional Mullen burst?
A: Ball burst presses a ball into the sheet to penetrate it, suiting low-grammage, easily deformed tissue and reflecting local puncture resistance; Mullen (pressure diaphragm) is used on stronger board-like structures. They are not interchangeable.
🔍 Q: What is the difference between opacity (Part 16) and brightness (Part 15)?
A: Brightness measures how much light the sheet reflects (ISO brightness); opacity measures how well the sheet hides a background behind it (preventing see-through of print or contents). Print and visual quality depend on both working together.
🔒