🔧 BS EN ISO 6520 is a foundational classification standard in the field of weld quality. It systematically classifies and codes the geometric imperfections that may occur in welds, providing a common “language” for the identification, recording, assessment and acceptance of weld defects. In the United Kingdom the series is implemented under the responsibility of Technical Committee WEE/1, “Definitions and symbols for welding”, and constitutes the official British adoption of both ISO 6520 and EN ISO 6520, classified under ICS 25.160.40. Whether the process is arc welding, gas welding, laser welding or electron beam welding among the fusion processes, or resistance welding, friction welding and explosion welding among the pressure processes, the imperfections in the resulting joints can be matched to a classification code in this series.
💡 The ISO 6520 classification is the universally recognised “dictionary of weld imperfections” in international welding engineering: acceptance standards such as EN ISO 5817 and EN ISO 10042, as well as documents issued by the International Institute of Welding (IIW), refer to this series’ imperfection numbers when specifying permitted imperfection types and limits.
1. Scope and General Framework 📌
The series comprises two parts, covering the two broad families of welding processes:
- BS EN ISO 6520-1:2007 (Fusion welding): specifies the classification and numbering of geometric imperfections in metallic materials welded by fusion welding. It supersedes the 1998 edition and was approved by CEN in April 2007, replacing EN ISO 6520-1:1998.
- BS EN ISO 6520-2:2013 (Welding with pressure): specifies the classification and numbering of geometric imperfections occurring in metallic materials welded by pressure welding. Approved by CEN in April 2013, it supersedes EN ISO 6520-2:2001 (the UK 2002 edition).
Both parts emphasise that they deal only with imperfections related to geometry — cracks, cavities, inclusions, lack of fusion and shape deviations, for example — and not with nonconformities in chemical composition or mechanical properties. It is important to understand that the series defines a classification framework; whether an imperfection is acceptable and what size limits apply are not specified here, but in the relevant product or acceptance standards such as EN ISO 5817.
⚠️ Always distinguish “classification” from “acceptance” when using this series: ISO 6520 tells you what the imperfection is and what number it carries; whether it is acceptable and its permitted size must be established from the applicable weld acceptance standard. Never treat a classification number as an acceptance criterion.
2. Series Structure and Technical Highlights 🔢
| Standard | Title | Scope | Supersedes |
| BS EN ISO 6520-1:2007 | Classification of geometric imperfections in metallic materials — Part 1: Fusion welding | All fusion welding processes (arc, gas, laser, electron beam, etc.) | BS EN ISO 6520-1:1998 |
| BS EN ISO 6520-2:2013 | Classification of geometric imperfections — Part 2: Welding with pressure | Resistance, friction, explosion and ultrasonic welding, etc. | EN ISO 6520-2:2001 |
The two parts share identical classification principles and numbering conventions, differing only in the imperfection entries particular to each process family. This “same system, divided parts” structure keeps the concept of imperfections consistent across fusion and pressure welding while leaving room for future extension to other processes such as brazing.
3. The Classification and Numbering System 🧩
The core of ISO 6520 is a three-digit code assigned to each family of geometric imperfections. The first digit identifies the imperfection group and the following digits identify the specific form. The principal groups include:
- Group 100 — Cracks: longitudinal cracks, transverse cracks, star cracks, crater cracks and more, further subdivided by location (internal, surface, heat-affected zone).
- Group 200 — Cavities: gas pores (uniformly distributed, localised, aligned, wormhole), shrinkage cavities and crater pipes.
- Group 300 — Solid inclusions: slag inclusions, flux inclusions, oxide inclusions and metallic inclusions such as tungsten and copper.
- Group 400 — Lack of fusion and penetration: lack of side fusion, lack of inter-run fusion, incomplete root penetration and similar.
- Group 500 — Imperfect shape: undercut, excess weld metal, misalignment, angular distortion, excessive convexity, sagging, overlap and irregular width.
- Group 600 — Miscellaneous imperfections: arc strikes, spatter, grinding marks and tack weld defects.
🚨 Always use the complete code, down to the last digit: 201 (gas pore) and 202 (localised porosity), for example, are subject to different limits in acceptance standards. If an inspection record merely states “Group 200 porosity”, the assessor cannot judge acceptance. Reports should carry the full three-digit (or appended) code.
4. Unified Terminology and Symbols 📖
To build a consistent understanding across industry, each imperfection in the series is presented with three elements: a verbal definition, an illustration and a code number. The illustration supports visual comparison, the definition removes ambiguity, and the number enables data exchange and statistics. This “word + picture + number” combination allows weld inspectors in different countries, companies and agencies to reach the same conclusion about the same imperfection — by far the most valuable practical contribution of the ISO 6520 series.
💡 The most common working combination is ISO 6520 together with EN ISO 5817 (quality levels of imperfections in fusion-welded joints in steel, nickel, titanium and their alloys): first identify and code the imperfection per ISO 6520, then judge acceptability against quality level B, C or D in EN ISO 5817.
5. Engineering Practice 🛠️
- 🔍 Standardised inspection records: use ISO 6520 codes in weld inspection reports and NDT reports (RT/UT/MT/PT), e.g. “201 gas pore, 2 mm diameter”, to support traceability and statistics.
- 📊 Defect statistics and quality improvement: grouping production defects by code quickly reveals high-frequency imperfection types, giving data-driven direction for optimising welding parameters.
- 📋 Referencing in specifications: write ISO 6520 codes into procurement technical agreements and Welding Procedure Specifications (WPS) so that both supplier and purchaser share an explicit understanding of what is and is not permitted.
- 🔧 Alignment with quality systems: repair management and record keeping required by ISO 3834 (quality requirements for welding) rely on the same unified defect language, for which this series is the foundation tool.
✅ Recommended practice: link ISO 6520 codes in your weld-quality organisation to an internal library of defect photographs and Repair Procedure Specifications (RWP), building a “code — picture — disposition” knowledge base that sharply reduces the training time of new inspectors.
6. Frequently Asked Questions ❓
❓ Q: Does ISO 6520 apply only to steel?
A: No. The scope covers “metallic materials” generally — steel, aluminium, titanium, nickel and their alloys — and Part 1 (fusion welding) is the most broadly applicable.
❓ Q: What is the difference between “100 cracks” and “101 micro-cracks”?
A: 101 micro-cracks is a subdivision of group 100 reserved for very small cracks that only become visible under magnification. Always select the closest final digit for the actual imperfection morphology.
❓ Q: What size limits does ISO 6520 set?
A: None. The series only classifies. Permitted imperfection types, numbers and sizes are given by product or acceptance standards, such as the quality levels of EN ISO 5817.
❓ Q: Do the Part 1 and Part 2 numbers ever conflict?
A: No — the numbering, and the meaning of most codes, is consistent across the two parts. Differences appear only for imperfections specific to pressure welding (e.g. resistance welding expulsion or poor fit-up). Always state which part you are citing.
❓ Q: How does the British version differ from the European one?
A: BS EN ISO 6520 is the UK edition of EN ISO 6520 — the text is identical, with an added National foreword and committee information, published under the BS prefix.