🌡️ BS EN ISO 11357 is the UK adoption by BSI of the ISO 11357 series covering differential scanning calorimetry (DSC) of plastics. DSC is one of the most widely used thermal analysis methods for polymer materials: by measuring the heat-flow difference between the sample and a reference, it reveals endothermic and exothermic behaviour of the material under controlled heating/cooling, allowing the determination of glass transition temperature, melting and crystallization temperature and enthalpy, crystallinity, specific heat capacity, characteristic reaction-curve temperatures and oxidation stability. The series comprises seven parts and is an essential tool for plastics R&D, quality inspection and failure analysis.
Some parts of this series were sourced from scanned documents; the technical content is compiled from publicly available domain knowledge and the authoritative text remains the official BSI publication.
BS EN ISO 11357 applies to DSC analysis of polymer materials and their articles, including thermoplastics, thermosets and rubbers. The standard specifies instrument calibration, specimen preparation, temperature programmes and data-processing methods, together with definitions and measurement procedures for the various thermal effects. The series is organised as “general principles (Part 1) + specific determination methods (Parts 2-7)”, ensuring consistency of instrument operation and data processing across methods.
The standard emphasises the significant influence of measurement conditions (heating rate, atmosphere, sample mass) on results, and requires complete recording of test conditions in the report to ensure comparability between laboratories.
The table below lists the subject and scope of each part.
| Part | Subject | Scope | Edition |
|---|---|---|---|
| BS EN ISO 11357-1 | General principles | DSC principles, instrument calibration, terminology | 2016 |
| BS EN ISO 11357-2 | Determination of glass transition temperature | Glass transition temperature and step height | 2014 |
| BS EN ISO 11357-3 | Determination of temperature and enthalpy of melting and crystallization | Melting and crystallization temperature and enthalpy | 2013 |
| BS EN ISO 11357-4 | Determination of specific heat capacity | Specific heat capacity | 2014 |
| BS EN ISO 11357-5 | Determination of characteristic reaction-curve temperatures | Characteristic reaction-curve temperatures | 2014 |
| BS EN ISO 11357-6 | Determination of oxidation induction time and temperature | Oxidation induction time (OIT) and temperature (OOT) | 2013 |
| BS EN ISO 11357-7 | Determination of crystallization kinetics | Crystallization kinetics | 2015 |
In the plastics industry, the 11357 series is widely used for material development, incoming inspection and quality management. R&D teams use DSC to determine the glass transition and crystallization behaviour of new formulations and optimise processing windows. Quality departments verify raw-material batch consistency with melting temperature and enthalpy. Failure-analysis engineers use oxidation induction time (OIT) to evaluate whether the antioxidant system has failed and diagnose the causes of product ageing.
Specific heat capacity (Part 4) is an important input for thermal design (e.g. injection-moulding cooling and heat-transfer calculations); crystallization kinetics (Part 7) provides data for modelling isothermal and non-isothermal crystallization and guides moulding process optimisation. DSC data has become standard information on material data sheets.