BS EN ISO 07093 — Plain Washers, Large Series (Product Grades A and C)

Part 1: Product Grade A and Part 2: Product Grade C (ISO 7093)

šŸ”§ BS EN ISO 7093 specifies the dimensions, tolerances, materials and surface treatment of large series plain washers, among the most commonly used washer product standards in bolted connections. Plain washers enlarge the bearing area beneath the bolt head or nut, protect the surface of the joined parts, spread the load and prevent local crushing. The “large series” denotes a larger outside diameter than the normal series, suited to soft joined parts or applications requiring a larger bearing area. In the UK the series is implemented under Technical Committee FME/9, “Bolts, nuts and accessories”, as the official British adoption of ISO 7093 and EN ISO 7093, classified under ICS 21.060.30.

šŸ’” Small as they are, washers matter: on wood, plastic, sheet metal and aluminium, large series plain washers significantly reduce contact stress, preventing the bolt head or nut from being pressed into the joined part — a common way to keep a joint reliable and its appearance intact.

1. Scope and General Framework šŸ“Œ

The series applies to plain washers, in two parts by product grade:

  • BS EN ISO 7093-1:2000: specifies product grade A plain washers — the tightest dimensional tolerances and highest precision, for precision assembly.
  • BS EN ISO 7093-2:2000: specifies product grade C plain washers — wider tolerances and better economy, for general use.

Both parts use the “large series”, i.e. for the same thread size the outside diameter and thickness are greater than the normal series, giving a larger bearing area. The standard gives nominal dimensions (bore, outside diameter, thickness), tolerances, material and surface-treatment requirements, and marking rules.

āš ļø The main difference between grades A and C is the tolerance band: grade A washers have tighter bore, outside-diameter and thickness tolerances, matching high-precision bolts; grade C washers have wider tolerances and lower cost, for general industrial and construction use. Choose by the assembly accuracy required.

2. Series Structure and Technical Highlights šŸ”¢

StandardTitleProduct gradeTolerance characteristics
BS EN ISO 7093-1:2000Plain washers — Large series — Part 1: Product grade AA (precision)Strict bore, outside-diameter and thickness tolerances
BS EN ISO 7093-2:2000Part 2: Product grade CC (general)Wider tolerances, economical

Both parts share the same large-series sizes and differ only in tolerance grade, so designers can select flexibly by precision and economy.

3. Dimensions and Tolerances šŸ“

The standard specifies the key dimensions and tolerances:

  • Bore (d₁): slightly larger than the nominal thread diameter of the mating bolt, so the washer slides on freely.
  • Outside diameter (dā‚‚): the large-series outside diameter is noticeably larger than the across-flats size of the bolt head or nut, giving a larger bearing area.
  • Thickness (h): set by the washer size, sufficient rigidity to prevent crushing and deformation.
  • Edges and fillets: rounded edges on the bore and outside, avoiding damage to the bolt and the bearing surface.
āœ… Selection pointers: the washer bore should be slightly larger than the nominal thread diameter; choose outside diameter and thickness from the permissible contact stress of the joined parts and the bolt size; for soft materials (aluminium, plastic, wood) prefer the large series to reduce contact stress.

4. Materials and Surface Treatment šŸ”§

Plain washers are usually made of carbon steel, with surface treatment according to the service environment:

  • Material: generally carbon steel (e.g. stamped from cold-rolled or hot-rolled sheet); stainless steel, brass and other special materials are also available.
  • Surface treatment: zinc plating, nickel plating, dacromet, blackening, etc., for corrosion protection and improved assembly behaviour.
  • Hardness: the washer must have sufficient hardness and rigidity to avoid indentation and deformation under preload.
🚨 A washer that is too thin or too soft will be indented or even pushed through under bolt preload, losing preload and loosening the joint; in high-strength bolted connections, select washers of hardness matched to the bolt strength.

5. Application Essentials and Marking šŸ“‹

The role of plain washers in bolted connections and key selection points:

  • Spreading contact stress: place washers on thin-wall, soft or cast bearing surfaces to prevent local crushing.
  • Surface protection: prevent the bolt head or nut from scratching the joined surface when rotating, helping appearance and corrosion protection.
  • Gap filling: within limits, compensate for uneven joined surfaces and improve load distribution.
  • Marking: mark the standard number, size, material and (where required) surface treatment per the standard, ensuring traceability.

6. Frequently Asked Questions ā“

ā“ Q: What is the difference between the large series and the normal series?
A: Large-series washers have a larger outside diameter and thickness, giving a larger bearing area for the same bolt size; they suit soft or thin-wall joined parts, while the normal series is more compact for general use.
ā“ Q: How do I choose between grades A and C?
A: Choose grade A for high-precision, precision assembly; choose grade C for general industrial and construction use where tolerance is not critical, to reduce cost.
ā“ Q: Why is the washer bore slightly larger than the thread diameter?
A: So the washer slides onto the bolt freely and seats properly, avoiding the washer edge engaging the thread and ensuring the preload is transmitted evenly to the bearing surface.
ā“ Q: When must large-series washers be used?
A: When the joined parts are soft materials such as aluminium alloy, plastic, wood or thin sheet, or where contact stress approaches the allowable value of the material, use large-series washers to prevent crushing.
ā“ Q: Does the series suit high-strength bolts?
A: Plain washers can be used with bolts of any strength, but high-strength joints need washers of adequate hardness, and the load capacity and thickness must be checked to match.
🔒
ę­£åœØåŠ č½½äø‹č½½åœ°å€ļ¼ŒčÆ·ēØå€™ 10 ē§’

Leave a Reply

Your email address will not be published. Required fields are marked *