BS EN ISO 08781 — Assessment of Dispersion Characteristics of Pigments and Extenders Standard Series (Tinting Strength, Fineness of Grind and Gloss)

Pigments and Extenders — Methods of Assessment of Dispersion Characteristics (ISO 8781 Series)

🎨 BS EN ISO 8781 is the series of standards on methods of assessment of dispersion characteristics of pigments and extenders, published by the British Standards Institution (BSI) as the UK implementation of EN ISO 8781, with technical content identical to ISO 8781. The performance of pigments in coatings, inks and plastics depends largely on how well they disperse in the binder system: the more thorough the dispersion, the better the tinting strength, hiding power, transparency and gloss. The series has three parts: Part 1 specifies assessment from the change in tinting strength of coloured pigments, Part 2 assessment from the change in fineness of grind, and Part 3 assessment from the change in gloss. The series corresponds to the BS 3483 pigment test methods.

💡 The “ease of dispersion” of a pigment determines the energy and efficiency of the grinding process: an easily dispersible pigment reaches its final tinting strength with little grinding work, while a difficult one needs long grinding time and may cause colour deviation and gloss defects.

1. Series Structure and Scope 📌

The series corresponds to ISO 8781 (originally the BS 3483-E series), developed by ISO/TC 35 (Paints and varnishes) working groups. In 1994 CEN adopted the ISO 8781 parts as European standards; from 1995 the UK renumbered them as BS EN ISO 8781. The structure is:

StandardTitle (English subject)Assessment Parameter
BS EN ISO 8781-1:1995Assessment from the change in tinting strength of coloured pigmentsRate of development of tinting strength (identical to ISO 8781-1:1990)
BS EN ISO 8781-2:1995Assessment from the change in fineness of grindChange in fineness of grind (identical to ISO 8781-2:1990)
BS EN ISO 8781-3:1995Assessment from the change in glossChange in gloss (identical to ISO 8781-3:1990)
⚠️ The series is used with ISO 8780 (methods for dispersion): ISO 8780 specifies how to prepare dispersions for assessment (e.g. oscillatory shaking machine, high-speed impeller mill), while ISO 8781 specifies how to assess the dispersion characteristics. They are inseparable.

2. Basic Principles of Pigment Dispersion 🔧

Pigments are solid particle agglomerates that must pass through three stages — wetting (the binder replaces surface air), deagglomeration (mechanical work breaks agglomerates into primary particles or small aggregates) and stabilisation (preventing re-agglomeration) — to form a stable dispersion. Dispersion characteristics are the amount of grinding work needed to reach the final optical properties (tinting strength, fineness, gloss): the less work required, the easier the dispersion and the better the dispersibility.

💡 Dispersion characteristics result from both the pigment’s intrinsic properties (particle size, surface treatment, crystal form) and the dispersion process (equipment, energy input). By sampling at successive dispersion stages and measuring property development, the ease of dispersion can be objectively assessed.

3. Part 1: Assessment from Change in Tinting Strength 🔬

Part 1 (BS EN ISO 8781-1) assesses dispersion characteristics by the rate of development of tinting strength of coloured pigments. Tinting strength is the ability of a pigment to impart colouring strength to a system; the better the dispersion, the higher the tinting strength. Method essentials:

  • Staged dispersion: prepare a series of dispersions by the appropriate ISO 8780 method in stages (progressively increasing grinding work).
  • Preparation of reduced pastes: prepare white-reduced (let-down) pastes from each dispersion stage and measure tinting strength.
  • Assessment: calculate the percentage increase in tinting strength with grinding work, or plot the rate of development, to judge ease of dispersion.
🚨 Tinting strength measurement is sensitive to dispersion concentration, grinding conditions and let-down ratio. Sample quantities, grinding time and measurement procedure must be consistent across stages, otherwise the “tinting strength — grinding work” curve is distorted and dispersibility is misjudged.

4. Part 2: Assessment from Change in Fineness of Grind 📏

Part 2 (BS EN ISO 8781-2) assesses dispersion characteristics by the change in fineness of grind. Fineness of grind reflects the size of residual coarse pigment agglomerates in the dispersion and is measured with a grindometer (Hegman gauge). Method essentials:

  • Staged dispersion: prepare staged dispersions per ISO 8780.
  • Fineness measurement: measure the fineness of grind of each stage with a grindometer (e.g. Hegman fineness, in µm).
  • Assessment: fineness becomes finer as grinding work increases; if the final fineness is easily attained, the pigment is considered readily dispersible.
💡 The grindometer reading represents the coarsest particle size in the dispersion and is an important indicator for controlling the grinding end point. When dispersion is good, fineness falls rapidly and stabilises at the target; a stagnant fineness indicates poor dispersibility or low grinding efficiency.

5. Part 3: Assessment from Change in Gloss 🛠️

Part 3 (BS EN ISO 8781-3) assesses dispersion characteristics by the change in gloss. Gloss is sensitive to film surface roughness and pigment dispersion state. Method essentials:

  • Staged dispersion: prepare staged dispersions per ISO 8780.
  • Film preparation: prepare and dry films from each stage dispersion.
  • Gloss measurement: measure the gloss of each film at the specified angle (e.g. 60° gloss).
  • Assessment: gloss increases with grinding work; rapid gloss development indicates thorough dispersion and good dispersibility.
⚠️ The gloss method is sensitive to film preparation conditions (film thickness, drying conditions, substrate) and suits gloss-sensitive systems. Poor dispersion in high-gloss films shows as reduced gloss and increased haze.

6. Engineering Practice and Application 🏭

  • 🔍 Pigment batch evaluation: evaluate dispersion stability of different pigment batches at incoming inspection.
  • 🔧 Grinding process optimisation: determine optimum grinding time and equipment parameters from the “tinting strength/fineness/gloss — grinding work” curves.
  • 📊 Formulation development: assess pigment-binder compatibility and guide the selection and dosage of wetting and dispersing agents.
  • 📋 Quality tracing: abnormal dispersion characteristics can be traced to changes in raw material particle size, surface treatment or process, supporting quality control.

7. Frequently Asked Questions ❓

❓ Q: Can the three assessment methods (tinting strength, fineness, gloss) substitute for one another?
A: Not completely. The three methods reflect dispersion from optical performance, particle size and surface state, and suit different pigment types and systems: Method 1 suits coloured pigments, Method 2 most systems, Method 3 gloss-sensitive systems.
❓ Q: Is better dispersion always economically optimal?
A: Usually yes, but over-grinding brings energy, equipment wear and over-grinding risks. Engineering seeks the “right dispersion end point” rather than unlimited fineness, balancing performance and cost.
❓ Q: Why does the same pigment vary in dispersibility between batches?
A: Particle size distribution, surface treatment (coating), moisture content and agglomeration state are affected by production process and fluctuate between batches, affecting ease of dispersion. This is why dispersion characteristics are evaluated at incoming inspection.
❓ Q: What is the relationship between ISO 8780 and ISO 8781?
A: ISO 8780 specifies methods for preparing dispersions (equipment and operation); ISO 8781 specifies how to assess the dispersion characteristics (tinting strength/fineness/gloss) after preparation. When using ISO 8781, dispersions must be prepared per ISO 8780.
🔒
正在加载下载地址,请稍候 10 秒