Physical Address
304 North Cardinal St.
Dorchester Center, MA 02124
Physical Address
304 North Cardinal St.
Dorchester Center, MA 02124
🎵 BS EN ISO 10534 specifies methods for determining the sound absorption coefficient and normal acoustic impedance of materials using an impedance tube (standing-wave or acoustic tube). It is a fundamental standard in building acoustics, material acoustics, and noise control. The series has two parts: BS EN ISO 10534-1 uses the standing wave ratio method, and BS EN ISO 10534-2 uses the transfer-function method. Both rely on the plane-wave acoustic theory of sound propagation in a rigid-wall tube, reconstructing the normal incidence absorption coefficient and normal acoustic impedance of a specimen from the standing wave field or transfer function measured in the tube.
In the UK this series is the responsibility of subcommittee EH/1/6 (Building acoustics). It was prepared by ISO/TC 43 “Acoustics” with CEN/TC 126. BS EN ISO 10534-1:2001 is identical to ISO 10534-1:1996, was approved by CEN in June 2001, and published as a British Standard on 2 November 2001; BS EN ISO 10534-2:2001 is identical to ISO 10534-2:1998, was approved by CEN in June 2001, and implemented in the UK on 11 April 2002 (Amd. 13701).
| Part | Subject | ICS | ISO Equivalent | Method |
|---|---|---|---|---|
| BS EN ISO 10534-1:2001 | Standing wave ratio method | 91.120.20; 17.140 | ISO 10534-1:1996 | Determines absorption coefficient and impedance from the standing-wave ratio |
| BS EN ISO 10534-2:2001 | Transfer-function method | 17.140.01 | ISO 10534-2:1998 | Two-microphone transfer function determines absorption coefficient and impedance |
In the standing wave ratio method the specimen is placed at one end of the tube and a loudspeaker at the other. The loudspeaker excites a plane wave; the incident wave and the reflected wave from the specimen combine into a standing wave. A traversing probe microphone moves along the tube axis and measures the maximum sound pressure pmax and minimum pmin, giving the standing-wave ratio n = pmax/pmin, from which the absorption coefficient and normal acoustic impedance are calculated.
The method measures at discrete frequencies and requires point-by-point scanning at each test frequency, so it is relatively slow, but the equipment is simple and the principle intuitive — well suited as a reference or arbitration method. The Standard specifies specimen size, mounting, probe traverse accuracy, wall rigidity, and frequency range.
The transfer-function method uses two microphones at fixed positions to measure the sound pressure at two points simultaneously; the transfer function, together with the tube geometry and acoustic parameters, is used to reconstruct the specimen’s normal absorption coefficient and acoustic impedance. Compared with the standing wave method, no point-by-point scan is needed — a full continuous spectrum is obtained in one broadband measurement, giving higher speed and accuracy. It is now the routine laboratory method.
The Standard sets strict requirements for microphone spacing, microphone-to-specimen distance, tube diameter, environmental conditions (temperature, humidity, pressure) and calibration, to ensure accuracy and repeatability. Tests typically cover roughly 50 Hz up to 10 kHz or higher, depending on tube size and microphone layout.
| Comparison | Standing Wave Ratio (Part 1) | Transfer Function (Part 2) |
|---|---|---|
| Measurement mode | Point-by-point scan, discrete frequencies | Broadband continuous measurement |
| Microphones | Single traversing probe microphone | Two fixed microphones |
| Speed | Slower | Faster |
| Best suited for | Reference/arbitration, simple materials | Routine testing, spectral analysis |
To ensure comparability and repeatability the Standard specifies specimen preparation and mounting: the specimen must represent the actual product state, with thickness, density, porosity, etc. consistent with the real product; it must be flat and mounted tightly against the rigid back plate at the tube end with no edge leakage. Porous materials (mineral wool, glass wool, polyurethane foam) and fibrous materials should keep their original structure without compaction or distortion.
Impedance-tube testing is widely used for acoustic performance evaluation and quality control of building acoustic materials, automotive interiors, aircraft cabins, and industrial silencers. In building acoustics the absorption coefficient is used to calculate reverberation time, design room acoustics, and control noise; in silencer design the normal acoustic impedance is a key input for computing insertion loss and optimising structure.