🧵 BS EN ISO 02286 (the ISO 2286 family, published in the UK as BS EN ISO 2286) is the standard series for determination of roll characteristics of rubber- or plastics-coated fabrics, published by the British Standards Institution (BSI) as the UK implementation of EN ISO 2286. Coated fabrics are widely used in tents, tarpaulins, inflatable structures, conveyor belting, protective clothing, luggage and architectural membranes, and their roll characteristics — length, width, mass and thickness — directly determine material usage, performance and cost of the finished product. The series is divided into: Part 1 determination of length, width and net mass; Part 2 determination of total mass per unit area, mass per unit area of coating and mass per unit area of substrate; and Part 3 determination of thickness.
The series applies to coated fabrics with rubber or plastics coatings on a woven (or other textile) substrate. It specifies specimen conditioning, measuring apparatus, procedure and expression of results, and requires measurements under standard atmospheres so that results are accurate and comparable.
The parts characterise the roll from different dimensions: length and width define the geometric size and material usage; net mass is the actual fabric mass excluding cores and packaging; total mass per unit area reflects the overall mass of fabric per unit area; coating and substrate mass per unit area characterise coating thickness/loading and substrate mass separately — key indices for coating uniformity and cost control; thickness directly reflects mechanical and protective performance.
| Part | Determination | Main Apparatus | Expression | Typical Application |
|---|---|---|---|---|
| BS EN ISO 2286-1:2016 | Length, width, net mass | Tape measure, measuring device, balance | m, mm, kg | Outgoing metering, pricing, acceptance |
| BS EN ISO 2286-2:2016 | Total / coating / substrate mass per unit area | Weighing, cutting, separation | g/m² | Cost control, coating uniformity |
| BS EN ISO 2286-3:2016 | Thickness | Thickness gauge (dial micrometer) | mm | Mechanical and protective performance |
All three parts were prepared by ISO/TC 45 “Rubber and rubber products” in collaboration with CEN/TC 248 “Textiles and textile products”, with ICS 59.080.40 (coated fabrics); UK participation was entrusted to BSI Technical Committee TCI/69 (Footwear, leather and coated fabrics). The 2016 editions supersede the corresponding 1998 editions.
The standards require calibrated measuring apparatus to measure length and width in the unrolled state, with readings to the stated division; net mass is obtained by deducting the core and packaging mass, possibly by weighing the whole roll and calculating. Measurement should avoid the irregular parts at the roll ends and average several points to reduce errors from winding tension and edges.
Total mass per unit area is computed by weighing a specimen of known area (e.g., a square or circular piece of stated size); coating and substrate mass per unit area are obtained by separating the coating from the substrate (mechanical peeling or chemical dissolution) and weighing each part separately. The standards give the separation methods and formulas and require account to be taken of interfacial residue and mass loss.
Thickness is measured with a thickness gauge at a specified pressure, with the pressure and dwell time per the standard. Measuring points should be evenly distributed and avoid coating defects, creases and edges; results are expressed as the average of several points. Non-uniform thickness affects strength, air tightness and appearance.
Conditioning (temperature, humidity, time) is required before all measurements; results are reported with the appropriate significant figures, including average, range or standard deviation. The relationship between mass per unit area and thickness may be reported where relevant.
For mass per unit area: cut specimens to the stated size → condition to constant mass → weigh to obtain total mass → divide by area for total mass per unit area → separate coating and substrate → weigh each → compute coating and substrate mass per unit area.
Net mass excludes the core and packaging and is the fabric mass alone; gross mass includes them. The standard takes net mass as the delivery and metering reference, so the buyer should clarify the pricing basis.
First measure the total mass per unit area, then separate coating from substrate (mechanical peeling or chemical dissolution), weigh each part and compute the individual mass per unit area. Separation should minimise coating loss.
Coated fabrics are compressible, so different gauge pressures give different readings. A uniform pressure and dwell time per the standard make results repeatable and comparable.
Coated fabrics absorb moisture, changing mass and dimensions, and temperature and humidity affect fabric and coating performance. Conditioning brings the specimen to the standard moisture and temperature equilibrium, ensuring repeatability.
Length, width, net mass and mass per unit area determine the usable area and material cost per roll — the core basis for pricing, acceptance and quality judgement — and standardised measurement avoids trading disputes.