BS EN ISO 03377 — Leather Physical and Mechanical Tests Tear Load Determination Standard Series (Single Edge and Double Edge Tear)

Leather — Physical and Mechanical Tests — Determination of Tear Load — Part 1: Single Edge Tear; Part 2: Double Edge Tear (ISO 3377-1:2011 / ISO 3377-2:2016)

🧥 BS EN ISO 3377 specifies methods for determining the tear load of leather. Tear load is an important mechanical property of leather, reflecting its resistance to tearing under load, and directly determines the durability of leather products such as shoe uppers, garments, sofas, bags and automotive interiors. The series comprises Part 1 (single edge tear) and Part 2 (double edge tear), providing test methods for different tearing modes, and is widely used in quality inspection and material evaluation of leather and leather products.

💡 Leather is an anisotropic material: its tear performance varies with sampling direction (parallel/perpendicular to the backbone), location and tanning process. The standard specifies sampling direction, specimen shape and conditioning to ensure comparability of results.

1. Series Composition and Scope 📌

The BS EN ISO 3377 series consists of two parts distinguished by tearing mode:

PartStandard TitleTearing ModeKey Feature
BS EN ISO 3377-1Leather — Physical and mechanical tests — Determination of tear load — Part 1: Single edge tear (2011)Single edge tear (single cut)One end of the specimen is cut; tearing starts from the cut and the tear load is measured
BS EN ISO 3377-2Leather — Physical and mechanical tests — Determination of tear load — Part 2: Double edge tear (2016)Double edge tear (two cuts)Two opposing cuts are made in the middle; tear load is measured as tearing proceeds from the centre
⚠️ Single and double edge tear reflect tearing behaviour under different loading modes and are not directly interchangeable. Choose the part according to the product’s service conditions and the requirements of the relevant product standard.

2. Principle of Tear Load Determination 🔧

Basic principle: A leather specimen of specified shape is stretched on a tensile testing machine at a specified speed so that tearing starts from the cut; the maximum load during tearing is recorded as the tear load. The higher the tear load, the stronger the leather’s resistance to tearing.

Test conditions: The standard specifies specimen shape and size, cut direction, test speed, grip separation and conditioning conditions. Tests are performed at specified temperature and humidity, with specimens conditioned to moisture equilibrium.

ElementDescription
SamplingCut specimens at the specified location and direction (parallel/perpendicular to the backbone)
Specimen shapeRectangular or specified shape, with a single cut (Part 1) or two cuts (Part 2)
ConditioningCondition to moisture equilibrium in the specified standard atmosphere
ProcedureStretch at the specified speed and record the maximum tear load
Expression of resultsTear load (N); average of multiple determinations with scatter reported
💡 The tear load reading should be taken as the maximum load during complete tearing of the specimen, avoiding misreading due to grip slip or abnormal specimen fracture.

3. Single Edge Tear (Part 1) and Double Edge Tear (Part 2) — Key Points 🔩

Part 1 — Single edge tear: One end of the specimen has a single cut perpendicular to the direction of pull; the crack propagates from the cut during stretching. This method simulates tearing under unilateral loading and is commonly used to evaluate edge tearing and the propagation of local defects.

Part 2 — Double edge tear: The middle of the specimen has two opposing cuts; during stretching the specimen tears from the centre outwards. This method simulates tearing under bilateral loading and reflects the overall tear resistance of the leather, commonly used for shoe upper and garment leather.

MethodNumber of cutsLoading modeTypical Application
Single edge tear (Part 1)One cutUnilateral tearingEdge tearing, defect propagation evaluation
Double edge tear (Part 2)Two cutsBilateral tearingOverall tear resistance of shoe upper, garment leather
⚠️ Specimen preparation should avoid burrs, notches or deformation at the cuts; the cuts should be flat and sharp, otherwise stress concentration changes and the tear load result is affected.

4. Key Technical Requirements and Quality Assurance 📏

  • Sampling direction: Leather is anisotropic; sampling direction (parallel/perpendicular to the backbone) significantly affects results, so sample in the direction specified by the standard.
  • Conditioning: Specimens must be conditioned to moisture equilibrium under standard atmosphere; humidity significantly affects leather mechanical properties.
  • Equipment calibration: Tensile testing machines should be calibrated periodically; grips and test speed must meet the standard.
  • Result reporting: Report average tear load, scatter, sampling direction and conditioning conditions.
✅ Using the ISO 3377 series, tear load of leather can be standardly determined, providing a reliable basis for leather product design and material acceptance.

5. Engineering Practice Applications 🛠️

  • Material acceptance: Testing the tear load of shoe upper, garment, sofa and other leather per product standards.
  • Process evaluation: Assessing the effect of tanning, fatliquoring and finishing processes on leather tear performance.
  • Defect analysis: Identifying local defects and weakened areas of leather through tear testing.
  • Product durability: Evaluating the service life of leather products combining tear load and other mechanical indicators.

6. Frequently Asked Questions ❓

❓ Q: What is the difference between single and double edge tear?
A: Single edge tear (Part 1) uses a single cut, simulating unilateral tearing; double edge tear (Part 2) uses two cuts, simulating bilateral tearing. Their loading modes differ and results are not interchangeable.
❓ Q: Why is sampling direction important?
A: Leather is anisotropic; tear performance differs significantly between directions parallel and perpendicular to the backbone, so sampling must follow the standard direction for comparability.
❓ Q: Does conditioning strongly affect results?
A: Yes. Leather moisture content varies with ambient humidity, and high humidity reduces tear strength, so specimens must be conditioned to equilibrium in a standard atmosphere before testing.
❓ Q: What is the difference between tear load and tensile strength?
A: Tensile strength reflects resistance to uniform tensile failure; tear load reflects resistance to crack propagation. They differ in physical meaning and test method.
❓ Q: Which leathers does this series apply to?
A: Various leathers including shoe-upper, garment, sofa, bag and automotive-interior leather, and also coated leathers.
🔒