📐 BS EN ISO 11299 is the British Standard implementing the European Standard for plastics piping systems used in the renovation of underground gas supply networks. The standard was developed by ISO/TC 138 “Plastics pipes, fittings and valves for the transport of fluids”, taken over as a European standard by CEN/TC 155 “Plastics piping systems and ducting systems”, and published in the UK by BSI. This batch includes Part 1: General and Part 3: Lining with close-fit pipes, superseding the withdrawn BS EN 14408 series. It applies to the design and construction of trenchless renovation of medium- and low-pressure buried gas distribution networks, and is a key technical reference for gas network renewal and rehabilitation.
BS EN ISO 11299 is directed at the renovation of buried gas supply networks and specifies general requirements, material selection, design criteria, installation practice, quality control, and acceptance methods for plastics piping systems used in renovation works. Part 1 provides the general provisions, terms and definitions, symbols and abbreviations applicable to the whole series, together with the classification of renovation methods and selection principles. Part 3 gives dedicated requirements for the close-fit lining technique.
The standard applies to the renovation of buried plastics or metal networks conveying natural gas. The renovated pipe must satisfy gas conveyance and long-term tightness requirements, accounting for the specific effects of the gas medium on materials, connections, and sealing. Because gas is combustible, the standard imposes stricter provisions on safety assessment, leak detection, and acceptance criteria.
| Part | Standard No. | Title | Main Content |
|---|---|---|---|
| Part 1 | BS EN ISO 11299-1:2013 | General | Terms, symbols, classification of renovation methods, general design principles, material and system requirements, quality control foundations |
| Part 3 | BS EN ISO 11299-3:2013 | Lining with close-fit pipes | Materials, dimensions, installation process, reduction and reversion, connections, testing and acceptance of close-fit liners |
The series follows a “general part plus specific technique part” structure: Part 1 establishes the common framework, while the later parts give detailed provisions for particular renovation technologies. This batch includes the general part and the close-fit lining part; other renovation technique parts are covered by the corresponding standards.
The plastics piping system used for renovation must satisfy both gas conveyance and structural strength requirements. The liner material must have sufficient long-term hydrostatic strength, resistance to gas permeation, corrosion resistance, and suitability for gas conveyance. System design must account for the condition of the host pipe, groundwater pressure, traffic loads, and the internal pressure and long-term tightness requirements after renovation.
Close-fit lining is a technique in which a plastics liner is reduced in cross-section, pulled into the host pipe, and then restored to conform closely to the host pipe wall. Common implementation methods include the fold-and-form method, reduction methods, and heat reversion / memory-reversion methods. After installation the liner fits tightly against the original pipe with virtually no annular gap, reducing the risk of gas retention and diffusion in the annulus under gas service conditions.
The standard sets requirements for minimum liner wall thickness, reduction ratio, reversion recovery ratio, allowable bending radius, pulling load, connections, and end treatments. Prior to installation, CCTV inspection should be carried out to assess the condition of the host pipe; during installation, pulling speed and lubrication must be controlled; after installation, tightness testing and final inspection confirm that the renovated section is leak-free, wrinkle-free, and round.