🛢️ BS EN ISO 10407 is the British Standard series on petroleum and natural gas industries — rotary drilling equipment, developed jointly by ISO/TC 67 (Materials, equipment and offshore structures for petroleum, petrochemical and natural gas industries) and CEN/TC 12, with UK participation through BSI committee PSE/17/-/4 (Drilling and production equipment for petroleum and natural gas industries). In rotary drilling, the drill string (rotating drill tools made of drill pipe, drill collars, tool joints, stabilisers, etc.) withstands enormous torque, tension, bending and vibration loads, making it a critical element of drilling safety. The series provides systematic methods for the inspection and classification of used (old) drill stem elements, and is an important basis for re-use, quality traceability and safety control of drilling tools.
The series applies to drill stem elements in rotary drilling equipment; this batch corresponds to Part 2: Inspection and classification of used drill stem elements (the standard is available in both English and Russian text versions). This part specifies the inspection content, inspection methods, defect assessment, classification criteria and re-use determination for used drill pipe, drill collars, tool joints, lifting subs and other drill stem elements.
During service, drill stem elements undergo wear, corrosion, fatigue, erosion and mechanical damage, and their load capacity decreases with service time. This part determines the damage state of the element through systematic inspection and classifies it according to the standard, providing the basis for continued use, downgraded use or scrapping.
| Standard Part | Subject | Object | Key Content |
|---|---|---|---|
| BS EN ISO 10407-2:2008 | Inspection and classification of used drill stem elements | Used drill pipe, drill collars, tool joints, etc. | Inspection content, methods, defect assessment, classification, re-use determination |
This part is one of the core parts of the ISO 10407 series, used together with Part 1 (general requirements for rotary drilling equipment) and ISO 10424 (drill stem elements and threaded connections), covering design, manufacture, inspection and re-use management of the drill string.
Carry out visual inspection and dimensional measurement of drill stem elements, checking wear (outside-diameter wear, tool-joint wear), bending, ovality, thread damage, erosion and mechanical damage, and measuring wall thickness and diameter to determine whether allowable limits are exceeded.
Use magnetic particle inspection (MPI), ultrasonic testing (UT), penetrant testing (PT) and other NDT methods to check surface and near-surface cracks, fatigue defects and inclusions, focusing on critical areas (such as thread roots, stress-concentration zones and upset transition zones).
Where necessary, perform material property tests (such as hardness, metallography, chemical analysis) to assess the degree of material degradation (fatigue, hydrogen embrittlement, corrosion fatigue) and estimate remaining life from service history (cycle count, load spectrum).
Based on defect type, size, location and severity, the standard divides used drill stem elements into several grades (such as fit for continued use, downgraded use, use after repair, scrap) and specifies corresponding re-use criteria. The main factors considered in classification include: