BS EN ISO 11997 — Paints and Varnishes: Determination of Resistance to Cyclic Corrosion Conditions

Paints and varnishes — Determination of resistance to cyclic corrosion conditions — Salt-fog / dry / humidity and UV cycles

🧪 BS EN ISO 11997 is the BSI implementation of the EN ISO 11997 series, which defines test methods for determining the corrosion resistance of paint and varnish coatings under cyclic corrosion conditions. Unlike conventional continuous salt-spray testing, cyclic corrosion tests apply alternating environmental stresses — salt fog (wet), drying, humidity, and ultraviolet (UV) light — to more realistically reproduce the corrosion-weathering coupling of outdoor and industrial environments. The series is widely used for automotive, marine, bridge, and industrial coating systems. It comprises two parts: Part 1 is wet (salt fog)/dry/humidity, and Part 2 is wet (salt fog)/dry/humidity/UV light. It was prepared by ISO/TC 35 (Paints and varnishes) with CEN/TC 139, classified under ICS 87.040 (Paints and varnishes).

💡 Cyclic corrosion testing is closer to real service than a single salt-spray test: in actual use, a coating is attacked by salt and also subjected to wet-dry cycling, temperature changes, and UV degradation, which a single condition cannot fully evaluate.

1. Scope and General Framework 📌

This series applies to evaluating the protective performance of paints, varnishes, and related coatings (including primers, topcoats, and organic coatings over metallic substrates) in cyclic corrosion environments. The cyclic tests defined by the standard accelerate corrosion and simulate ageing by periodically changing environmental conditions (temperature, humidity, salt fog, drying, light), enabling a relative ranking of coating systems.

The scope of the standard includes:

  • Test object: paints, varnishes, and the composite coating systems they form, applied on metal or other substrates.
  • Test conditions: different combinations and cycles of salt fog, drying, humidity, and UV light.
  • Result evaluation: the corrosion resistance is assessed by the grade of defects such as blistering, rusting, cracking, flaking, and loss of gloss (typically per the ISO 4628 series).
⚠️ There is a correlation, but not a full equivalence, between cyclic corrosion test results and real outdoor exposure. The choice of cyclic parameters, salt-fog concentration, temperature, and humidity levels significantly affects the results and the corrosion mechanism; the purpose and acceptance criteria must be defined before testing.

2. Series Composition and Sub-parts 🗂️

Standard No.TitlePublishedMain Technical Content
BS EN ISO 11997-1:2006Paints and varnishes — Determination of resistance to cyclic corrosion conditions — Part 1: Wet (salt fog)/dry/humidityFebruary 2006Defines a salt-fog / dry / humidity alternating-cycle test method
BS EN ISO 11997-2:2013Paints and varnishes — Determination of resistance to cyclic corrosion conditions — Part 2: Wet (salt fog)/dry/humidity/UV lightSeptember 2013Adds a UV-light stage to the cycle, simulating corrosion-weathering coupling

Part 1 was first published as BS ISO 11997-1 in 2005 and renumbered as BS EN ISO 11997-1:2006 in February 2007; Part 2 was published by BSI in January 2014. Part 2 attracted a negative UK vote concerning the specification of light/dark period durations in clause 8.4 and the retention of informative Annex A, indicating that parameter details are debated — users should pay attention to the version and the specific cycle definition.

3. Part 1: Wet (salt fog)/dry/humidity Cycle 🌧️

Part 1 defines a typical “salt-fog-dry-humidity” cyclic corrosion test that simulates the salt deposition, wet-dry alternation, and high humidity that coatings experience in marine or industrial atmospheres. Key technical points:

  • Salt-fog stage: panels are placed in a salt-spray cabinet and sprayed with a sodium chloride solution of defined concentration and pH at a controlled temperature.
  • Drying stage: the spray is stopped and the panel surface is dried under specified temperature and humidity.
  • Humidity stage: panels are held under high temperature and humidity, promoting corrosion-product formation and coating water uptake.
  • Cycle period: salt fog, drying, and humidity follow the standard’s specified time sequence to form one cycle, repeated for the specified number of cycles.
  • Panel preparation: panels are prepared on the specified substrate, surface treatment, and coating thickness, with a scratch (scribed) line to evaluate corrosion spread from the defect.
🚨 The salt-fog stage requires strict control of the sodium chloride concentration, pH, and fog deposition rate, and prevention of nozzle clogging by salt crystals; deviations in time and temperature/humidity during the drying and humidity stages directly change the corrosion rate and distort results.

4. Part 2: Wet (salt fog)/dry/humidity/UV light Cycle ☀️

Part 2 adds a UV-light irradiation stage to the Part 1 cycle, forming a corrosion plus photo-ageing coupled cycle that more fully simulates outdoor coating service. Key technical points:

  • UV stage: panels are irradiated by UV fluorescent lamps, simulating the photo-degradation of coatings by solar UV radiation.
  • Light/dark cycle: the standard specifies the time allocation between light and dark periods (the UK committee raised reservations about the light/dark durations in clause 8.4).
  • Coupling effect: UV degradation creates micro-cracks, chalking, and loss of gloss on the coating surface, reducing its barrier function and accelerating subsequent salt-fog corrosion.
  • Equipment requirements: UV lamp irradiance, spectral distribution, and chamber temperature and humidity must be controlled per the standard.
  • Result evaluation: loss of gloss, chalking, colour change, cracking, and rusting are evaluated, combined with corrosion spread for an overall assessment.

5. Test Cycles and Equipment Requirements 🔧

Test ElementTypical RequirementNote
Salt-fog solutionSodium chloride solution of defined concentration, controlled pHSimulates marine/industrial salt
Salt-spray cabinet temperatureAt the specified temperature (e.g., near 35 °C)Affects corrosion rate
Drying/humidity conditionsSpecified temperature, humidity, and timeCreates wet-dry alternation stress
UV light (Part 2)Specified irradiance and spectrum, light/dark cycleSimulates solar UV ageing
Number of cyclesPer product requirement or standardDetermines total test duration
EvaluationDefect grades per ISO 4628, etc.Blistering, rusting, cracking, flaking, loss of gloss
✅ Cyclic corrosion testing gives a relative ranking of coating systems within a relatively short time by accelerated environmental stress, widely used for coating formulation screening, process validation, and product acceptance.

6. Engineering Practice and Applications 🛠️

  • 🚗 Automotive coatings: evaluate the combined corrosion resistance of e-coat primers, intermediate coats, topcoats, and anti-corrosion wax systems under salt-fog-dry-UV cycles.
  • 🚢 Ships and offshore equipment: evaluate the anti-corrosion performance of ballast-tank, hull, and offshore-platform coatings in marine atmospheres and seawater splash.
  • 🌉 Bridges and steel structures: verify the long-term protection capability of heavy-duty coating systems in industrial atmospheres and humid environments.
  • 🏭 Industrial equipment: screen and verify the corrosion and weathering resistance of surface coatings and powder-coating systems.
  • 📊 Formulation development: compare the corrosion resistance of different resins, pigments, additives, and curing systems to guide formulation optimisation.

7. Frequently Asked Questions ❓

❓ Q: How does a cyclic corrosion test differ from a continuous salt-spray test?
A: A continuous salt-spray test applies only sustained fog and corrosion is mainly electrochemical; a cyclic test alternately applies salt fog, drying, humidity (and UV), closer to real service, and reflects the coupling of wet-dry alternation, coating water uptake, and photo-ageing.
❓ Q: What is the purpose of a scribed (scratched) panel?
A: The scratch penetrates the coating to the substrate, used to evaluate corrosion spread at the defect (rust creepage width); it is an important indicator of protective performance, reflecting the coating’s ability to inhibit corrosion after damage.
❓ Q: Why does Part 2 add UV light?
A: UV light simulates solar ultraviolet radiation, causing photo-degradation (loss of gloss, chalking, cracking) that reduces the coating’s barrier performance and accelerates corrosion. Adding UV gives a combined “corrosion + ageing” evaluation of outdoor coatings.
❓ Q: Can test results directly predict service life?
A: No simple extrapolation is possible. Cyclic corrosion testing gives a relative ranking and accelerated-failure information; real life depends on environmental exposure, stress, maintenance, and many other factors, and requires correlation models built from outdoor exposure data.
🔒
正在加载下载地址,请稍候 10 秒

Leave a Reply

Your email address will not be published. Required fields are marked *