BS EN ISO 08394 — Building Construction Jointing Products — Determination of Extrudability of Sealants Series

Building construction — Jointing products — Determination of extrudability of sealants (ISO 8394 series)

🏗️ BS EN ISO 8394 is a British Standard published by BSI implementing the European Standard EN ISO 8394. It specifies methods for determining the extrudability of sealants used for building joints. Extrudability reflects how easily a sealant can be forced out of its container under application pressure and is a key indicator of the workability of a sealant. The series has two parts: Part 1 specifies the determination of extrudability in general, while Part 2 specifies determination using a standardized apparatus. Together the two parts supersede the earlier BS EN 28394:1991.

💡 Extrudability directly determines whether a sealant can be smoothly and evenly applied into a joint on site. Poor extrudability causes application difficulty, incomplete beads, or even impossible application; overly good extrudability can lead to sagging or flow problems.

1. Series Structure and Scope 📌

The BS EN ISO 8394 series has two parts, both falling under ICS 91.100.50 (adhesives / joint sealers for construction):

PartStandard No.ContentTypical Use
Part 1BS EN ISO 8394-1:2010Determination of extrudability of sealantsGeneral extrudability evaluation
Part 2BS EN ISO 8394-2:2010 (incl. corrigendum May 2011)Determination using standardized apparatusStandardized, reproducible measurement

The technical content was developed by ISO/TC 59 “Buildings and civil engineering works” together with CEN/TC 349 “Sealants for joints in building construction”; UK participation was entrusted to BSI Technical Committee B/547, “Sealants for building and construction”. Parts 1 and 2 together supersede BS EN 28394:1991.

2. Definition and Test Principle 🔍

Extrudability is the quantity (usually by volume or mass) of sealant extruded through a nozzle of specified bore within a specified time under a standard extrusion force or pressure and prescribed conditions. The test essentially simulates the process of forcing a sealant out of a gun or tube during actual application.

The basic principle is: load the sealant into a prescribed container or cartridge, apply a standardized pressure or thrust, force the sealant through a nozzle of specified bore, and measure the extruded quantity over a given time or stroke. The larger the extruded quantity and the smaller the required force, the better the extrudability and workability of the sealant.

⚠️ Extrudability is strongly temperature-dependent. Rising temperature lowers viscosity, increases flow and improves extrudability; falling temperature does the opposite. The Standard therefore prescribes standard test temperature, and since results are temperature-sensitive, ambient temperature must be strictly controlled.

3. Standardized Apparatus and Test Conditions 🔧

The essence of Part 2 is the use of a standardized apparatus so that results from different laboratories and batches are comparable. A standardized apparatus typically includes:

  • Cartridge or container: specified volume and dimensions to ensure consistent loading.
  • Plunger / piston: applies a standardized, measurable, constant extrusion force or pressure.
  • Nozzle: specified bore and length, simulating an actual application nozzle.
  • Timing and metering devices: to record extrusion time and quantity accurately.

The typical procedure is:

  • Condition the sealant at the standard temperature (e.g. 23 °C) to reach thermal equilibrium;
  • Load the sealant into the standard cartridge, expelling air bubbles;
  • Fit the standard nozzle and drive the piston at the standard pressure;
  • Measure the mass or volume extruded within the specified time;
  • Calculate the extrusion rate (e.g. g/s or mL/s) per the Standard’s formula, or record the time to extrude a fixed quantity.

4. Result Assessment and Influencing Factors 📊

Results are usually expressed as an extrusion rate or the quantity extruded at a prescribed pressure. Acceptance criteria vary by product standard but generally require:

  • An extrusion rate not below a lower limit, to ensure application efficiency;
  • Continuous, uniform extrusion with no interruption, no abnormal particle blockage;
  • A smooth extrudate surface, free from bubbles or lamination.

Main factors affecting extrudability include:

  • Temperature: higher temperature lowers viscosity and improves extrudability;
  • Formulation: polymer type, filler content, plasticizer dosage and thixotropic agents all affect viscosity and rheology;
  • Storage time and conditions: thixotropic changes, thickening or curing during storage can degrade extrudability;
  • Nozzle bore: a smaller bore raises extrusion resistance and makes extrusion harder.
💡 Extrudability is closely related to thixotropy. A quality sealant keeps a higher viscosity at rest (anti-sag) but its viscosity drops under shear during application (easy to extrude). This “shear-thinning” behaviour is central to sealant workability.

5. Engineering Practice Applications 🛠️

Extrudability testing is of significant engineering importance in curtain walls, door and window sealing, waterproofing and related fields:

  • 🔍 Workability verification: during procurement and incoming inspection, extrudability tests confirm the sealant can be applied smoothly under site conditions, avoiding rework.
  • 📋 Formulation and process control: manufacturers monitor extrudability to verify formulation stability and production consistency between batches.
  • 🔧 Site adaptation: for low-temperature application, choose sealant grades that retain good extrudability at low temperature, or adopt preheating measures.
  • 📊 Product standard compliance: many sealant standards list extrudability as a release-test item and an important basis for product acceptance.

6. Frequently Asked Questions ❓

❓ Q: What is the difference between Parts 1 and 2 of BS EN ISO 8394?
A: Part 1 specifies the general method based on principle and general procedure; Part 2 specifies measurement with a standardized apparatus for better reproducibility and interlaboratory comparability. They can be used together, with Part 2 preferred where strict, cross-comparable results are required.
❓ Q: Why must the test be carried out at a specified temperature?
A: Sealant viscosity varies significantly with temperature, which directly affects extrusion resistance. Testing at a standard temperature (e.g. 23 °C) ensures comparable results that reflect the product’s inherent workability.
❓ Q: Does poor extrudability always mean poor sealant quality?
A: Not necessarily. Poor extrudability may be caused by low temperature, long storage, or an overly fine nozzle; but it can also indicate formulation ageing or thickening. Judge in the light of product standards, application conditions and storage state.
🔍 Q: How should “shear-thinning” behaviour of sealants be understood?
A: Many sealants are thixotropic: viscosity is high at rest (no sagging) but drops under shear (extrusion, trowelling), allowing easy flow. This property makes the sealant easy to apply while keeping shape stability within the joint.
🔒